Strengthening concrete building structure via reinforcement external system from carbon plastic
UDC
678.747.2:620.1
DOI
10.18577/2307-6046-2020-0-10-73-80
Article PDF (Russian)
(700.43 KB)
How to cite
Evdokimov A.A., Imametdinov E.S., Malakhovskiy S.S. Strengthening concrete building structure via reinforcement external system from carbon plastic // Proceedings of VIAM. 2020. No. 10. DOI: 10.18577/2307-6046-2020-0-10-73-80. URL: https://viam-works.ru/en/journal/2020/10/8
Keywords
carbon plastic, concrete, concrete hardening, external reinforcement system, exposure, stretch when bending.
Abstract
The article describes the results of research work on the reinforcement of concrete structures via carbon reinforcing filler with a cold curing resin. As an object of research were selected: brand of concrete M-350 and experimental cold curing carbon fiber based on an epoxy matrix. The physico-mechanical characteristics of carbon fiber are investigated. The properties of concrete samples externally reinforced with carbon fiber after conducting full-scale exposure in various conditions and without it are investigated. It was established, that strength gain of reinforced samples compared to purely concrete samples is up to 550%.
Reference list
- Vlasenko F.S., Raskutin A.E., Doneckij K.I. Application of braided preforms for polymer composite materials in civil industries (review). Trudy VIAM, 2015, no. 1, paper no. 05. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2015-0-1-5-5.
- Doneckij K.I., Karavaev R.Yu., Raskutin A.E., Panina N.N. Properties of carbon fiber and fiberglass on the basis of braiding preforms. Aviacionnye materialy i tehnologii, 2016, No. 4 (45), pp. 54–59. DOI: 10.18577/2071-9140-2016-0-4-54-59.
- Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Veshkin A.E. Technology of non-autoclave molding of low-porous polymer composite materials and large-sized structures from them: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2016, pp. 5–15.
- Evdokimov A.A., Raskutin A.E., Mishkin S.I., Mikhaldykin E.S. Arched bridges with the use of carbon-fiber arched elements. Konstruktsii iz kompozitsionnykh materialov, 2019, no. 2, pp. 22–29.
- Chursova LV, Raskutin AE, Gurevich Ya.M., Panina N.N. Cold curing binder for the construction industry. Klei. Germetiki. Tekhnologii, 2012, no. 5, pp. 40–44.
- Petrova A.P., Mukhametov R.R., Akhmadieva K.R. Internal stresses in cured polyester binders for polymer composites. Trudy VIAM, 2019, no. 5 (77), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 13, 2020). DOI: 10.18577/2307-6046 -2019-0-5-12-21.
- Volkova A.A., Paykov A.V., Stolyarov O.N. The structure and properties of textile-reinforced concrete. Inzhenerno-stroitelny zhurnal, 2015, no. 7 (59), pp. 50–56.
- Gaynanov D.G., Sizov A.G., Filippov Yu.N. Strengthening of reinforced concrete building structures with carbon fiber. Ekspertiza promyshlennoy bezopasnosti i diagnostika opasnykh proizvodstvennykh obektov, 2015, no. 4, pp. 107–108.
- Bashzhanov A.E. The use of innovative composite materials in the reinforcement of reinforced concrete structural elements. Nauka, tekhnika i obrazovaniye, 2015, no. 4, pp. 117–119.
- Development and use of a system of external reinforcement with carbon polymer fibers for reinforced concrete structures. Available at: https://afzir.com/wp-content/uploads/2017/11/Externally-bonded-FRP-Reinforcement-for-RC-structures.pdf (date accessed: July 01, 2020).
- Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
- Kablov E.N. Trends and guidelines for the innovative development of Russia. 3rd ed. Moscow: VIAM, 2015, 720 p.
- Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
- Venediktova M.A., Krasnov L.L., Kirina Z.V. Some aspects of the use of fire retardant coatings (review). News of material science. Novosti materialovedeniya. Nauka i tekhnika, 2018, no. 1. paper no. 02. Available at: http://www.materialsnews.ru (accessed: June 25, 2020).
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Mishkin S.I., Raskutin A.E., Evdokimov A.A., Gulyaev I.N. Technologies and the main stages of construction of the arch bridge first in Russia from composite materials. Trudy VIAM, 2017, no. 6 (54), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2017-0-6-5-5.