Influence of corrosion inhibiting primer on properties of the glued joints executed using organic silicon glue-hermetic

Petrova A.P., Kuznetsova V.A., Lukina N.F., Isaev A.Yu.
Petrova A.P., Kuznetsova V.A., Lukina N.F., Isaev A.Yu. Influence of corrosion inhibiting primer on properties of the glued joints executed using organic silicon glue-hermetic // Proceedings of VIAM. 2020. No. 10. DOI: 10.18577/2307-6046-2020-0-10-13-20. URL: https://viam-works.ru/en/journal/2020/10/2
Keywords
glue-hermetic, priming covering, glued joint, thermal aging, water resistance, tropic resistance, climatic resistance.
Abstract

Properties of glued joints of D16-AT aluminum alloy with previously put adhesive priming covering EP-0214, received using glue-hermetic Elasil 137-175M are given. Stability of properties of glued joints, both without first coat, and with first coat EP-0214 is shown, is direct after pasting and after thermal aging at temperatures up to 250 °С, influences of water, tropical conditions. Application of priming covering allows to increase gap between anodizing and pasting operations and to increase corrosion resistance.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Abstracts of report XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: UB of RAS, 2016, pp. 25–26.
  3. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Investigation of epoxy-polysulfone polymer systems as the basis for high-strength adhesives for aviation purposes. Klei. Germetiki. Tekhnologii, 2017, no. 3, pp. 7–12.
  4. Petrova A.P., Anikhovskaya L.I. Effect of EP-0234 adhesive primer on the properties of adhesive joints made with VK-50 phenolic rubber glue. Klei. Germetiki. Tekhnologii, 2016, no. 6, pp. 26–28.
  5. Petrova A.P., Lukina N.F. Influence of EP-0234 adhesive primer on the performance of epoxy film glue. Klei. Germetiki. Tekhnologii, 2015, no. 9, pp. 16–19.
  6. Armor for «Buran». Materials and technologies of VIAM for the ISS «Energia-Buran». Ed. E.N. Kablov. Moscow: Nauka i zhizn, 2013, 128 p.
  7. Storozhenko P.A., Minasyan R.M., Polivanov A.N., Nikitushkin I.V., Minasyan O.I. New heat-conducting silicone sealants. Klei. Germetiki. Tekhnologii, 2017, no. 2, pp. 7–10.
  8. Minasyan R.M. One-component silicone sealants. Klei. Germetiki. Tekhnologii, 2010, no. 10, pp. 18–20.
  9. Minasyan R.M., Polivanov A.N., Minasyan O.I. The main directions of work of GNIICHTEOS in the field of organosilicon adhesives-sealants. Khimicheskaya promyshlennost segodnya, 2015, no. 11, pp. 28–32.
  10. Aviation materials: reference book: in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2019. Vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1: Adhesives, adhesive prepregs, 275 p.
  11. Petrova A.P., Donskoy A.A. Adhesive materials. Sealants: a reference book. Saint Petersburg: Professional, 2008, 589 p.
  12. Kuznetsova V.A., Zheleznyak V.G., Silayeva A.A. Influence of mechanical characteristics of priming coverings on stability to cyclic mechanical loads of systems of the erosion resistant disperse reinforced coatings. Trudy VIAM, 2018, no. 6 (66), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 03, 2020). DOI: 10.18577/2307-6046-2018-0-6-59-67.
  13. Antipov V.V., Petrova A.P., Kozlov I.A., Fomina M.A., Volkov I.A. Influence of technological heatings and ways of surface preparation under pasting on mechanical properties of aluminum foil from alloy AMg2N. Trudy VIAM, 2018, no. 7 (67), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 03, 2020). DOI: 10.18577/2307-6046-2018-0-7-10-24.
  14. Baranovskaya N.B., Zakharova M.Z., Mizikin A.I., Berlin A.A. Catalytic curing of polydimethylsiloxane at room temperature. Doklady AN SSSR, 1958, vol. 122, no. 4, pp. 603–606.
  15. Northern V.V., Minasyan R.M., Makarenko I.A., Bizyukova N.M. The mechanism of «cold» vulcanization of low-molecular polyorganosiloxane rubbers. Vysokomolekulyarnye soyedineniya, 1976, vol. 18, no.6, pp. 1276–1281.
  16. Method for producing silicone glue and glue composition: pat. 2009145967/05 Rus. Federation, no. 2467048; filed 07.12.09; publ. 20.11.12.
  17. Primer composition for organosilicon sealants: pat. 2004109931/04 Rus. Federation, no. 2272059; filed 02.04.04; publ. 20.03.06.
  18. Savenkova A.V., Tikhonova I.V., Trebukova E.A. Heat and frost-resistant sealants. Aviation materials at the turn of the XX–XXI centuries. Moscow: VIAM, 1994, pp. 432–439.
  19. Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P. Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material. Trudy VIAM, 2018, no. 4 (64), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 03, 2020). DOI: 10.18577/2307-6046-2018-0-4-59-65.
  20. Sorokin M.F., Kochnova Z.A., Zakharova A.A., Golova N.A. Curing of epoxy oligomers with aminoalkoxysilanes. Lakokrasochnyye materialy i ikh primeneniye, 1986, no. 5, pp. 24–28.
  21. Chalykh A.E., Kochnova Z.A., Zhavoronok E.S. Compatibility and diffusion in the systems epoxy oligomers – liquid carboxylate rubbers. Vysokomolekulyarnyye soyedineniya, ser. A. 2001, vol. 43, no. 12, pp. 1–9.
  22. Anikhovskaya L.I., Pavlovskaya T.G., Dementyeva L.A., Petrova A.P. Surface preparation for bonding. Available at: https://docplayer.ru/61526227-Podgotovka-poverhnostey-pod-skleivanie.html (accessed: August 25, 2020).