Comparative structure control of single-crystal castings of nickel superalloys X-ray diffraction methods of oscillation and Laue

Kuzmina N.A., Lifshitz V.A., Potrakhov E.N., Potrakhov N.N.
Kuzmina N.A., Lifshitz V.A., Potrakhov E.N., Potrakhov N.N. Comparative structure control of single-crystal castings of nickel superalloys X-ray diffraction methods of oscillation and Laue // Proceedings of VIAM. 2019. No. 9. DOI: 10.18577/2307-6046-2019-0-9-15-25. URL: https://viam-works.ru/en/journal/2019/9/2
Keywords
single crystal, crystallographic orientation, subgrain disorientation, lauegram, x-ray diffraction.
Abstract

The article compares the possibilities of x-ray swing and Laue methods for mass control of the structure perfection of single-crystal castings of nickel heat-resistant alloys. It is concluded that both methods give similar results in determining the axial orientation of single crystals. In determining the misalignment of the block substructure, the swing method allows us to find the axial deviation of each block relative to the Z axis of the sample, that is, relative to the direction of the main acting voltage, and the Laue method allows us to calculate the angles of disorientation of the blocks relative to the orientation of the main crystal. The advantage of the method of Laue in determining the angle of disorientation blocks, as it allows you to test the disorientation of casting blocks of complex shape.

Reference list
  1. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Monokristallicheskie zharoprochnye nikelevye splavy dlya turbinnyh lopatok perspektivnyh GTD [Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. Metallurgicheskie osnovy obespecheniya vysokogo kachestva monokristallicheskih zharoprochnyh nikelevykh splavov [The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  3. Tolorayya V.N., Kablov E.N., Demonis I.M. Tekhnologiya polucheniya monokristallicheskikh otlivok turbinnykh lopatok GTD zadannoy kristallograficheskoy oriyentatsii iz reniysoderzhashchikh zharoprochnykh splavov [The technology for producing single-crystal castings of turbine engine turbine blades of a given crystallographic orientation from rhenium-containing heat-resistant alloys] // Liteynye zharoprochnyye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 206–219.
  4. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] // Aviacionnye materialy i tehnologii. 2011. №4. S 25–31.
  5. Kablov E.N., Bondarenko Yu.A., Echin A.B. Issledovaniye vliyaniya peremennogo upravlyayemogo temperaturnogo gradiyenta na osobennosti struktury, fazovyy sostav, svoystva vysokotemperaturnykh zharoprochnykh splavov pri ikh napravlennoy kristallizatsii [Investigation of the influence of a variable controlled temperature gradient on structural features, phase composition, and properties of high-temperature heat-resistant alloys during their directed crystallization] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2016. №6 (111). S. 43–61.
  6. Toloraya V.N., Kablov E.N., Svetlov I.L., Orekhov N.G., Golubovskiy E.R. Anizotropiya prochnostnykh kharakteristik monokristallov nikelevykh zharoprochnykh splavov [Anisotropy of the strength characteristics of single crystals of nickel heat-resistant alloys] // Gornyy informatsionno-analiticheskiy byulleten. 2005. Spetsvypusk. S. 225–236.
  7. Toloraya V.N., Kablov E.N., Orekhov N.G., Ostroukhova G.A. Struktura i rostovyye defekty monokristallov nikelevykh zharoprochnykh splavov [Structure and growth defects of single crystals of heat-resistant nickel alloys] // Gornyy informatsionno-analiticheskiy byulleten. 2005. Spetsvypusk. S. 190–202.
  8. Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov. M.R. Izmeneniya mikrostruktury monokristallov zharoprochnyh nikelevyh splavov v processe dlitelnoj ekspluatacii turbinnyh lopatok [The microstructure modifications of single crystals of Ni-based superalloys in time-tested turbine blades] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 9–17. DOI: 10.18577/2071-9140-2016-0-4-9-17.
  9. Nazarkin R.M. Rentgenodifrakcionnye metodiki precizionnogo opredeleniya parametrov kristallicheskih reshetok nikelevyh zharoprochnyh splavov (kratkij obzor) [X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 41–48. DOI: 10.18577/2071-9140-2015-0-1-41-48
  10. Khayutin S.G. O razoriyentatsii zeren pri napravlennoy kristallizatsii [On the disorientation of grains in directed crystallization] // Metallovedeniye i termicheskaya obrabotka metallov. 2007. №6. S. 42–43.
  11. Sidokhin E.F., Sidokhin F.A., Khayutin S.G. O substrukture monokristallicheskikh lopatok GTD [About the substructure of single-crystal GTE blades] // Aviatsionnaya promyshlennost. 2009. №1. S. 34–36.
  12. Sidokhin F.A., Sidokhin A.F., Sidokhin E.F. Ob opredelenii kristallograficheskoy oriyentatsii monokristallov metodom Laue [On the determination of the crystallographic orientation of single crystals by the Laue method] // Zavodskaya laboratoriya. Diagnostika materialov. 2009. T. 75. №1. S. 35–37.
  13. Lisoyvan V.I., Zadneprovskiy G.M. K metodike opredeleniya oriyentatsii kristallograficheskoy ploskosti v monokristalle na difraktometre [On the methodology for determining the orientation of the crystallographic plane in a single crystal on a diffractometer] // Apparatura i metody rentgenovskogo analiza. 1969. Vyp. 4. S. 64–70.
  14. Kheyker D.M. Rentgenovskaya difraktometriya monokristallov [X-ray diffractometry of single crystals]. L.: Mashinostroyeniye, 1973. 256 s.
  15. Potrakhov N.N., Khayutin S.G., Lifshits V.A., Oses R. Ustanovka PRDU-KROS dlya ekspressnogo opredeleniya kristallograficheskoy oriyentatsii kubicheskikh monokristallov po obratnym lauegrammam [Installation of PRDU-CROS for the express determination of the crystallographic orientation of cubic single crystals by inverse lauegrams] // Zavodskaya laboratoriya. Diagnostika materialov. 2015. T. 81. №8. S. 27–30.
  16. Oses R., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Programma rasshifrovki obratnykh lauegramm GTSK-monokristallov dlya opredeleniya kristallograficheskoy oriyentatsii obraztsov (KGO-analiz): svid. o gos. reg. Programmy dlya EVM. №201164448 [The decoding program for the inverse lauagrams of fcc single crystals to determine the crystallographic orientation of the samples (KGO analysis): certificate. about state reg. Computer Programs. No. 2011164448]. 2011.