Fractographic study of Co–Cr–Ni–W–Ta alloy samples obtained by selective laser melting
UDC
620.187:669.017.165
DOI
10.18577/2307-6046-2019-0-4-3-10
Article PDF (Russian)
(312.54 KB)
How to cite
Aslanyan G.G., Sukhov D.I., Mazalov P.B., Sulyanova E.A. Fractographic study of Co–Cr–Ni–W–Ta alloy samples obtained by selective laser melting // Proceedings of VIAM. 2019. No. 4. DOI: 10.18577/2307-6046-2019-0-4-3-10. URL: https://viam-works.ru/en/journal/2019/4/1
Keywords
cobalt alloy, selective laser melting, long-term strength, destruction, fracture, growth.
Abstract
Fractographic investigation of Co–Cr–Ni–W–Ta alloy samples obtained by selective laser melting and having horizontal and vertical orientation on a build platform is performed. The samples underwent hot isostatic pressing. The microstructure near the fractures was investigated and type of destruction and porosity were determined. The dependence of the samples orientation on their rupture character is investigated. All samples exhibit viscous rupture during long-term strength test.
Reference list
- Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and technologies of VIAM for «Aviadvigatel»] // Permskiye aviatsionnyye dvigateli. 2014. №31. S. 43–47.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.Ye., Kablov D.Ye. Osobennosti tekhnologii vyplavki i razlivki sovremennykh liteynykh vysokozharoprochnykh nikelevykh splavov [Features of the technology of smelting and casting of modern foundry high-heat resistant nickel alloys] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2011. №SP2. S. 68–78.
- Kablov E.N., Tolorajya V.N. VIAM – osnovopolozhnik otechestvennoj tehnologii litya monokristallicheskih turbinnyh lopatok GTD i GTU [VIAM – the founder of domestic casting technology of single-crystal turbine blades of GTE and GTU] // Aviacionnye materialy i tehnologii. 2012. №S. S. 105–117.
- Kablov E.N. Razrabotki VIAM dlya gazoturbinnykh dvigateley i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
- Kablov E.N., Sidorov V.V., Rigin V.E. Metallurgiya liteynykh zharoprochnykh splavov [Metallurgy of casting superalloys] // 75 let. Aviacionnye materialy. Izbrannyye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 125–132.
- Kishkin S.T., Kablov E.N. Liteynyye zharoprochnyye splavy dlya turbinnykh lopatok [Foundry superalloys for turbine blades] // Aviacionnye materialy. Izbrannyye trudy «VIAM» 1932–2002. M.: VIAM, 2002. S. 48–58.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Liteynyye zharoprochnyye splavy novogo pokoleniya [Foundry superalloys of a new generation] // 75 let. Aviacionnye materialy. Izbrannyye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 27–44.
- Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
- Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing – the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
- Hagedorn Y.-C., Risse T., Meiners W. et al. Processing of Nickel Based Superalloy MAR M-247 by means of High Temperature – Selective Laser Melting (HT-SLM) // High Value Manufacturing. 2014. P. 291–295. DOI: 10.1201/b15961-54.
- Marchese G., Basila G., Bassini E. et al. Study of the Microstructure and Cracking Mechanism of Hastelloy X Produced by Laser Powder Bed Fusion // Materials. 2018. Vol. 11. P. 106–118. DOI: 10.3390/ma11010106.
- Petrushin N.V., Evgenov A.G., Zavodov A.V., Treninkov I.A. Struktura i prochnost' zharoprochnogo nikelevogo splava ZhS32-VI, poluchennogo metodom selektivnogo lazernogo splavleniya na monokristallicheskoy podlozhke [The structure and strength of the ZS32-VI heat-resistant nickel alloy obtained by the method of selective laser alloying on a single-crystal substrate] // Materialovedeniye. 2017. №11. S. 19–26.
- 3D Printing Industry. Available at: http://3dprintingindustry.com/news/general-electrics-ge9x-engine-undergoes-testing-3d-printed-components-104180/ (accessed: February 27, 2019).
- Evgenov A.G., Lukina E.A., Aslanyan I.R. Struktura i svoystva splavov na osnove nikelya, poluchennykh metodom SLS [Structure and properties of nickel-based alloys obtained by the SLS method] // Additivnyye tekhnologii: nastoyashcheye i budushcheye: mater. II Mezhdunar. konf. M.: VIAM, 2016. St. 1 (CD).
- Ovsepyan S.V., Akhmedzyanov M.V., Mazalov I.S., Rastorguyeva O.I. Legirovaniye uglerodom splava sistemy Ni–Co–Cr–W–Ti, uprochnyayemogo khimiko-termicheskoy obrabotkoy [Alloying by carbon of superalloy of the Ni–Co–Cr–W–Ti system strengthened by thermo-chemical treatment] // Aviaconnye materialy i tehnologii. 2015. №4 (37). S. 21–24. DOI: 10.18577/2071-9140-2015-0-4-21-24.
- Karpov I.D., Em V.T., Mazalov P.B., Sulyanova E.A. Characterisation of residual stresses by neutron diffraction at the research reactor IR-8 of NRC «Kurchatov Institute» // Journal of Phisics Conference Series. November, 2018. 1109: SP012046. DOI: 10.1088/1742-6596/1109/1/012046.
- Wei H.L., Mazumder J., DebRoy T. Evolution of solidification texture during additive manufacturing // Scientific Reports. 2015. Vol. 5. Art. No. 16446. DOI: 10.1038/srep16446.
- Treninkov I.A., Filonova E.V., Medvedev P.N., Lukina E.A. Zakonomernosti formirovaniya tekstury i mikrotekstury v zharoprochnom nikelevom splave v protsesse selektivnogo lazernogo splavleniya [Texture and microstructure formation in the nickel-base superalloy during selective laser melting] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2018. №1–2. St. 02. Available at: http://viam-works.ru (accessed: February 27, 2019).