Ultra-high molecular weight polyethylene: market, properties, directions of application (review)

Valueva M.I., Kolobkov A.S., Malakhovskiy S.S.
Valueva M.I., Kolobkov A.S., Malakhovskiy S.S. Ultra-high molecular weight polyethylene: market, properties, directions of application (review) // Proceedings of VIAM. 2020. No. 3. DOI: 10.18577/2307-6046-2020-0-3-49-57. URL: https://viam-works.ru/en/journal/2020/3/5
Keywords
ultra-high molecular weight polyethylene (UHMWPE), fibers, reinforcing filler, polymer composite materials.
Abstract

The article provides an overview of scientific and technical information in the field of ultra-high molecular weight polyethylene (UHMWPE), information on foreign and Russian manufacturers of UHMWPE, release forms, data on the assortment and properties of fibers and fabrics from UHMWPE of various manufacturers, an overview of applications, ongoing research and prospects development of work in this area. Including data is provided on the rapidly developing market of UHMWPE products manufactured by Chinese manufacturers, as well as on Russian developments in the field of UHMWPE.

Reference list
  1. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Tez. dokl. XX Mendeleyevskogo sezda po obshchey i prikladnoy khimii. Ekaterinburg: UrO RAN, 2016, pp. 25–26.
  3. Buznik V. M., Kablov E. N., Koshurina A. A. Materials for complex technical devices of the Arctic application. Nauchno-tekhnicheskiye problemy osvoyeniya Arktiki. Moscow: Nauka, 2015, pp. 275–285.
  4. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  5. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Grigoreva K.N. Research of the influence of the modifying additives nature on the rheological and thermomechanical properties of a photopolymer composition based on epoxy vinyl ester resin. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 31–40. DOI: 10.18577 / 2071-9140-2019-0-3-31-40.
  6. Erasov V.S. Visualization of mechanical testing processes and experimental data processing via 3D-presentation. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 22–28. DOI: 10.18577/2071-9140-2014-0-s4-22-28.
  7. Kosarina E.I., Krupnina O.A., Demidov A.A., Mikhaylova N.A. Digital optical pattern and its dependence on the radiation image at non-destructive testing by method of digital radiography. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 37–42. DOI: 10.18577/2071-9140-2019-0-1-37-42.
  8. Krivushina A.A., Bobyreva T.V., Yakovenko T.V., Nikolaev E.V. Methods of microorganisms-destructors storage in FSUE «VIAM» collection (review). Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 89–94. DOI: 10.18577 / 2071-9140-2019-0-3-89-94.
  9. Valueva M.I. Modern materials and technologies for obtaining armored products. Voprosy materialovedeniya, 2017, no. 2, pp. 197–207.
  10. Valueva M.I., Zhelezina G.F., Gulyaev I.N. Polymer composite materials of increased̆ wear resistance based on ultra high molecular weight polyethylene. Vse materialy. Entsiklopedicheskiy spravochnik¸ 2017, no. 6, pp. 23–29.
  11. Mikhaylin Yu.A. Ultra-high molecular weight polyethylene (part 1). Polimernyye materialy, 2003, no. 3, pp. 18–21.
  12. Mikhaylin Yu.A. Ultra-high molecular weight polyethylene (part 2). Polimernyye materialy, 2003, no. 4, pp. 24–27.
  13. Ultra-high molecular weight polyethylene market (UHMWPE) by form (sheets, rods & tubes), end-use industry (aerospace, defense, & shipping, healthcare & medical, mechanical equipment), region - global forecast to 2021. Available at: https://www.marketsandmarkets.com/Market-Reports/ultra-high-molecular-weight-polyethylene-market-257883188.html (accessed: November 11, 2019).
  14. Gautam Y.R., Singh S., Verma M.K. Application of UHMWPE fiber based composite material. Available at: https://www.researchgate.net/publication/327221940 (accessed: November 11, 2019).
  15. Sergeeva E.A., Kostina K.D. Methods for producing composites and products based on fabric from UHMWPE and rubber for the production of fuel tanks. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2014, vol. 17, no. 5, pp. 101–105.
  16. Ultra high molecular weight polyethylene (UHMWPE) market size, share & trends analysis report by product (medical grade & prosthetics, fibers, sheet, r), by application, and segment sorecasts, 2019–2025. Available at: https://www.grandviewresearch.com/industry-analysis/ultra-high-molecular-weight-polyethylene-market (accessed: November 11, 2019).
  17. Ianucci L., Pope D.J., Dalzell M. A constitutive model for DYNEEMA UD composites. Available at: https://www.researchgate.net/publication/286130335_A_constitutive_model_for_dyneema_UD_composites (accessed: November 11, 2019).
  18. Marissen R., Duurkoop D., Hoefnagels H., Bergsma O.K. Creep forming of high strength polyethylene fiber prepregs for the production of ballistic protection helmets. Composites Science and Technology, 2010, no. 70, pp. 1184–1188.
  19. Galibeev S.S., Khayrullin R.Z., Arkhireev V.P. Ultra high molecular weight polyethylene. Trends and Prospects. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2008, no. 2, pp. 50–55.
  20. Adashkevich S.V., Bakaev A.G., Zhigulin D.V., Markevich M.I., Stelmakh V.F., Chaplanov A.M., Scherbakova E.N. Properties of a composite based on ultrahigh molecular weight polyethylene. Materialy 9 Mezhdunar. nauch.-tekhn. konf. «Priborostroyeniye-2016» (Minsk, November 23–25, 2016). Minsk: BNTU, 2016, pp. 246–247.
  21. Products of Teijin Aramid B.V. Available at: http://www.teijinaramid.com/en (accessed: November 11, 2019).
  22. Belyaeva E.A., Kosolapov A.F., Osipchik V.S. et el. The effect of modifiers of various chemical nature on the operational properties of epoxyamine binders for composites based on fibers from UHMWPE. Plasticheskiye massy, 2019, no. 7–8, pp. 57–61.
  23. Sergeeva EA, Ibatullina A.R., Brysaev A.S. Strength characteristics of composite materials based on plasma-activated ultra-high molecular weight polyethylene fibers. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, no. 18, pp. 133–135.
  24. Pakhomov P.M., Khizhnyak S.D., Golikova A.Yu., Galitsyn V.P. Structural rearrangements during gel-forming of high-strength polymer fibers. Fizika tverdogo tela, 2005, vol. 47, no. 6, pp. 994–999.
  25. OXEA Werk Ruhrchemie. Available at: http://www.ruhrchemie.de/ueberblick/geschichte.html (accessed: November 11, 2019).
  26. Global and China ultra high molecular weight polyethylene (UHMWPE) industry. Report, 2019–2025. Available at: https://www.marketresearch.com/Research-in-China-v3266/Global-China-Ultra-High-Molecular-12403936 (accessed: November 11, 2019).
  27. Selyutin G.E., Gavrilov Yu.Yu., Voskresenskaya E.N., Zakharov V.A., Nikitin V.E., Poluboyarov V.A. Composite materials based on ultra high molecular weight polyethylene: properties, prospects for use. Khimiya v interesakh ustoychivogo razvitiya. 2010, no. 18. S. 375–388.
  28. Kurtz S.M. Ultra-high molecular weight polyethylene in total joint replacement: UHMWPE handbook. Elsevier Academic Press, 2004, 337 p.
  29. Vishnyakova E.A., Selyutin G.E., Gavrilov Yu.Yu. et al. Obtaining composites based on ultra-high molecular weight polyethylene with bactericidal properties. Journal of Siberian Federal University. Chemistry 4. 2013, no. 6, pp. 372–379.
  30. Global and China ultra high molecular weight polyethylene (UHMWPE) industry. Report, 2017–2021. Available at: http://www.researchinchina.com/htmls/report/2017/10432.html (accessed: November 11, 2019).
  31. High-strength, high-modulus polyethylene fiber Dyneema®. Available at: http://download.unitexrussia.ru/DSM_Dyneema_factsheet_UHMWPE-RUS.pdf (accessed: November 11, 2019).
  32. Abrasion and impact resistance with excellent mechanical properties. Available at: https://celanese.com/engineered-materials/products/gur-uhmw-pe.aspx (accessed: November 11, 2019).
  33. BraskemUTEC. Available at: https://www.braskem.com.br/utec (accessed: November 11, 2019).
  34. Lupolen UHM 5000. Available at: https://www.lyondellbasell.com/en/polymers/p/Lupolen-UHM-5000/c452d062-5073-4b19-ad79-383bf90a7e90 (accessed: November 11, 2019).
  35. Products and support of Beijing protech new material science Co., Ltd. Available at: http://www.chn-protech.com (accessed: November 11, 2019).
  36. Products of Jiangsu Dongrun Safety Technology Co., Ltd. Available at: http://www.dongrunsafety.com (accessed: November 11, 2019).
  37. Products of Jiangxi Great Wall Protection Equipment Industry Co., Ltd. Available at: http://www.chinaccgk.com (accessed: November 11, 2019).
  38. Sinty UHMWPE fiber. Available at: http://www.sintyfiber.com (accessed: November 11, 2019).
  39. China uhmwpe fiber. Available at: https://www.alibaba.com/countrysearch/CN/uhmwpe-fiber.html (accessed: November 11, 2019).
  40. Matveeva N.V., Musin R.R. 3D-design of a plant for the production of ultra-high molecular weight polyethylene. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2013, no. 10, pp. 146–147.
  41. Ashpin O. Ultra-high molecular weight project. The Chemical Journal, 2006. Sept, pp. 30–33.
  42. Ultra-high molecular weight polyethylene (UHMWPE) – material for extreme operating conditions. Available at: http://catalysis.ru/block/ index.php? ID = 3 & SECTION_ID = 1487 (accessed: November 11, 2019).
  43. Polynit Textile of Polinit Group of Companies. Available at: http://polinit-textile.ru/pdf/spravka.pdf (accessed: November 11, 2019).
  44. UHMWPE fibers and products from them. Available at: http://www.formoplast-spb.ru/volokna-svmp (accessed: November 11, 2019).