Investigation of the influence of component composition of PEO electrolytes on their stability and coating properties

Kuzin Ya.S., Kozlov I.A., Sibileva S.V., Fomina M.A.
Kuzin Ya.S., Kozlov I.A., Sibileva S.V., Fomina M.A. Investigation of the influence of component composition of PEO electrolytes on their stability and coating properties // Proceedings of VIAM. 2020. No. 11. DOI: 10.18577/2307-6046-2020-0-11-102-112. URL: https://viam-works.ru/en/journal/2020/11/11
Keywords
aluminum alloys, plasma electrolytic oxidation, electrolyte stability, PEO properties.
Abstract

The efficiency of various variants of the component composition of alkaline electrolytes of plasma electrolytic oxidation (PEO) was studied. Technical liquid glass, NaOH, Na2B4O7, Na3PO4, and NaAlO2 were used as components of aqueous solutions. All of the studied components of electrolytes are the most common for use in PEO processes of aluminum alloys. The influence of the component composition of electrolytes on their stability during 30 days of exposure was evaluated, and the most stable compositions were selected. The structure and properties of coatings formed on samples of aluminum alloy AK6 during PEO are studied. The dependences of the hardness of coatings and their growth rate on the composition of the electrolyte are established. Possible variants of coating growth in the PEO process with different component composition of electrolytes are proposed.

Reference list
  1. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Aluminum-lithium alloys of a new generation and layered aluminum-glass-fiber-reinforced plastics based on them. Tsvetnye metally, 2016, no. 8, pp. 86–91.
  2. Kablov E.N., Lukina E.A., Sbitneva S.V. et al. Formation of metastable phases during the decay of a solid solution in the process of artificial aging of Al-alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 7–17.
  3. Han L.N., Sui Y.D., Wang Q.D. et al. Effects of Nd on microstructure and mechanical properties of cast Al–Si–Cu–Ni–Mg piston alloys. Alloys Compound, 2017, no. 695, pp. 1566–1572.
  4. Klochkov G.G., Grushko O.E., Klochkova Ju.Ju., Romanenko V.A. Industrial development of strength alloy V-1469 of Al–Cu–Li–Mg. Trudy VIAM, 2014, no. 7, paper no. 01. Available at: http://viam-works.ru (accessed: August 26, 2020). DOI: 10.18577/2307-6046-2014-0-7-1-1.
  5. Li S., He C., Fu J., Xu J., Wang Z. Evolution of microstructure and properties of novel aluminum lithium alloy with different roll casting process parameters during twin-roll casting. Materials Characterization, 2020, vol. 161, art. 110145. DOI: 10.1016/j.matchar.2020.110145.
  6. Han J., Wang J., Zhang M., Niu K. Susceptibility of lithium containing aluminum alloys to cracking during solidification. Materialia, 2019, vol. 5, art. 100203. DOI: 10.1016/j.mtla.2018.100203.
  7. Meriç C. Physical and mechanical properties of cast under vacuum aluminum alloy 2024 containing lithium additions. Materials Research Bulletin, 2000, vol. 35, is 9, pp. 1479–1494.
  8. Ghosh A., Adesola A., Szpunar J.A. et al. Effect of tempering conditions on dynamic deformation behavior of an aluminum-lithium alloy. Materials & Design, 2015, vol. 81, pp. 1–10.
  9. Nayan N., Gurao N.P., Narayana Murty S.V.S. et al. Microstructure and micro-texture evolution during large strain deformation of an aluminum-copper-lithium alloy AA2195. Materials & Design, 2015, vol. 65, pp. 862–868.
  10. Odeshi A.G., Tiamiyu A.A., Das D. et al. High strain-rate deformation of T8-tempered, cryo-rolled and ultrafine grained AA 2099 aluminum alloy. Materials Science and Engineering: A, 2019, vol. 754, pp. 602–612.
  11. Yang H.L., Ji S.X., Fan Z.Y. Effect of heat treatment and Fe content on the microstructure and mechanical properties of die-cast Al–Si–Cu alloys. Materials & Design, 2015, no. 85, pp. 823–832.
  12. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys. Trudy VIAM, 2015, no. 4, paper no. 6. Available at: http://www.viam-works.ru (accessed: August 26, 2020). DOI: 10.18577/2307-6046-2015-0-4-6-6.
  13. Yoganandan G., Balaraju J.N., Low C.H.C. et al. Electrochemical and long term corrosion behavior of Mn and Mo oxyanions sealed anodic oxide surface developed on aerospace aluminum alloy (AA2024). Surface & Coatings Technology, 2016, no. 288, pp. 115–125.
  14. Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P. Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material. Trudy VIAM, 2018, no. 4 (64), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 26, 2020). DOI: 10.18577/2307-6046-2018-0-4-59-65.
  15. Ma Y., Zhou X., Liao Y. et al. Effect of anodizing parameters on film morphology and corrosion resistance of AA2099. Journal of the Electrochemical Society, 2016, no. 163 (7), pp. 369–376.
  16. Kablov E.N., Antipov V.V., Senatorova O.G. Laminated glass-fiber reinforced plastics SIAL-1441 and cooperation with AIRBUS and TU DELFT. Tsvetnyye metally, 2013, no. 9, pp. 50–53.
  17. Pavlovskaya T.G., Volkov I.A., Kozlov I.A., Naprienko S.A. Ecologically improved technology of aluminum alloys surface treatment. Trudy VIAM, 2016, no. 7, paper no. 02. Available at: http://viam-works.ru (accessed: August 26, 2020). DOI: 10.18577/2307-6046-2016-0-7-2-2.
  18. Method of obtaining a coating on aluminum alloys: pat. 2547983 Rus. Federation, no. 2014114615/02; filed 14.04.14; publ. 10.04.15.
  19. Duyunova V.A., Kozlov I.A., Oglodkov M.S., Kozlova A.A. Modern trends in the anodic oxidation of aluminum-lithium and aluminum alloys (review). Trudy VIAM, 2019, No. 8 (80), paper no. Art. 09. Available at: http://www.viam-works.ru (accessed: August 27, 2020). DOI: 10.18577/2307-6046-2019-0-8-79-89.
  20. Suminov I.V., Epelfeld A.V., Lyudin V.B. et al. Microarc oxidation (theory, technology, equipment). Moscow: EKOMET, 2005, 368 p.
  21. Suminov I.V., Belkin P.N., Epelfeld A.V. et al. Plasma-electrolytic modification of the surface of metals and alloys: in 2 vols. Moscow: Tekhnosfera, 2011, vol. 2, 512 p.
  22. Rakoch A.G., Bardin I.V. Microarc oxidation of light alloys. Metallurg, 2010, no. 6, pp. 58–61.
  23. Markov G.A., Terleeva O.P., Shulepko E.K. Improving wear resistance of parts of gas and oil equipment due to the implementation of the effect of selective transfer and the creation of wear-resistant coatings. Microarc and arc methods of applying protective coatings: collection of articles, 1985, is 185, pp. 54–64.
  24. Jovović J., Stojadinović S., Šišović N. M., Konjević N. Spectroscopic characterization of plasma during electrolytic oxidation (PEO) of aluminum. Surface and Coatings Technology, 2011, vol. 206, pp. 24-28.
  25. Parfenov E.V., Yerokhin A., Nevyantseva R.R., Gorbatkov M.V. Towards smart electrolytic plasma technologies: An overview of methodological approaches to process modeling. Surface and Coatings Technology, 2015, vol. 269, pp. 2–22.
  26. Hussein R.O., Northwood D.O., Nie X. Coating growth behavior during the plasma electrolytic oxidation process. Journal of Vacuum Science and Technology A: Vacuum, Surfaces and Films, 2010, no. 28, pp. 766–773.
  27. Gnedenkov S.V., Khrisanfova O.A., Sinebryukhov S.L., Puz A.V. Composite protective coatings on the surface of steel. Korroziya: materialy, zashchita, 2007, no. 11, pp. 27–33.
  28. Gnedenkov S.V., Khrisanfova O.A., Sinebryukhov S.L. and others. Composite protective coatings on the surface of titanium nickelide. Korroziya: materialy, zashchita, 2007, no. 2, pp. 20–25.
  29. Gnedenkov S.V., Khrisanfova O.A., Zavidnaya A.G. and others. Silicate protective coatings on steel. Korroziya: materialy, zashchita, 2009, no. 11, pp. 26–32.
  30. Kim G.W., Kim Y.S., Shin D.H. et al. Influence of ZrO2 incorporation into coating layer on electrochemical response of low-carbon steel processed by electrochemical plasma coating. Surface and Coatings Technology, 2015, vol. 269, no. 1, pp. 314–318.
  31. Minaev A.N., Gnedenkov A.S., Gnedenkov S.V. and others. Multifunctional protective coatings for ship power equipment. Morskie intellektualnye tekhnologii, 2013, no. S1, pp. 49–55.