Study of microorganisms the destructors of functional polymeric materials exposed under conditions of tropical climate simulation

Krivushina A.A., Bobyreva T.V., Goryashnik J.S., Bukharev G.M.
Krivushina A.A., Bobyreva T.V., Goryashnik J.S., Bukharev G.M. Study of microorganisms the destructors of functional polymeric materials exposed under conditions of tropical climate simulation // Proceedings of VIAM. 2019. No. 7. DOI: 10.18577/2307-6046-2019-0-7-76-83. URL: https://viam-works.ru/en/journal/2019/7/9
Keywords
biodeterioration, biodegradation, microorganisms-destructors, microbiological resistance, non-metallic materials, microflora, microbial damage, exposure, tests.
Abstract

Tests are carried out in various conditions in order to study the microbiological resistance of functional materials and the isolation of new microorganisms-destructors. Polymeric materials and structural elements were exposed for 18 months under imitation of tropical climate weathering conditions. In exposition were used samples of rubber and sealant. Cultures of microscopic fungi were isolated after exposure from the samples surfaces and thereafter their species identified along with theirs occurrence frequency counting. The dominant species of micromycetes were Penicillium lanosum and Cladosporium sphaerospermum. Such species as Penicillium sp. (non P. lanosum), Cladosporium oxysporum and Aspergillus ochraceus were rarely isolated. Single occurrence was noted for Rhizopus oryzae, Aspergillus terreus, Acremonium sp., Stachybotrys chartarum and Trichoderma viride. Most of the isolated fungi are known as destructors of polymeric materials in different climatic zones and environmental conditions.

Reference list
  1. Kablov E.N. Klyuchevaya problema – materialy [The key problem is materials] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M.: VIAM, 2015. S. 458–464.
  2. Kablov E.N., Erofeev V.T., Svetlov D.A., Smirnov V.F., Bogatov A.D. Biopovrezhdeniya v kosmicheskikh apparatakh [Biodetermination in spacecraft] // Tr. Mezhdunar. nauch.-tekhnich. konf. «Kompozitsionnyye materialy. Teoriya i praktika», 2015. S. 40–46.
  3. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  4. Krivushina A.A., Goryashnik Yu.S. Sposoby zashchity materialov i izdeliy ot mikrobiologicheskogo porazheniya (obzor) [Ways of protection of materials and products from microbiological damage (review)] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 80–86. DOI: 10.18577/2071-9140-2017-0-2-80-86.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Polyakova A.V., Krivushina A.A., Goryashnik Yu.S., Buharev G.M. Ispytaniya na mikrobiologicheskuyu stojkost v naturnyh usloviyah razlichnyh klimaticheskih zon [Microbiological resistance tests under nature conditions in variety of climatiс zones] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4. St. 11. Available at: http://www.viam-works.ru (accessed: March 25, 2019). DOI: 10.18577/2307-6046-2016-0-4-11-11.
  7. Romanov M.S., Zolkin S.Yu., Kolomeytseva G.L. Istoriya i dinamika komplektovaniya fondovoy oranzherei Glavnogo botanicheskogo sada im. N.V. Tsitsina RAN [The history and dynamics of stock picking greenhouses of the Main Botanical Gardens them. N.V. Tsitsina RAS] // Byulleten Glavnogo botanicheskogo sada. 2015. №2 (201). S. 23–36.
  8. Dudka I.A., Vasser S.P., Ellanskaya I.A i dr. Metody eksperimentalnoy mikologii: spravochnik / pod red. V.I. Bilay [Methods of Experimental Mycology: handbook]. Kiyev: Naukova dumka, 1982. S. 432–460.
  9. Raper K.B., Fennell D.I. The genus Aspergillus. Baltimore: The Williams and Wilkins Company, 1965. 686 p.
  10. Raper K.B., Thom C., Fennell D.I. A Manual of the Penicillia. New York–London: Hafner Publishing Company, 1968. 875 p.
  11. Ellis M.V. Dematiaceous hyphomycetes. Kew, Surreg, England, 1971. 608 p.
  12. Gams W., Holubova-Jechova V. Chloridium and some other Dematiaceous Hyphomycetes growing on decaying wood // Studies in Mycology. 1976. No. 13. P. 59–71.
  13. Domsch K.H., Gams W., Anderson T.H. Compendium of Soil Fungi. London: Academic Press, 1980. Vol. 1, 2. 1264 p.
  14. Domsch K.H., Gams W., Anderson T.H. Compendium of Soil Fungi. 2nd ed. Lubrecht & Cramer Ltd, 2007. 672 p.
  15. Lugauskas A.Yu., Mikulskene A.I., Shlyauzhene D.Yu. Katalog mikromitsetov – biodestruktorov polimernykh materialov [Catalog of micromycetes – biodestructors of polymeric materials]. M: Nauka, 1987. S. 258–259.
  16. Watanabe T. Pictorial Atlas of soil and seed fungi: morphologies of cultured fungi and key to species. Boca Raton-Ann Arbor-London-Tokyo: Lewis publishers, 1994. 411 p.
  17. De Hoog G.S., Guarro J., Gene J., Figueras M.J. Atlas of clinical fungi. CBS, Utrecht; Universitat Rovira i Virgili Reus, 2000. 1126 p.
  18. GOST 9.049–91. Edinaya sistema zashchity ot korrozii i stareniya (ESZKS). Materialy polimernyye i ikh komponenty. Metody laboratornykh ispytaniy na stoykost k vozdeystviyu plesnevykh gribov [State Standard 9.049–91. Uniform system of protection against corrosion and aging (EUPCA). Polymer materials and their components. Laboratory test methods for resistance to mold fungi]. M.: Izd-vo standartov, 1994. 15 s.
  19. GOST 9.048–89. Edinaya sistema zashchity ot korrozii i stareniya (ESZKS). Izdeliya tekhnicheskiye. Metody laboratornykh ispytaniy na stoykost k vozdeystviyu plesnevykh gribov [State Standard 9.048–89. Uniform system of protection against corrosion and aging (EUPCA). Technical products. Laboratory test methods for resistance to mold fungi]. M.: Izd-vo standartov, 1994. 23 s.
  20. Krivushina A.A., Chekunova L.N., Mokeyeva V.L. Morfologicheskiye osobennosti shtammov «kerosinovogo» griba Hormoconis resinae pri roste v aviatsionnom toplive i na pitatelnykh sredakh [Morphological features of the «kerosene» fungus Hormoconis resinae with growth in aviation fuel and in nutrient media] // Mikologiya i fitopatologiya. 2019. №1. S. 23–32.
  21. GOST 9.023–74. Edinaya sistema zashchity ot korrozii i stareniya (ESZKS). Topliva neftyanyye. Metod laboratornykh ispytaniy biostoykosti topliv, zashchishchennykh protivomikrobnymi prisadkami [State Standard 9.023–74. Uniform system of protection against corrosion and aging (EUPCA). Fuel oil. Laboratory test method for biostability of fuels protected by antimicrobial additives]. M.: Izd-vo standartov, 1994. 9 s.