Investigation of the physicomechanical properties of volume-reinforced carbon fiber reinforced plastic
Evdokimov A.A., Gulyaev I.N., Nacharkina A.V. Investigation of the physicomechanical properties of volume-reinforced carbon fiber reinforced plastic // Proceedings of VIAM. 2020. No. 3. DOI: 10.18577/2307-6046-2020-0-3-66-73. URL: https://viam-works.ru/en/journal/2020/3/7
Keywords
carbon fiber reinforced plastic, volume-reinforced preform, orthogonal type of weaving, physical and mechanical characteristics, centrifugal compressor impeller, helicopter engine.
Abstract
The physical and mechanical properties of carbon fiber made using a volume-reinforced preform of the orthogonal weave type and a binder VSN-31 at room and elevated (300 °C) temperatures are investigated. The presented research results are presented in comparison with carbon fiber, made on the basis of equal-strength fabric and binder VSN-31. The analysis of the obtained results of the compared carbon fiber plastics is carried out and conclusions are made about their performance at high temperature. The influence of the orientation of the base, weft, and vertical ligation bundles on the physical and mechanical characteristics of carbon fiber plastics is explained.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
- Kablov E.N. Russia in the market of intellectual resources. Ekspert, 2015, no. 28 (951), pp. 48–51.
- Donetskiy K.I., Karavayev R.YU., Raskutin A.Ye., Dun V.A. Carbon fibers composite material on the basis of volume reinforcing triax braiding preformes. Trudy VIAM, 2019, no. 1 (73), paper no. 07. Available at: http://viam-works.ru (accessed: December 13, 2019). DOI: 10.18577/2307-6046-2019-0-1-55-63.
- Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577 / 2071-9140-2019-0-4-18-26.
- Composite fan blade with multilayer reinforcing material: pat. 2384749 Rus. Federation; filed 11.11.08; publ. 20.03.10.
- Novikov A.S., Karimbaev T.D. High-bypass fans for advanced turbofan engines. Dvigatel, 2015, no. 5 (101), pp. 6–11.
- Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), paper no. 08. Available at: http://www.viam-works.ru (accessed: December 13, 2019). DOI: 10.18577/2307-6046-2016-0-2-8-8.
- Evdokimov A.A., Gulyaev I.N., Zelenina I.V. Investigation of the physicomechanical properties and microstructure of volume-reinforced carbon fiber reinforced plastic Trudy VIAM, 2019, no. 4 (76), paper no. 05. Available at: http://viam-works.ru (accessed: December 13, 2019). DOI: 10.18577/2307-6046-2019-0-4-38-47.
- Doneckij K.I., Karavaev R.Yu., Raskutin A.E., Panina N.N. Properties of carbon fiber and fiberglass on the basis of braiding preforms. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 54–59. DOI: 10.18577/2071-9140-2016-0-4-54-59.
- Shimkin A.A., Ponomarenko S.A., Mukhametov R.R. Investigation of the curing process of diphthalonitrile binder. Zhurnal prikladnoy khimii, 2016, vol. 89, no. 2, pp. 256–264.
- Guseva M.A. Cyanic esters are prospective thermosetting binders (review). Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 45–50. DOI: 10.18577 / 2071-9140-2015-0-2-45-50.
- Valevin E.O., Zelenina I.V., Marakhovsky P.S., Gulyaev A.I., Bukharov S.V. Investigation of the influence of heat-moisture effects on the phthalonitrile matrix. Materialovedeniye, 2015, no. 9, pp. 15–19.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.