Climatic tests of paint coating based on fluoroplastic and features of its destruction

Pavlov A.V., Andreeva N.P., Pavlov M.R., Merkulova Yu.I.
Pavlov A.V., Andreeva N.P., Pavlov M.R., Merkulova Yu.I. Climatic tests of paint coating based on fluoroplastic and features of its destruction // Proceedings of VIAM. 2019. No. 5. DOI: 10.18577/2307-6046-2019-0-5-103-110. URL: https://viam-works.ru/en/journal/2019/5/12
Keywords
paint and varnish coatings, paintwork materials, climatic tests, infrared spectroscopy, fluoroplastics.
Abstract

The article presents the main results of the climatic tests of the coating based on the fluoroplastic and developed in the FSUE “VIAM”. It is shown that this coating has a high resistance to the effects of a tropical humid climate for a period of at least two years without changing the protective properties. The exposition was held at climate stations of the Republic of Vietnam (Hoa Lac and Dam Bay stations) and also on the Russian climate station (Gelendzhik). Using FTIR-spectroscopy, it was found that in the process of coating destruction, the fluoroplastic component decreases.

Reference list
  1. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  2. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  3. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk, 2012. T. 82. №6. S. 520–530.
  4. Andreeva N.P., Pavlov M.R., Nikolaev E.V., Slavin A.V. Vliyaniye klimaticheskikh faktorov tropicheskogo i umerennogo klimata na svoystva lakokrasochnykh pokrytiy na uretanovoy osnove [Influence of climatic factors of tropical and temperate climate on the properties of urethane-based paint and varnish coatings] // Lakokrasochnyye materialy i ikh primeneniye. 2018. №4. S. 24–28.
  5. Kablov E.N., Semenova L.V., Yeskov A.A., Lebedeva T.A. Kompleksnyye sistemy lakokrasochnykh pokrytiy dlya zashchity metallicheskikh polimernykh kompozitsionnykh materialov, a takzhe ikh kontaktnykh soyedineniy ot vozdeystviya agressivnykh faktorov [Complex systems of paint and varnish coatings for the protection of metal polymer composites, as well as their contact compounds from the effects of aggressive factors] // Lakokrasochnyye materialy i ikh primeneniye. 2016. №6. S. 32–35.
  6. Pavlov A.V., Merkulova Yu.I., Zelenskaya A.D., Zheleznyak V.G. Iznosostoykost lakokrasochnykh pokrytiy [Wear resistance of paint coatings] // Lakokrasochnyye materialy i ikh primeneniye. 2018. №1–2. S. 40–43.
  7. Zelenskaya A.D., Fedyakova N.V. Epoksidnaya antistaticheskaya benzostoykaya grunt-emal dlya vnutrenney okraski neftetransporta [Epoxy antistatic petrol-resistant primer-enamel for internal painting of oil transport] // Mnogofunktsionalnyye lakokrasochnyye pokrytiya: materialy Vseros. nauch.-tekhnich. konf. (g. Moskva, 6 dek. 2018 g.) M.: VIAM, 2018. S. 122–127.
  8. Malova N.E., Kondrashov E.K., Vereninova N.P., Kozlova A.A. Termostoykaya atmosferostoykaya ftorpoliuretanovaya emal [Heat-resistant weatherproof fluoride polyurethane enamel] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 28–30. DOI: 10.18577/2071-9140-2014-0-S3-28-30.
  9. Semenova L.V., Novikova T.A., Nefedov N.I. Klimaticheskaya stojkost i starenie lakokrasochnogo pokrytiya [Climatic stability and ageing paint coating] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 31–34. DOI: 10.18577/2071-9140-2017-0-s3-31-34.
  10. Voytovich V.A. Lakokrasochnyye materialy s ftorirovannymi komponentami [Paintwork materials with fluorinated components] // Promyshlennaya okraska. 2013. №4. S. 23–27.
  11. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Lakokrasochnye pokrytiya dlya zashhity metallicheskih i polimernyh kompozicionnyh materialov ot stareniya, korrozii i biopovrezhdeniya [Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration] // Aviacionnye materialy i tehnologii. 2017. №S. S. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  12. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Sistemy lakokrasochnyh pokrytij dlya vertoletnoj tehniki [Systems of paint coatings for helicopter equipment] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  13. Nikolayev E.V., Pavlov M.R., Andreyeva N.P., Slavin A.V., Skirta A.A. Issledovaniye protsessov stareniya polimernykh kompozitsionnykh materialov v naturnykh usloviyakh tropicheskogo klimata Severnoy Ameriki [Investigation of the aging processes of polymeric composite materials in natural conditions of tropical climate of North America] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №3–4 (30). St. 08. Available at: http://www.materialsnews.ru (accessed: April 30, 2019).
  14. Karyakina M.I. Fiziko-khimicheskiye osnovy protsessov formirovaniya i stareniya pokrytiya [Physico-chemical bases of the processes of formation and aging of the coating]. M.: Khimiya, 1980. 216 s.
  15. Prech E., Byulmann F., Affolter K. Opredeleniye stroyeniya organicheskikh soyedineniy. Tablitsy spektralnykh dannykh. Per. s angl. [Determination of the structure of organic compounds. Spectral data tables. Line from Engl.]. M.: Mir, 2006. 438 s.