Polymers and polymer composites in sport (review)

Klimenko O.N., Valueva M.I., Rybnikova A.N.
Klimenko O.N., Valueva M.I., Rybnikova A.N. Polymers and polymer composites in sport (review) // Proceedings of VIAM. 2020. No. 10. DOI: 10.18577/2307-6046-2020-0-10-81-89. URL: https://viam-works.ru/en/journal/2020/10/9
Keywords
polymeric composite materials, polymeric materials, reinforcing fillers, carbon plastics, sports, sports infrastructure, sports equipment.
Abstract

Рrovides an overview of scientific and technical information – Russian and foreign periodicals, patents for inventions – in the field of the use of polymeric materials in the sports industry and sports infrastructure. Data on world manufacturers, applied technologies, Russian developments in this direction are presented, examples of the practical use of polymeric materialsin the sports industry are shown. Special attention is paid to polymer composite materials,in particular, based on carbon fibers.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N. Composites: Today and Tomorrow. Metally Yevrazii, 2015, no. 1, pp. 36–39.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. All for the match. Neftekhimiya, 2017, no. 1, pp. 28–33. Available at: http://neftehimia-journal.ru/infrastructure/vse-na-match (accessed: June 25, 2020).
  5. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  6. Zhang L. The application of composite fiber materials in sports equipment. 5th International Conference on Education, Management, Information and Medicine (EMIM 2015), 2015, pp. 450–453. Available at: https://www.atlantis-press.com/proceedings/emim-15/21459 (accessed: 20.06.2020).
  7. The sports market of composites by 2021 will amount to almost $ 4 billion. Basalt. Today. Available at: http://basalt.today/2016/06/5270 (accessed: June 25, 2020).
  8. Sports pole for high jump and polymer composite material for its manufacture: pat. 2050879 Rus. Federation, no. 92012699/12; filed 17.12.92; publ. 27.12.95.
  9. Hockey stick shaft: pat. US5419553A, no. 07/954,156; filed 30.09.92; publ. 30.05.95.
  10. Hockey stick from one hollow source tube: pat. 2401688 Rus. Federation, no. 2006135849/05; filed 10.10.06; publ. 20.10.10.
  11. Improved sports stick design: pat. 2472559 Rus. Federation, no. 2010108680/12; filed 21.08.08; publ. 20.01.13.
  12. Tyunina A.V. Composite materials: production, application, market trends. Polimernyye materialy, 2018, no. 2, pp. 27–29.
  13. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  14. Paton W. Carbon fiber in sports equipment. Composites, 1970, vol. 1, no. 4, pp. 221–226.
  15. Tang D. The application of carbon fiber materials in sports equipment. Applied Mechanics and Materials, 2014, vol. 443, pp. 613–666. Available at: https://www.scientific.net/AMM.443.613 (accessed: June 20, 2020).
  16. Audi Carbon Ski: lightweight construction for winter sports. Available at: https://www.drive.ru/blogs/audi/4efb339100f11713001e5d01.html (accessed: June 25, 2020).
  17. A method of manufacturing a tennis racket frame: pat. SU1801525A1, no. 4862846/12; filed 27.06.90; publ. 15.03.93.
  18. Bicycle frame: pat. 2452649 Rus. Federation, no. 2011105881/11; filed 17.02.11; publ. 10.06.11.
  19. Sports: new records and sports victories. Available at: https://umatex.com/applications/sport (accessed: June 25, 2020).
  20. Kiyanenko E.A., Zenitova L.A., Kuzmin M.G. Innovative technologies in the production of honeycomb panels. Vestnik tekhnologicheskogo universiteta, 2015, vol. 18, no.19, pp. 60–63.
  21. Kalashnikov A.A. Technologies for vacuum forming and pressing of sheet thermoplastic composites with subsequent mechanical processing from GEISS AG. Proceedings of the conference «Polymer composite materials of a new generation for civilian industries» (Moscow, September 11, 2015). Moscow: VIAM, 2015. Available at: https://conf.viam.ru/conf/165/proceedings (accessed: June 25, 2020).
  22. How bobsleigh works. Populyarnaya mekhanika, 2014, no. 2. Available at: https://www.popmech.ru/adrenalin/15339-gonki-na-bobakh (accessed: June 25, 2020).
  23. McLaren Carbon Composite Center. Composite World, 2018, no. 1, p. 11.
  24. Composites in the first place. Composite World, 2019, no. 5, pp. 58–59.
  25. Mishkin S.I., Malakhovskiy S.S. Fast curing resins and prepregs: receiving, properties and areas of application (review). Trudy VIAM, 2019, no. 5 (77), paper no. 04. Available at: http://viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2019-0-5-32-40.
  26. Vlasenko F.S., Raskutin A.E., Doneckij K.I. Application of braided preforms for polymer composite materials in civil industries (review). Trudy VIAM, 2015, no. 1, paper no. 05. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2015-0-1-5-5.
  27. ISPO MUNICH 2020. Available at: https://www.ispo.com/en/munich (accessed: June 25, 2020).
  28. Method of making a stick from polymer composite materials: pat. 2635137 Rus. Federation, no. 2016111517; filed 28.03.16; publ. 03.10.17.
  29. Russian production of hockey sticks. Available at: https: //charger.rf (accessed: June 25, 2020).
  30. Composite materials and structures. Available at: https://www.hexcel.com/Products/Prepregs-and-Resins/HexPly-Prepregs (accessed: June 25, 2020).
  31. Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Phenolformaldehyde binding new generation for interior materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 265–272.
  32. Sokolov I.I., Lukina A.I., Tundaykin K.O., Kovalenko A.V. Assessment of the properties and structure of SMC-materials. Plasticheskiye massy, 2019, no. 1–2, pp. 52–56.
  33. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  34. Zarubin A., Chistyakov G. World Cup-2018: features of carrying out state examination of football stadiums. Messenger of state examination, 2018, no. 2, p. 18–34. Available at: https://www.gge.ru/upload/iblock/002/vestnik-02-2018.pdf (accessed: June 25, 2020).
  35. Arenas of Kazan, Kaliningrad and Rostov-on-Don: changes in architectural images during the evolution of projects. Available at: http://sportengineering.ru/article/futbolnye-stadiony-izmenenie-arhitekturnyh-obrazov-v-hode-evoljutsii-proektov (accessed: June 25, 2020).