Effect of sintering additives on the properties of silicon carbide-based ceramics (review)

Zhitnyuk S.V.
Zhitnyuk S.V. Effect of sintering additives on the properties of silicon carbide-based ceramics (review) // Proceedings of VIAM. 2019. No. 3. DOI: 10.18577/2307-6046-2019-0-3-79-86. URL: https://viam-works.ru/en/journal/2019/3/9
Keywords
silicon carbide, sintering additives, liquid-phase sintering, hot pressing, microstructure, mechanical properties, thermal conductivity.
Abstract

Silicon carbide has a number of unique physical and chemical properties. Studies in the field of silicon carbide-based materials densification in the synthesis process have shown that a promising method of consolidation is liquid-phase sintering with the additives of different composition, contributing to reduction of the synthesis temperature to 1850°C, intensification of diffusion processes, filling of intergranular pores and restructuring of silicon carbide grains. In this paper the modern approaches to modification of silicon carbide-based ceramics with the additives of different composition are considered.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Folomeykin Yu.I., Stolyarova V.L., Lopatin S.I. Protsessy vzaimodeystviya niobiy-kremniyevogo rasplava s ogneupornoy keramikoy [Interaction processes of niobium-silicon melt with refractory ceramics] // Zhurnal obshchey khimii. 2016. T. 86. №9. S. 1542–1546.
  3. Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh sistem [The role of chemistry in the creation of a new generation of materials for complex technical systems] // Tez. dokl. XX Mendeleyevskogo syezda po obshchey i prikladnoy khimii. UrO RAN, 2016. S. 25–26.
  4. Kablov E.N., Zhestkov B.E., Grashchenkov D.V., Sorokin O.Yu., Lebedeva Yu.E., Vaganova M.L. Issledovaniye okislitel'noy stoykosti vysokotemperaturnogo pokrytiya na SiC-materiale pod vozdeystviyem vysokoental'piynogo potoka [Investigation of the oxidative stability of a high-temperature coating on a SiC material under the influence of a high-enthalpy flow] // Teplofizika vysokikh temperatur. 2017. T. 55. №6. S. 704–711.
  5. Zhitnyuk S.V. Keramika na osnove karbida kremniya, modifitsirovannaya dobavkami evtekticheskogo sostava: dis. … kand. tekhn. nauk [Ceramics based on silicon carbide, modified additives eutectic composition: thesis, Cand. Sc. (Tech.)]. M.: RKhTU im. D.I. Mendeleyeva, 2014. 174 s.
  6. Berezovskij V.V., Shavnev A.A., Lomov S.B., Kurganova Yu.A. Poluchenie i analiz struktury dispersno-uprochnennyh kompozicionnyh materialov sistemy Al–SiC s razlichnym soderzhaniem armiruyushhej fazy [Receiving and the analysis of structure of the disperse strengthened composite materials of Al–SiC system with the different maintenance of the reinforcing phase] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 17–23. DOI: 10.185577/2071-9140-2014-0-S6-17-23.
  7. Sorokin O.Yu., Solntsev S.St., Evdokimov S.A., Osin I.V. Metod gibridnogo iskrovogo plazmennogo spekaniya: princip, vozmozhnosti, perspektivy primeneniya [Hybrid spark plasma sintering method: principle, possibilities, future prospects] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 11–16. DOI: 10.18577/2071-9140-2014-0-s6-11-16.
  8. Grishina O.I., Shavnev A.A., Serpova V.M. Osobennosti vliyaniya strukturnyh parametrov na mehanicheskie harakteristiki metallicheskogo kompozicionnogo materiala na osnove alyuminievyh splavov, uprochnennyh chasticami karbida kremniya (obzor) [Features of influence of structural parameters on mechanical properties of metallic composite material based on particle-reinforced aluminum alloys by silicon carbide] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 24–27. DOI: 10.18577/2071-9140-2014-0-s6-24-27.
  9. Kurbatkina E.I., Kosolapov D.V., Hodykin L.G., Nigmetov M.S. Issledovanie vliyaniya dobavki kremniya na fazovyj sostav alyuminievyh kompozicionnyh materialov, armirovannyh chasticami karbida kremniya [Influence of the silicon addition on the phase composition of aluminum composite materials reinforced with silicone carbide particles] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 35–38. DOI: 10.18577/2071-9140-2014-0-s6-35-38.
  10. Fides M., Kovalcikova A., Hvizdos P. et al. Mechanical and tribological properties of electrically conductive SiC based cermets // International Journal of Refractory Metals and Hard Materials. 2017. No. 65. P. 76–82.
  11. Lee K.N. Current status of environmental barrier coatings for Si-based ceramics // Surface and Coatings Technology. 2000. No. 133. P. 1–7.
  12. Jianxin D., Lili L., Jianfeng L. et al. Development of SiC/(W, Ti)C gradient ceramic nozzle materials for sand blasting surface treatments // International Journal of Refractory Metals and Hard Materials. 2007. No. 25. P. 130–137.
  13. Gupta S., Sharma S.K., Kumar B.V.M., Kim Y.-W. Tribological characteristics of SiC ceramics sintered with a small amount of yttria // Ceramics International. 2015. No. 41. P. 14780–14789.
  14. Ji R., Liu Y., Zhang Y., Wang F. Machining performance of silicon carbide ceramic in end electric discharge milling // International Journal of Refractory Metals and Hard Materials. 2011. No. 29. P. 117–122.
  15. Jianxin D., Lili L., Jinlong Z., Junlong S. Erosion wear of laminated ceramic nozzles // International Journal of Refractory Metals and Hard Materials. 2007. No. 25. P. 263–270.
  16. Sharma S.K., Kumar B.V.M., Kim Y.-W. Tribological behavior of silicon carbide ceramics – a review // Journal of the Korean Ceramic Society. 2016. No. 53. P. 581–596.
  17. Mettyuz F., Rolings R. Kompozitsionnyye materialy. Mekhanika i tekhnologiya. Per. s angl. [Composite materials. Mechanics and technology. Trans. from Engl.]. M.: Tekhnosfera, 2004. 408 s.
  18. Low I.M., Sakka Y., Hu C.F. MAX phases and ultra–high temperature ceramics for extreme environments // Engineering Science Reference. 2013. 649 p.
  19. Heimann R.B. Classic and Advanced Ceramics: From Fundamentals to Applications. Weinheim: WILEY-VCH Verlag GmbH & Co. KGaA, 2010. 553 p.
  20. Perevislov S.N. Rol modifikatsii struktury spechennykh i goryachepresovannykh SiC-materialov [The role of modifying the structure of sintered and hot pressed SiC materials] // Ogneupory i tekhnicheskaya keramika. 2018. №10. S. 18–24.
  21. Jang S.H., Kim Y.-W., Kim K.J. Electrical and thermal properties of SiC–Zr2CN composites sintered with Y2O3–Sc2O3 additives // Journal of the European Ceramic Society. 2017. Vol. 37. P. 477–484.
  22. Balkevich V.L. Tekhnicheskaya keramika [Technical ceramics]. M.: Stroyizdat, 1984. 256 s.
  23. Omori M., Takei H. Preparation of Pressureless Sintered SiC–Y2O3–Al2O3 // Journal of Materials Science. 1988. No. 23. P. 3744–3749.
  24. Zhou Y., Hirao K., Toriyama M. et al. Effects of Intergranular Phase Chemistry on the Microstructure and Mechanical Properties of Silicon Carbide Ceramics Densified with Rare–Earth Oxide and Alumina Additives // Journal of the American Ceramic Society. 2001. Vol. 84. No. 7. P. 1642.
  25. Liu D.-M. Oxidation of Polycrystalline–Silicon Carbide Ceramic // Ceramics International. 1997. Vol. 23. No. 5. P. 425.
  26. Dijen F.K., Mayer E. Liquid Phase Sintering of Silicon Carbide // Journal of the European Ceramic Society. 1996. No. 16. P. 413–420.
  27. Iwata H.P., Lindefelt U., Oberg S., Briddon P.R. Stacking faults in silicon carbide // Physica B Condensed Matter. 2003. Vol. 340–342. P. 165–170.
  28. Kim Y.-W., Cho T.Y., Kim K.J. Effect of grain growth on electrical properties of silicon carbide ceramics sintered with gadolinia and yttria // Journal of the European Ceramic Society. 2015. No. 35. P. 4137–4142.
  29. Jang S.H., Kim Y.-W., Kim K.J. Electrical and thermal properties of SiC–Zr2CN composites sintered with Y2O3–Sc2O3 additives // Journal of the European Ceramic Society. 2017. No. 37. P. 477–484.
  30. Gu J., Sang L., Pan B. et al. Thermal Conductivity and High–Frequency Dielectric Properties of Pressureless Sintered SiC–AlN Multiphase Ceramics // Materials. 2018. No. 11 (6). P. 969.
  31. Virkar A.V., Jackson T.B., Culter R.A. Thermodynamic and kinetic effects of oxygen removal on the thermal conductivity of aluminum nitride // Journal of the American Ceramic Society. 1989. No. 72. P. 2031–2042.
  32. Nakano H., Watari K., Kinemuchi Y. et al. Microstructural characterization of high–thermal–conductivity SiC ceramics // Journal of the European Ceramic Society. 2004. No. 24. P. 3685–3690.
  33. Kim Y.-H., Kim Y.-W., Lim K.-Y., Lee S.-J. Mechanical and thermal properties of silicon carbide ceramics with yttria–scandia–magnesia // Journal of the European Ceramic Society. 2019. Vol. 39 (2–3). P. 144–149.