Modern trends of protective galvanic coatings working at high temperatures (review)

Khmeleva K.M., Kozlov I.A., Nikitin Ya.Yu., Nikiforov A.A.
Khmeleva K.M., Kozlov I.A., Nikitin Ya.Yu., Nikiforov A.A. Modern trends of protective galvanic coatings working at high temperatures (review) // Proceedings of VIAM. 2020. No. 12. DOI: 10.18577/2307-6046-2020-0-12-75-86. URL: https://viam-works.ru/en/journal/2020/12/8
Keywords
hot corrosion, electrodeposition coating, corrosion resistance, high-temperature alloy, composite coating, oxidation.
Abstract

Provides an overview of foreign scientific and technical literature in the field of protective galvanic coatings for heat-resistant alloys based on nickel and γ-TiAl. Various types and systems of alloying of galvanic coatings are considered, which can be used to protect parts of the hot part of gas turbine engines from high-temperature sulfide-oxide corrosion at operating temperatures up to 1000 °С. Data on the influence of the deposition technology, electrolyte composition, additives on the properties of coatings, the morphology of individual coatings, as well as the results of corrosion tests of some coatings are presented.

Reference list
  1. Kablov E.N. The key problem is materials. Trends and guidelines for innovative development in Russia. Moscow: VIAM, 2015.S. 458–464.
  2. Volkov A.M., Karashaev M.M., Bakradze M.M., Pustynnikov T.O. Alternative technologies of the incresing of mechanical properties of p/m Ni-based superalloys for jet-engine disk application (review). Trudy VIAM, 2019, No. 8 (80), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 12, 2020). DOI: 10.18577/2307-6046-2019-0-8-3-8.
  3. Chabina E.B., Lomberg B.S., Filonova E.V., Ovsepyan S.V., Bakradze M.M. Change of structural and phase condition of heat resisting deformable nickel alloy at alloying tantalum and rhenium. Trudy VIAM, 2015, no. 9, paper no. 03. Available at: http://www.viam-works.ru (accessed: October 12, 2020). DOI: 10.18577/2307-6046-2015-0-9-3-3
  4. Chabina E.B. Microalloying influence by lanthanoids on feature of forming of structure grain boundaries and interphase boundaries of / heat resisting nickel alloy of the VZh175 type. Trudy VIAM, 2017, no. 2 (50), paper no. 09. Available at: http://www.viam-works.ru (accessed: October 12, 2020). DOI: 10.18577/2307-6046-2017-0-2-9-9.
  5. Razuvaev E.I., Bubnov M.V., Bakradze M.M., Sidorov S.A. HIP and deformation of the granulated heat resisting nickel alloys. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 80–86. DOI: 10.18577/2071-9140-2016-0-S1-80-86.
  6. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally of Evrazii, 2012, no. 3, pp. 10–15.
  8. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  9. Khorev A.I. Fundamental and applied projects on titanium alloys and prospective areas of their development as applied to «Buran» spaceship. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 10–14.
  10. Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details. Trudy VIAM, 2013, no. 3, paper no. 02. Available at: http://www.viam-works.ru (accessed: October 12, 2020).
  11. Horev A.I. Fundamental and applied works on structural titanium alloys and perspective directions of their development. Trudy VIAM, 2013, no. 2, paper no. 04. Available at: http://www.viam-works.ru (accessed: October 12, 2020).
  12. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  13. Kablov E.N. VIAM. The direction of the main blow. Nauka i zhizn, 2012., no. 6, pp. 14–18.
  14. Antipov V.V. Strategy of development of titanium, magnesium, beryllium and aluminum alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 157–167.
  15. Beltran A.M., Shores D.A., Sims C.T., Hagel W.C. Hot Corrosion, the Superalloys. New York: Wiley-Interscience, 1972, pp. 317–339.
  16. Balashadehi M.M., Nourpour P., Rouh Aghdam A.S. et al. The formation, microstructure and hot corrosion behaviour of slurry aluminide coating modified by Ni/Ni–Co electrodeposited layer on Ni-base superalloy. Surface & Coatings Technology, 2020, vol. 402, pp. 126–283.
  17. Karimzadeh A., Aliofkhazraei M., Walsh F.C. A review of electrodeposited Ni–Co alloy and composite coatings: microstructure, properties and applications. Surface Coatings Technology, 2019, vol. 372, pp. 463–498.
  18. Donachie M.J., Donachie S.J. Superalloys: a technical guide. 2nd ed. ASM international: Materials Park, 2002, 432 p.
  19. Bouchaud B., Rannou B., Pedraza F. Slurry aluminizing mechanisms of Ni-based superalloys incorporating an electrosynthesized ceria diffusion barrier. Materials Chemistry and Physics, 2013, vol. 143, pp. 416–424.
  20. Electroplating nickel, cobalt, nickel–cobalt alloys and binary or ternary alloys of nickel, cobalt and iron: pat. US 4069112A; filed 18.06.76; publ. 04.10.76.
  21. Choi S.C., Cho H.J., Lee D.B. Effect of Cr, Co, and Ti additions on the hightemperature oxidation behavior of Ni3Al. Oxidation of Metals, 1996, vol. 46, pp. 109–127.
  22. Lai G.Y. High Temperature Corrosion in Energy Systems: Proceeding of the Symposium. The Metallurgical Society of AIME, 1985, 832 p.
  23. Bakhit Babak, Akbari Alireza, Nasirpouri Farzad, Ghasem Hosseini Mir. Corrosion resistance of Ni–Co alloy and Ni–Co/SiC nanocompositecoatings electrodeposited by sediment codeposition technique. Applied Surface Science, 2014, vol. 307, pp. 351–359.
  24. Pavlatou E.A., Stroumbouli M., Gyftou P., Spyrellis N. Hardening effect induced by incorporation of SiC particles in nickel electrodeposits. Journal of Applied Electrochemistry, 2006, vol. 36, pp. 385–394.
  25. Zimmerman A.F., Palumbo G., Aust K.T., Erb U. Mechanical properties of nickel silicon carbide nanocomposites. Materials Science and Engineering: A, 2002, vol. 328, pp. 137–146.
  26. Balaji R., Pushpavanam M., Kumar K.Y., Subramanian K. Electrodeposition of bronze-PTFE composite coatings and study on their tribological characteristics. Surface Coatings Technology, 2006, vol. 201, pp. 3205–3211.
  27. Yue-bo Z., Yuan-zh D. Oxidation resistance of co-deposited Ni–SiC nanocomposite coating. Transactions of Nonferrous Metals Society of China, 2007, vol. 17, pp. 925–928.
  28. Lekka M., Kouloumbi N., Gajo M., Bonora P.L. Corrosion and wear resistant electrodeposited composite coatings. Electrochimica Acta, 2005, vol. 50, pp. 4551–4556.
  29. Xu J., Zhuo C., Han D. et al. Erosion-corrosion behavior of nanoparticle-reinforced Ni matrix composite alloying layer by duplex surface treatment in aqueous slurry environment. Corrosion Science, 2009, vol. 51, pp. 1055–1106.
  30. Gogotsi Y. Nanomaterials handbook. Taylor & Francis Group. New York: CRC Press, 2006, 800 p.
  31. Conway B.E., Vayenas C.G., White R., Gamboa-Adelco M. Modern Aspects of Electrochemistry. Springer Science and Business Media, Inc., 2005, no. 38, pp. 475–532.
  32. Ma Li, Zhou Kechao, Li Zhiyou. Hot corrosion of a novel (Ni, Co)O/(Ni, Co)Fe2O4 composite coating thermally converted from an electrodeposited Ni–Co–Fe2O3 composite coating. Corrosion Science, 2011, vol. 53, pp. 2357–2367.
  33. El-Shobaky G.A., Fagal G.A., El-Aal A.A., Ghozza A.M. Solid–solid interactions in the NiO/Fe2O3 system with and without LiO2 doping. Thermochimica Acta, 1995, vol. 256, pp. 429–441.
  34. Rezaeiolum A., Aliofkhazraei M., Karimzadeh A. et al. Electrodeposition of Ni–Mo and Ni–Mo-(nano Al2O3) multilayer coatings. Surface Engineering, 2017, vol. 34, pp. 423–432.
  35. Prioteasa P., Anicai L., Visan T. Synthesis and corrosion characterization of electrodeposited Ni–Mo alloys obtained from aqueous solutions. UPB Scientific Bulletin, series B, 2010, vol. 72, pp. 11–24.
  36. Huang P.-C., Hou K.-H., Sheu H.-H. et al. Wear properties of Ni–Mo coatings produced by pulse electroforming. Surface Coating Technology, 2014, vol. 258, pp. 639–645.
  37. Alizadeh M., Cheshmpish A. Electrodeposition of Ni–Mo/Al2O3 nano-composite coatings at various deposition current densities. Applied Surface Science, 2019, vol. 466, pp. 433–440.
  38. Szczygieł B., Kołodziej M. Composite Ni/Al2O3 coatings and their corrosion resistance. Electrochimica Acta, 2005, vol. 50, pp. 4188–4195.
  39. Zhang C., Peng X., Zhao J., Wang F. Hot corrosion of an electrodeposited Ni–11 wt. % Cr nanocomposite under molten Na2SO4–K2SO4–NaCl. Journal of Electrochemestry Society, 2005, vol. 152, pp. B321–B326.
  40. Zhou Y., Peng X., Wang F. Oxidation of a novel electrodeposited Ni–Al nanocomposite film at 1050 °C. Scripta Materialia, 2004, vol. 50, p. 1429.
  41. Zhou Y., Peng X., Wang F. Size effect of Al particles on the oxidation of electrodeposited Ni–Al composite coatings. Oxidation of Metals, 2005, vol. 64, p. 169.
  42. Zhang Y., Peng X., Wang F. Development and oxidation at 800 °C of a novel electrodeposited Ni–Cr nanocomposite film. Materials Letters, 2004, vol. 58, p. 1134.
  43. Yang X., Peng X., Wang F. Hot corrosion of a novel electrodeposited Ni–6Cr–7Al nanocomposite under molten (0.9Na, 0.1K)2SO4 at. 900 °С. Scripta Materialia, 2007, vol. 56, pp. 891–894.
  44. Chen H., Si Y.Q., McCartney D.G. An analytical approach to the b-phase coarsening behaviour in a thermally sprayed CoNiCrAlY bond coat alloy. Journal of Alloys and Compounds, 2017, vol. 704, pp. 359–365.
  45. Rana N., Mahapatra M.M., Jayaganthan R., Prakash S. Deposition of nanocrystalline coatings by modified LVOF thermal spray method. Journal of Alloys and Compounds, 2014, vol. 615, pp. 779–783.
  46. Gong X., Ma Y., Guo H., Gong S. Effect of thermal cycling on microstructure evolution and elements diffusion behavior near the interface of Ni/NiAl diffusion couple. Journal of Alloys and Compounds, 2015, vol. 642, pp. 117–123.
  47. Christensen R.J., Tolpygo V.K., Clarke D.R. The influence of the reactive element yttrium on the stress in alumina scales formed by oxidation. Acta Materialia, 1997, vol. 45, pp. 1761–1766.
  48. Evans A.G., Mumm D.R., Hutchinson J.W. et al. Mechanisms controlling the durability of thermal barrier coatings. Progress in Materials Science, 2001, vol. 46, pp. 505–553.
  49. Chen W.R., Wu X., Marple B.R., Patnaik P.C. The growth and influence of thermally grown oxide in a thermal barrier coating. Surface Coating Technology, 2006, vol. 201, pp. 1074–1079.
  50. Tianquan L., Hongbo G.U.O., Hui P., Shengkai G. Cyclic oxidation behavior of an EB-PVD CoCrAlY coating influenced by substrate/coating interdiffusion. Chinese Journal of Aeronautics, 2012, vol. 25, pp. 796–803.
  51. Narita T. Advanced coatings on high temperature applications. Materials Science Forum, 2006, vol. 522–523, pp. 1–14.
  52. Coutsouradis D., Davin A., Lamberigts M. Cobalt–based superalloys for applications in gas turbines. Materials Science and Engineerin, 1987, vol. 88, pp. 11–19.
  53. Yapontseva Yu.S., Kublanovsky V.S., Vyshnevskyi O.A. Electrodeposition of CoMoRe alloys from a citrate electrolyte. Journal of Alloys and Compounds, 2018, vol. 766, pp. 894–901.
  54. Song Y., Wei G., Xiong R. Properties and structure of RE–Ni–W–P–SIC composite coating prepared by impulse electrodeposition. Transaction of Nonferrous Metals Society of China, 2007, vol. 17, pp. 363–367.
  55. Wu L.-K., Wu W.-Y., Song J.-L. et al. Enhanced high temperature oxidation resistance for γ-TiAl alloy with electrodeposited SiO2 film. Corrosion Science, 2018, vol. 140, pp. 388–401.