Investigation of fiberglass properties based on the melt binder VSE-1212 for radio engineering purposes

Gamazina A.V., Kurnosov A.O., Vavilova M.I., Kochetov N.R.
Gamazina A.V., Kurnosov A.O., Vavilova M.I., Kochetov N.R. Investigation of fiberglass properties based on the melt binder VSE-1212 for radio engineering purposes // Proceedings of VIAM. 2024. No. 12. DOI: 10.18577/2307-6046-2024-0-12-56-65. URL: https://viam-works.ru/en/journal/2024/12/5
Keywords
polymer composite materials, quartz fiber, molten epoxy binder, vacuum autoclave molding, fiberglass, elastic-strength characteristics, dielectric characteristics
Abstract

The properties of various types of glass filler are considered. The main characteristics of a molten epoxy binder VSE-1212 are described. Studies of the wettability of quartz filler fibers are presented. Fiberglass samples were examined by ultrasonic inspection. The results of the physico-mechanical and dielectric characteristics of fiberglass of the VPS-48/7781-14 are presented. The results of the research of the developed fiberglass for radio engineering purposes based on quartz filler and molten epoxy binder VSE-1212 are presented.

Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Getman A.A. Main directions of development of materials science for the creation of new technology. Armaturostroenie, 2021, no. 4 (133), pp. 48–51.
  3. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  4. Kablov E.N. Main results and directions of development of materials for advanced aviation technology. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
  5. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-s-344-348.
  6. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Shershak P.V., Yakovlev N.O., Sutubalov A.I. Standards for testing polymer composite materials. Part 1. Tensile properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 12. Available at: http://www.journal.viam.ru (accessed: May 29, 2024). DOI: 10.18577/2713-0193-2023-0-3-152-166.
  8. Gutnikov S.I., Lazoryak B.I., Seleznev A.N. Glass fibers: textbook. Moscow: Moscow State Univ., 2010, 53 p.
  9. Bataev A.A., Bataev V.A. Composite materials. Moscow: Logos, 2006, 400 p.
  10. Vavilova M.I., Kavun N.S. The properties of glass filler for constructions of fiberglass. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 33–37. DOI: 10.18577/2071-9140-2014-0-3-33-37.
  11. Borodulin A.S. Properties and features of the structures of glass fibers used for the production of fiberglass. Materialovedenie, 2012, no. 7, pp. 34–37.
  12. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technologies, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: July 01, 2024). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  13. Burov A.K., Andreevskaya G.D. High-strength fiberglass: textbook. Moscow: Publ. House of the USSR Academy of Sciences, 1958, 72 p.
  14. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composite materials: textbook. Ed. E.N. Kablov. Moscow: National Research Center «Kurchatov Institute» – VIAM, 2021, 528 p.
  15. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: May 17, 2024). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  16. Tkachuk A.I., Gurevich Ya.M., Guseva M.A., Mishurov K.S. Technological and operational characteristics and areas of application of the epoxy binder VSE-1212, processed using prepreg technology. Klei. Germetiki. Tekhnologii, 2018, no. 4, pp. 29–34.
  17. Zagora A.G., Tkachuk A.I., Terekhov I.V., Mukhametov R.R. Methods of chemical modification of epoxy oligomers (review). Trudy VIAM, 2021, no. 7 (101), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 17, 2024). DOI: 10.18577/2307-6064-2021-0-7-73-85.
  18. Doroshenko Yu.E., Lebedeva E.D. Binders for composite materials. Moscow: Mendeleyev Univ. of Chemical Technology of Russia, 2003, 56 с.