The main trends in the field of machining and joining Al-based MMCs (review)

Pripisnov Ya.A., Kurbatkina E.I., Kosolapov D.V.
Pripisnov Ya.A., Kurbatkina E.I., Kosolapov D.V. The main trends in the field of machining and joining Al-based MMCs (review) // Proceedings of VIAM. 2020. No. 2. DOI: 10.18577/2307-6046-2020-0-2-60-71. URL: https://viam-works.ru/en/journal/2020/2/7
Keywords
metal matrix composite material, aluminum matrix composites, silicon carbide, particle reinforcement, ultrasonic assisted machining, high power diode laser welding, friction stir welding, joining.
Abstract

The paper presents a review of current information in the field of machining and production of permanent joints of low-filled and high-filled metal matrix composites (MMCs) based on aluminum alloys, reinforced with various reinforcing fillers. The comparison of technological methods of joining of aluminum MMCs obtained by different manufacturing methods is given. Such modern methods and technologies of forming and obtaining permanent joints of parts from aluminum МMCs as ultrasonic turning and milling, friction welding with mixing are considered, high power diode laser welding. The properties of reinforcing components for metal matrices and their influence on the wear of the cutting tool and the quality of the resulting surface are shown. Analysis of foreign experience for the appropriateness of decisions Lee–Schaeffer and Ernst–Merchant in processing of aluminum MMCs and technologies, laser welding and brazing of highly filled backings of Al–SiC. At the end of the review, conclusions are drawn and the latest trends in the field of aluminum MMCs processing and the formation of the connection of final products from them are indicated.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp.16–21.
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  6. Narayana Murty S.V.S., Nageswara Rao B., Kashyap B.P. On the hot working characteristics of 6061Al–SiC and 6061–Al2O3 particulate reinforced metal matrix composites. Composites science and technology, 2003, vol. 63, pp. 119. DOI: 10.1016/S0266-3538(02)00197-5.
  7. Previtali B., Pocci D., Taccardo C. Application of traditional investment casting process to aluminum matrix composites. Composites: Part A, 2008, vol. 39, p. 1606. DOI: 10.1016/j.compositesa.2008.07.001.
  8. Rino J., Sivalingappa D., Koti H., Jebin V.D. Properties of Al6063 MMC Reinforced With Zircon Sand and Alumina. IOSR Journal of Mechanical and Civil Engineering (IOSR-JMCE), 2013, vol. 5. is. 5, pp. 72–73. DOI: 10.9790/1684-0557277.
  9. Li X., Seah W.K.H. Tool wear acceleration in relation to workpiece reinforcement percentage in cutting of metal matrix composites. Wear, 2001, vol. 2472, pp. 161–171. DOI: 10.1016/S0043-1648(00)00524-X.
  10. Ozben T., Kilickap E., Cakır O. Investigation of mechanical and machinability properties of SiC particle reinforced Al-MMC. Journal of Materials Processing Technology, 2008, vol. 198, pp. 574–579. DOI: 10.1016/j.jmatprotec.2007.06.082.
  11. El-Gallab М., Sklad M. Machining of Al/SiC particulate metal-matrix composites. Part I. Tool performance. Journal of Materials Processing Technology, 1998, vol. 83, pp. 151–158. DOI: 10.1016/S0924-0136(98)00054-5.
  12. El-Gallab М., Sklad M. Machining of Al/SiC particulate metal-matrix composites. Part III. Comprehensive tool wear models. Journal of Materials Processing Technology, 2000, vol. 101, pp. 10–20. DOI: 10.1016/S0924-0136(99)00351-9.
  13. El-Gallab М., Sklad M. Machining of Al/SiC particulate metal-matrix composites. Part IV. Residual stresses in the machined workpiece. Journal of Materials Processing Technology, 2004, vol. 152, pp. 23–34. DOI: 10.1016/S0924-0136(98)00072-7.
  14. Kovrizhnykh A.M. Generalization of the Lee – Schaeffer solution in the theory of metal cutting. Doklady Akademii Nauk, 2008, vol. 418, no. 2, pp.184–187.
  15. Nikouei S.M., Yousefi R., Kouchakzadeh M.A., Kadivar M.A. Cutting Model in Machining of Al/SiCp Metal Matrix Composite. Advanced Materials Research, 2011, vol. 410, pp. 291–297. DOI: 10.4028/www.scientific.net/AMR.410.291.
  16. Pripisnov Ya.A., Grishina O.I. Modern methods of mechanical processing of composite materials (review). Trudy VIAM, 2018, no. 10 (70), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 12, 2019). DOI: 10.18577/2307-6046-2018-0-10-53-61.
  17. Feucht F., Ketelaer J., Wolff A., Mori M., Fujishima M. Latest machining Technologies of Hard-to-cut Materials by Ultrasonic Machine Tool. Procedia CIRP, 2014, vol. 14, pp. 148–152. DOI: 10.1016/j.procir.2014.03.040.
  18. Zhong Z.W., Lin G. Ultrasonic assisted turning of an aluminium-based metal matrix composite reinforced with SiC particles. The International Journal of Advanced Manufacturing Technology, 2006, vol. 27, is. 11–12, pp. 1077–1081. DOI: 10.1007/s00170-004-2320-3.
  19. Ellis M.B.D. Joining of Al-Based Metal Matrix Composites. Materials and Manufacturing Processes. 1996, vol. 11, pp. 45–46. DOI: 10.1080/10426919608947460.
  20. Sheikh-Ahmad Y., Ali D.S., Deveci S., Almaskari F., Jarrar F. Friction stir welding of high density polyethylene-Carbon black composite. Journal of Materials Processing Technology. 2019, vol. 264, pp. 402–413. DOI: 10.1016/j.jmatprotec.2018.09.033.
  21. Periyasamy P., Mohan B., Balasubramanian V. et al. Multi-objective optimization of friction stir welding parameters using desirability approach to join Al/SiCp metal matrix composites. Transactions of Nonferrous Metals Society China. 2013, vol. 23, pp. 942–955. DOI: 10.1016/S1003-6326(13)62551-0.
  22. Rams J., Ferrer M., Múnez C.J., Urena A. High-power diode laser welding of highly reinforced Al–SiC composites. 13th European Conference on Composite Materials (Jun 2–5, 2008). Available at: http://www.escm.eu.org/docs/eccm13/1312.pdf (accessed: January 09, 2020).