Predictions of first-year corrosion losses of structural metals depending on the orientation of samples at different distances from the seashore

Panchenko Yu.M., Marshakov A.I., Nenasheva T.A., Kutyrev A.E., Fomina M.A., Vdovin A.I.
Panchenko Yu.M., Marshakov A.I., Nenasheva T.A., Kutyrev A.E., Fomina M.A., Vdovin A.I. Predictions of first-year corrosion losses of structural metals depending on the orientation of samples at different distances from the seashore // Proceedings of VIAM. 2024. No. 6. DOI: 10.18577/2307-6046-2024-0-6-92-104. URL: https://viam-works.ru/en/journal/2024/6/9
Keywords
atmospheric corrosion, structural metals, corrosive aggressiveness, dose-response functions, chloride deposition rate, orientation of samples, distance from shore, salinity
Abstract

An anomalously high rate of chloride deposition observed in Gelendzhik in February 2023 during the annual corrosion tests was investigated. An estimation of the threshold value of the chloride deposition rate on samplers corresponding to the rate of chloride deposition directly on the surface of metal samples is given. The correction of calculation of the average annual rate of chloride deposition ([Cl]) under anomalously high salinity of the atmosphere is proposed. Based on the average annual climatic parameters and [Cl] by dose-response functions the forecast of first-year corrosion losses of metals is made.

Reference list
  1. Startsev V.O., Slavin A.V., Nikolaev E.V. Study of the content of aggressive ions in the atmosphere and sea water of the Gelendzhik bay. Trudy VIAM, 2020, no. 10 (92), paper no. 12. Available at: http://www.viam-works.ru (accessed: March 26, 2024). DOI: 10.18577/2307-6046-2020-0-10-106-115.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the coastal atmosphere. Part 2. New approaches to assessing the corrosivity of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1–15.
  3. Knotkova D., Kreislova K., Dean S.W. ISOCORRAG International Atmospheric Exposure Program: Summary of Results. West Conshohocken: ASTM International, 2010, 112 p.
  4. Morcillo M. Atmospheric corrosion in Ibero-America. The MICAT project. Atmospheric corrosion. Eds. W.W. Kirk, H.H. Lawson. Philadelphia: American Society for Testing and Materials, 1995. ASTM STP 1239, рр. 257–275. DOI: 10.1520/STP14924S.
  5. Chico B., de la Fuente D., Díaz I. et al. Annual atmospheric corrosion of carbon steel worldwide. An integration of ISOCORRAG, ICP/UNECE and MICAT databases. Materials, 2017, no. 10 (6), p. 601. DOI: 10.3390/ma10060601.
  6. Morcillo M., Chico B., Otero E., Mariaca L. Effect of marine aerosol on atmospheric corrosion. Materials Performance, 1999, no. 38, pp. 72–77.
  7. Alcántara J., Chico B., Díaz I. et al. Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel. Corrosion Science, 2015, no. 97, pp. 74–88. DOI: 10.1016/j.corsci.2015.04.015.
  8. Castañeda A., Corvo F., Fernández D., Valdés C. Outdoor-indoor atmospheric corrosion in a coastal wind farm located in a tropical island. Engineering Journal, 2017, no. 21 (2), pp. 43–62. DOI: 10.4186/ej.2017.21.2.43.
  9. Morcillo M., Chico B., Alcantara J. et al. Atmospheric corrosion of mild steel in chloride‐rich environments. Questions to be answered Materials and Corrosion, 2015, no. 66 (9), pp. 882–892. DOI: 10.1002/maco.201407940.
  10. Franzen L.G. Transport, deposition and distribution of marine aerosols over southern Sweden during dry westerly storms. AMBIO, 1990, no. 19 (4), pp. 180–188.
  11. State Standard 9.107–2023. Unified system of protection against corrosion and aging. Corrosive aggressiveness of the atmosphere. Basic provisions. Moscow: RST, 2023, pp. 6–8.
  12. Panchenko Yu.M., Marshakov A.I., Igonin T.N. et al. Corrosion resistance of zinc and zinc-aluminum-magnesium coatings in atmosphere on the territory of Russia. Materials, 2023, no. 16, pp. 2–17. DOI: 10.3390/ma16155214.
  13. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  14. ISO 9225–2012. Corrosion of metals and alloys – Corrosivity of atmospheres – Measurement of environmental parameters affecting corrosivity of atmospheres. Geneva: International Standards Organization, 2012, 12 р.
  15. Panchenko Yu., Marshakov A., Nikolaeva L., Igonin T. Corrosion resistance of structural metals depending on the sample orientation and initial exposure conditions in coastal and rural atmospheres. Part 1. Corrosivity toward structural metals at coastal and rural test sites under various exposure conditions. Corrosion Engineering, Science and Technology, 2023, no. 58 (7), pp. 645–658. DOI: 10.1080/1478422X.2023.2245642.
  16. Panchenko Yu.M., Marshakov A.I., Nenasheva T.A., Igonin T.N., Kutyrev A.E., Fomina M.A., Vdovin A.I. Corrosion resistance of structural metals depending on the orientation of samples at various distances from the seashore. Korroziya: zashchita materialov i metody issledovaniy, 2024, no. 2, pp. 29–44. DOI: 10.61852/2949-3412-2024-2-2-29-44.
  17. Diaz I., Cano H., de la Fuente D. et al. Atmospheric corrosion of Ni-advanced weathering steels in marine atmospheres of moderate salinity. Corrosion Science, 2013, no. 76, pp. 348–360. DOI: 10.1016/j.corsci.2013.06.053.
  18. Abramova M.G., Panchenko Yu.M., Vetrova E.Yu., Nenasheva T.A. Corrosive aggressiveness of the atmosphere in various climatic regions of the Russian Federation. Korroziya: materialy, zashchita, 2020, no. 3, pp. 12–22. DOI: 10.31044/1813-7016-2020-0-3-12-22.
  19. Vera R., Rosales B.M., Tapia C. Effect of the exposure angle in the corrosion rate of plain carbon steel in a marine atmosphere. Corrosion Science, 2003, no. 45, pp. 321–337.
  20. Alcаntara J., de la Fuente D., Chico B. et al. Marine atmospheric corrosion of carbon steel: A review. Materials, 2017, no. 10, p. 406. DOI: 10.3390/ma10040406.
  21. Zezza F., Macrì F. Marine aerosol and stone decay. Science of Total Environment, 1995, no. 167, pp. 23–143. DOI: 10.1016/0048-9697(95)04575-L.
  22. Whitby K.T. The physical characteristics of sulfate aerosols. Atmospheric Environment, 1978, no. 12, рр. 135–159. DOI: 10.1016/0004-6981(78)90196-8.
  23. Li S., Hihara L.H. Aerosol salt particle deposition of metals exposed to marine environments: A study related to marine atmospheric corrosion. Journal of electrochemical society, 2014, no. 161, pp. 268–275. DOI: 10.1149/2.071405jes.
  24. Varchenko E.А., Vetrova E.Yu. Research of the biological and corrosion resistance of samples of aluminum alloy after natural tests in the Gelenjik bay. Part 1. Trudy VIAM, 2020, no. 6–7 (89), paper no. 10. Available at: http://www.viam-works.ru (accessed: March 06, 2024). DOI: 10.18577/2307-6046-2020-0-67-91-100.
  25. Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
  26. Jaen J.A., Iglesias J., Hernandez C. Analysis of Short-Term Steel Corrosion Products Formed in Tropical Marine Environments of Panama. International Journal of Corrosion, 2012, vol. 2012, art. ID 162729. DOI: 10.1155/2012/162729.