Erosion resistant paint coverings of aviation purpose

Part 1. Erosion resistant paint coatings based on epoxy and polyurethane films forming (review)
Kondrashov E.K., Naidenov N.D.
Kondrashov E.K., Naidenov N.D. Erosion resistant paint coverings of aviation purpose. Part 1. Erosion resistant paint coatings based on epoxy and polyurethane films forming (review) // Proceedings of VIAM. 2020. No. 2. DOI: 10.18577/2307-6046-2020-0-2-81-90. URL: https://viam-works.ru/en/journal/2020/2/9
Keywords
erosion resistance, cycles, heat resistance, film formers: epoxy, polyurethane, polyimide.
Abstract

This paper summarizes the research results on the development of erosion-resistant coatings based on epoxy, polyurethane and polyimide film formers with heat resistance up to 350 °C. It was found that the erosion resistance of coatings depends not only on their strength and elongation, but also on their dynamic parameters and structure of fillers. Comparative data on the technological and physicomechanical properties of epoxy-polyamide, epoxy-rubber and polyurethane enamels intended for protection against impact-abrasive wear are given.

Reference list
  1. Chebotarevskiy V.V., Kondrashov E.K. Technology of coatings in mechanical engineering. Moscow: Mashinostroyeniye, 1978, 296 p.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Buznik V.M., Kablov E.N., Koshurina A.A. Materials for complex technical devices of the Arctic application. Nauchno-tekhnicheskiye problemy osvoyeniya Arktiki. Moscow: Nauka, 2015, pp. 275–285.
  4. Kablov E.N. Quality control of materials – a guarantee of the safety of operation of aircraft. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
  5. Khrushchov M.M., Babichev M.A. Abrasive wear. Moscow: Nauka, 1970, 252 p.
  6. Ratner A.V., Zelinsky V.G. Erosion of materials of heat power equipment. Moscow; Leningrad: Energiya, 1966, 271 p.
  7. Urvantsev L.A. Erosion and metal protection. Moscow: Mashinostroyeniye, 1966, 235 p.
  8. Gorlin S.M. Experimental aeromechanics. Moscow: Vysshaya shkola, 1970, 424 p.
  9. Kashcheev V.N. Abrasive destruction of solids. Moscow: Nauka, 1970, 248 p.
  10. Kozyrev S.P. Hydroabrasive wear of metals during cavitation. Moscow: Mashinostroyeniye, 1964, 139 p.
  11. Perelman R.G. Erosive strength of engine parts and aircraft power plants. Moscow: Mashinostroyeniye, 1980. 246 p.
  12. Erosion / line from Engl., ed. Yu.V. Polezhaev. Moscow: Mir, 1982, 2644 p.
  13. Kleis I.R. Theory of friction, wear and standardization problems. Bryansk, 1978, 387 p.
  14. Kondrashov E.K., Vladimirsky V.N., Bejder E.Ya. Erosion-resistant coatings. Moscow: Khimiya, 1989. 135 p.
  15. Vladimirsky V.N. Development and research of coatings for the protection of GTE blades from erosion and corrosion damage: thesis, Cand. Sc. (Tech.). Moscow, 1977, 34 p.
  16. Kuznetsova V.A., Kondrashov E.K., Semenova L.V., Kuznetsov G.V. On the effect of the shape of particles of zinc oxide on the operational properties of polymer coatings. Materialovedeniye, 2012, no. 12, pp. 12–14.
  17. Kuznetsova V.A., Kondrashov E.K., Vladimirsky V.N., Kuznetsov G.V. Dispersion-reinforced erosion-resistant coatings. Aviacionnye materialy i tehnologii, 2003, Issue: Lakokrasochnye materialy i pokrytiya, pp. 53–56.
  18. Kuznetsova V.A., Vladimirsky V.N., Kondrashov E.K. Prediction of erosion resistance of paint coatings taking into account dynamic parameters. Aviacionnye materialy i tehnologii, 2003, ssue: Lakokrasochnyye materialy i pokrytiya, pp. 50–53.
  19. Kuznetsova V.A. Erosion-resistant composition based on a three-phase system epoxy oligomer – rubber – reinforcing filler: thesis abstract, Cand. Sc. (Tech.). Moscow, 1999. 24 p.
  20. Rabek Ya. Experimental methods in the chemistry of polymers: in 2 parts, line from Engl. Moscow: Mir, 1983. 480 p.
  21. Solyankin I.N., Kuznetsova V.A., Kondrashov E.K., Myagkov M.V., Bolonin A.B., Drozdov M.A., Pensky N.V. Changes in the chemical composition of the polymer matrix of an erosion-resistant coating during gas-abrasive wear. Lakokrasochnye materialy, 1994, no. 5, pp. 34–38.
  22. Kuznetsova V.A., Vladimirsky V.N., Kondrashov E.K. Weather-resistant erosion-resistant enamel VE-62 for the protection of propeller fan blades. Aviacionnye materialy i tehnologii, 2003, Issue: Lakokrasochnyye materialy i pokrytiya, pp. 58–60.
  23. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  24. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  25. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  26. Semenova L.V., Novikova T.A., Nefedov N.I. Study of removing ability of removers for paint systems removal. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 32–37. DOI: 10.18577 / 2071-9140-2017-0-1-32-37.
  27. Kuznetsova V.A., Shapovalov G.G. Tendencies of development of the erosion-resistant coatings (review. Trudy VIAM, 2018, no. 11 (71), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 12, 2019). DOI: 10.18577/2307-6046-2018-0-11-74-85.