Morphology and structure features of heat-resistant reactive for protection of heat-resistant nickel alloys

Denisova V.S., Kurshev E.V., Lonskii S.L., Vlasova O.V.
Denisova V.S., Kurshev E.V., Lonskii S.L., Vlasova O.V. Morphology and structure features of heat-resistant reactive for protection of heat-resistant nickel alloys // Proceedings of VIAM. 2020. No. 4-5. DOI: 10.18577/2307-6046-2020-0-45-54-61. URL: https://viam-works.ru/en/journal/2020/4-5/6
Keywords
glass, silicon tetraboride, structure, nickel alloys, scanning electron microscopy, heat resistance.
Abstract

The surface structure of reaction cured coatings based on a composition of refractory glass in system BaO–Al2O3–SiO2 and silicon tetraboride was studied using atomic force microscopy and scanning electron microscopy depending on the conditions of heat treatment of coatings. Non-significant roughness of the coatings was revealed, the level of which reduces as the result of firing in oxidizing atmosphere. The key structural feature of the reaction cured coatings is the preservation of non-oxidized particles of silicon tetraboride in the glass matrix volume what determines the high level of reaction cured coatings properties.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Solntsev S.S., Rosenenkova V.A., Mironova N.A. Modern multifunctional high-temperature coatings for nickel alloys, sealing metal materials and beryllium alloys. Novosti materialovedeniya. Nauka i tekhnika, 2013, no. 1, paper no. 05. Available at: http://www.materialsnews.ru (accessed: February 03, 2020).
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Bragina L.L. Enamel and protective coating technology. Kharkov: NTU KhPI, 2003, 483 p.
  5. Denisova V.S., Soloveva G.A. Heat-resistant glass-ceramic coating for protection of gas turbines’ combustion chambers parts. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 18–22. DOI: 10.18577/2071-9140-2016-0-4-18-22.
  6. Ovsepyan S.V., Lukina E.A., Filonova E.V., Mazalov I.S. Formation of the Strengthening Phase during the High-Temperature Nitriding of Ni–Co–Cr Weldable Wrought Superalloy. Aviacionnye materialy i tehnologii, 2013, no. 1, pp. 3–8.
  7. Kozlova O.Yu., Hovsepyan S.V., Pomelnikova A.S., Akhmedzyanov M.V. The effect of high-temperature nitriding on the structure and properties of welded heat-resistant nickel alloys. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana, ser.: Mashinostroyeniye, 2016, no. 6 (111), pp. 33–42.
  8. Lukina EA, Hovsepyan SV, Davydova EA, Akhmedzyanov M.V. Structural features of a heat-resistant alloy based on the Ni – Co – Cr system hardened by volume nitriding. Tsvetnye Metally, 2016, no. 7 (883), pp. 76–82.
  9. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  10. Kablov E.N., Solntsev S.S. Oxythermosynthesis – a new step towards materials for advanced aerospace engineering. Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002. Moscow: VIAM, 2002. S. 131–137.
  11. Solncev S.S., Denisova V.S., Rozenenkova V.A. Reaction cure – the new direction in technology ofhigh-temperature composite coatings and materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 329–343. DOI: 10.18577/2071-9140-2017-0-S-329-343.
  12. Solntsev St.S. Erosionand moisture resistant thermoregulating coating for thermal protection system of «Buran» reusable spaceship. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 94–124.
  13. Solntsev S.S. Some features of coatings for tiles reusable heat-protection orbiting spacecraft. Trudy VIAM, 2014, no. 2, paper no. 01. Available at: http://www.viam-works.ru (accessed: February 09, 2020). DOI: 10.18577/2307-6046-2014-0-2-1-1.
  14. Armor for the Buran. VIAM materials and technologies for the ISS «Energy-Buran». Ed. E.N. Kablov. Moscow: Nauka i zhizn, 2013. 128 p.
  15. Solntsev S.S., Denisova V.S., Agarkov A.B., Gavrilov S.V. The influence of BaO–Al2O3–SiO2-glasses addition on reaction-cured coatings properties for nickel alloys protection. Trudy VIAM, 2018, no. 1 (61), paper no. 11. Available at: http://www.viam-works.ru (accessed: November 09, 2019). DOI: 10.18577/2307-6046-2018-0-1-11-11.
  16. Denisova V.S., Lonskii S.L., Kurshev E.V., Malinina G.A. Investigation of structure formation of reaction cured coatings by scanning electron microscopy. Trudy VIAM, 2019, no. 4 (76), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 09, 2020). DOI: 10.18577/2307-6046-2019-0-4-76-87.