The main trends of receiving and applications secondary carbon fibres (review)
Malakhovskiy S.S., Mishkin S.I. The main trends of receiving and applications secondary carbon fibres (review) // Proceedings of VIAM. 2019. No. 9. DOI: 10.18577/2307-6046-2019-0-9-73-79. URL: https://viam-works.ru/en/journal/2019/9/8
Keywords
polymer composite material, recycling, secondary use, fiber reinforced plastic.
Abstract
Describes the modern methods of extracting carbon reinforcing fibers from polymer composite materials. The most popular methods are solvolysis and pyrolysis. Presents specific products from recycled carbon fiber and firms that specialize in this area of production. It is shown that the most popular method of manufacturing using recycled carbon fiber is 3D-printing from granules based on a thermoplastic polymer.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Chursova L.V., Babin A.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE VIAM in the field of melt binders for polymer composite materials] // Polimernyye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
- Kablov E.N. Rossiya na rynke intellektualnykh resursov [Russia in the market of intellectual resources] // Ekspert. 2015. №28 (951). S. 48–51.
- Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
- Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polimernyye kompozitsionnyye materialy novogo pokoleniya na osnove svyazuyushchego VSE-1212 i napolniteley, alternativnykh napolnitelyam firm Porcher Ind. i Toho Tenax [Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. AND Toho Tenax] // Aviacionnye materialy i tehnologii. 2018. №3 (52). S. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Daskovskij M.I., Doriomedov M.S., Skripachev S.Yu. Sistematizaciya bazisnyh faktorov, prepyatstvuyushhih vnedreniyu polimernyh kompozicionnyh materialov v Rossii (obzor) [Underlying factors preventing the introduction of polymer composite materials in Russia (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5 St. 06. Available at: http://www.viam-works.ru (accessed: July 09, 2019). DOI: 10.18577/2307-6046-2016-0-5-6-6.
- Mishkin S.I., Malakhovskiy S.S. Bystrootverzhdayemyye svyazuyushchiye i prepregi: polucheniye, svoystva i oblasti primeneniya (obzor) [Fast curing resins and prepregs: receiving, properties and areas of application (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №5 (77). St. 04. Available at: http://viam-works.ru (accessed: July 10, 2019). DOI: 10.18577/2307-6046-2019-0-5-32-40.
- Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: July 10, 2019).
- Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviaсionnye materialy i tehnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Pimenta S., Pinho S.T. Recycling carbon fibre reinforced polymers for structural applications: technology review and market outlook // Waste Management. 2011. Vol. 31. No. 2. P. 378–392.
- Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Tehnologii utilizacii polimernyh kompozicionnyh materialov (obzor) [Recycling technologies of polymer composite materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 09. Available at: http://viam-works.ru (accessed: July 11, 2019). DOI: 10.18577/2307-6046-2015-0-8-9-9.
- Chursova L.V., Tsybin A.I., Grebeneva T.A., Panina N.N. Retsikling epoksidnykh svyazuyushchikh i polimernykh kompozitsionnykh materialov na ikh osnove (obzor) [Recycling of epoxy resins and polymer composite materials on their bases (review)] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №5–6 (31). St. 06. Available at: http://materialsnews.ru (accessed: July 12, 2019).
- Kulikova Yu.V., Tukacheva K.O. Analiz tekhnologiĭ utilizatsii polimernykh kompozitsionnykh materialov [Analysis of the utilization of polymer composite materials] // Transport. Transportnyye sooruzheniya. Ekologiya. 2017. №4. S. 103–122.
- Conroy A., Halliwell S., Reynolds T. Composite recycling in the construction industry // Composites. Part A. 2006. Vol. 37. P. 1216–1222.
- Products: Application and Properties // Vartega. Available at: https://www.vartega.com (accessed: July 12, 2019).
- Steelhead composites winds first recycled COPV with Vartega fiber // Vartega. Available at: https://www.vartega.com/news-and-media/2017/5/24/steelhead-composites-winds-first-recycled-copv-with-vartega-fiber (accessed: July 13, 2019).
- Smalley M. Boeing, ELG Carbon Fibre to recycle aerospace materials // Recycling today. Available at: https://www.recyclingtoday.com/article/boeing-carbon-fibre-recycle-aerospace-materials/ (accessed: July 15, 2019).
- Po materialam www.recyclingtoday.com, www.compositesworld.com. Pererabotka kompozitov nabirayet silu // Kompozitnyy mir. 2017. №3. S. 48–53.
- Katalog materialov dizaynerskoy mebeli [Catalog of materials for designer furniture] // Kickstater. Available at: https://www.kickstarter.com/projects/1868198703/the-recycled-carbon-chair (accessed: July 14, 2019).
- UAM Says It’s First To Recycle Aircraft Carbon Fiber // The ProfitChain. Available at: https://www.theprofitchain.com/recycle-aircraft-carbon-fiber/ (accessed: July 16, 2019).
- Maty i tekstil iz pererabotannogo uglerodnogo volokna // Carbon Conversations: ofits. sayt. Available at: http://www.carbonconversations.co.uk/2017/01/new-website.html (accessed: July 17, 2019).
- Job S. Summary of recent research and development // Composite Recycling – Materials KTN Report. 2010. P. 5–7.
- Shaydurova G.I., Shevyakov Ya.S., Vasilev I.L. Otsenka vozmozhnosti utilizatsii ugleplastikov khimicheskim metodom [Assessment of the possibility of utilizing carbon plastics by the chemical method] // Prikladnaya ekologiya. 2018. №3. T. 8. S. 135–140. DOI: 10.21285/2227-2925-2018-8-3-135-140.
- Pavlyuchenkova M.A., Kulikova Yu.V. Analiz napravleniy ispolzovaniya vtorichnogo uglevolokna [Analysis of the directions of the use of secondary carbon fiber] // Khimiya. Ekologiya. Urbanistika. 2018. T. 1. S. 470–473.