Some technological features of manufacturing polymer composite materials by non-autoclave molding of prepregs

Tkachuk A.I., Kuznetcova P.A., Donetskiy K.I., Karavaev R.Y.
Tkachuk A.I., Kuznetcova P.A., Donetskiy K.I., Karavaev R.Y. Some technological features of manufacturing polymer composite materials by non-autoclave molding of prepregs // Proceedings of VIAM. 2024. No. 12. DOI: 10.18577/2307-6046-2024-0-12-44-55. URL: https://viam-works.ru/en/journal/2024/12/4
Keywords
vacuum forming, prepreg, semipreg, binder, technological package, vacuuming, impregnation, polymer composite materials
Abstract

The processing of polymer composite materials by methods of non-autoclave molding is increasingly used in the manufacture of products for a wide variety of applications. To carry out the process of manufacturing the material and obtaining its maximum properties, it is necessary to use technological processes that ensure the manufacture of materials with predictable and optimal properties. The review is devoted to the technological features of the manufacture of polymer composite materials by non-autoclave molding of prepregs.

Reference list
  1. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Kablov E.N. The role of fundamental research in creating new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  4. Varvani-Farahani A. Composite materials: characterization, fabrication and application-research challenges and directions. Applied Composite Materials, 2010, vol. 17, is. 2, pp. 63–67.
  5. Lachaud F., Espinosa C., Michel L. et al. Modelling strategies for predicting the residual strength of impacted composite aircraft fuselages. Applied Composite Materials, 2015, vol. 22, is. 6, pp. 599–621.
  6. Alderliesten R.C. Critical review on the assessment of fatigue and fracture in composite materials and structures. Engineering Failure Analysis, 2013, vol. 35, is. 15, pp. 370–379.
  7. Grunenfelder L.K., Dills A., Centea T., Nutt S.R. Effect of prepreg format on defect control in out-of-autoclave processing. Composites. Part A: Applied Science and Manufacturing, 2017, vol. 93, pp. 88–99.
  8. Aleksendri D., Carlone P., Сiroviс V. Optimization of the temperature-time curve for the curing process of thermoset matrix composites. Applied Composite Materials, 2016, vol. 23, is. 5, pp. 1047–1063.
  9. Bodaghi M., Cristоvаo C., Gomes R., Correia N.C. Experimental characterization of voids in high fibre volume fraction composites processed by high injection pressure RTM. Composites. Part A: Applied Science and Manufacturing, 2016, vol. 82, pp. 88–99.
  10. Marsh G. De-autoclaving prepreg processing. Plast Reinforced plastics, 2012, vol. 56, is. 5, pp. 20–25.
  11. Xu X., Wang X., Liu W. et al. Microwave curing of carbon fiber/bismaleimide composite laminates: material characterization and hot-pressing pretreatment. Materials and Design, 2016, vol. 97, is. 5, pp. 316–323.
  12. Grunenfelder L.K., Nutt S.R. Void formation in composite prepregs – effect of dissolved moisture. Composites Science and Technology, 2010, vol. 70, is. 16, pp. 2304–2309.
  13. Helmus R., Centea T., Hubert P., Hinterhölzl R. Out-of-autoclave prepreg consolidation: coupled air evacuation and prepreg impregnation modeling. Journal of Composite Materials, 2015, vol. 50, is. 10, pp. 1403–1413.
  14. Garschke C., Weimer C., Parlevlie P.P., Fox B.L. Out-of-autoclave cure cycle study of a resin film infusion process using in situ process monitoring. Composites. Part A: Applied Science and Manufacturing, 2012, vol. 43, is. 6, pp. 935–944.
  15. Han K., Jiang S., Zhang C., Wang B. Flow modeling and simulation of SCRIMP for composites manufacturing. Composites. Part A: Applied Science and Manufacturing, 2000, vol. 31, is. 1, pp. 79–86.
  16. Li W., Krehl J., Gillespie J.W. et al. Process and performance evaluation of the vacuum-assisted process. Journal of Composite Materials, 2004, vol. 38, is. 20, pp. 1803–1814.
  17. Centea T., Grunenfelder L.K., Nutt S.R. A review of out-of-autoclave prepregs – Material properties, process phenomena, and manufacturing considerations. Composites. Part A: Applied Science and Manufacturing, 2015, vol. 70, pp. 132–154.
  18. Turner T.A., Harper L.T., Warrior N.A., Rudd C.D. Low-cost carbon-fibre-based automotive body panel systems: a performance and manufacturing cost comparison. Proceedings IMechE. Part D: Journal Automobile Engineering, 2006, vol. 222, pp. 53–62.
  19. Murray J.J., Pappa E.J., Mamalis D. et al. Сharacterisation of carbon fibre reinforced powder epoxy composites for wind energy blades. ECCM18: 18th European Conference on Composite Materials. Athens, 2018, art. 5.03-02.
  20. Boyd J., Maskell R.K. Product design for low cost manufacturing of composites for aerospace applications. Proceedings SAMPE conference. California, 2001, pp. 59–90.
  21. Irving P.E., Soutis C. Polymer composites in the aerospace industry. Cambridge: Woodhead Publishing, 2019, 536 p.
  22. Dushin M.I., Donetski K.I., Karavaev R.Y., Korotkov I.A. Some features of liquid formation of polymeric composite materials (review). Trudy VIAM, 2017, no. 2 (50), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 26, 2024). DOI: 10.18577/2307-6046-2017-0-2-8-8.
  23. Karavaev R.Yu., Gorodilova N.A., Donetskiy K.I. Production of polymer composite materials based on semipregs. Trudy VIAM, 2023, no. 5 (123), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2023-0-5-64-74.
  24. Hrulkov A.V., Karavaev R.Yu., Gorodilova N.A., Donetskiy K.I. Some causes of voids formation in polymer composite materials (review). Trudy VIAM, 2023, no. 6 (124), paper no. 07. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2023-0-6-72-86.
  25. Takagaki K., Hisada S., Minakuchi S., Takeda N. Process improvement for out-of-autoclave prepreg curing supported by in-situ strain monitoring. Journal of Composite Materials, 2017, vol. 51, pp. 1225–1237.
  26. Dong A., Zhao Y., Zhao X., Yu Q. Cure Cycle Optimization of Rapidly Cured Out-Of-Autoclave Composites. Materials, 2018, vol. 11, p. 421.
  27. Hubert P., Poursartip A. A review of flow and compaction modelling relevant to thermoset matrix laminate processing. Journal of Reinforced Plastics and Composites, 1998, vol. 17, pp. 286–318.
  28. Ma Y., Centea T., Nutt S.R. Defect reduction strategies for the manufacture of contoured laminates using vacuum BAG-only prepregs. Polymer Composites, 2017, vol. 38, pp. 2016–2025.
  29. Sherwin G.R. Non-autoclave processing of advanced composite repairs. International Journal of Adhesion and Adhesives, 1999, vol. 19, pp. 155–159.
  30. Mujahid Y., Sallih N., Abdullah M.Z. A Comparison of Single-Vacuum-Bag and Double-Vacuum-Bag Methods for Manufacturing High-Quality Laminated Composites. Conference paper «Advances in Manufacturing Engineering». New York: Springer, 2020, pp. 457–467.
  31. Pishvar M., Amirkhosravi M., Altan M.C. Magnet assisted composite manufacturing: A novel fabrication technique for high-quality composite laminates. Polymer Composites, 2019, vol. 40, pp. 159–169.
  32. Amirkhosravi M., Pishvar M., Altan M.C. Improving laminate quality in wet lay-up/vacuum bag processes by magnet assisted composite manufacturing (MACM). Composites. Part A: Applied Science and Manufacturing, 2017, vol. 98, pp. 227–237.
  33. Grunenfelder L.K., Centea T., Hubert P., Nutt S.R. Effect of room-temperature out-time on tow impregnation in an out-of-autoclave prepreg. Composites. Part A: Applied Science and Manufacturing, 2013, vol. 45, pp. 119–126.
  34. Resin composition, a fiber reinforced material having a partially impregnated resin and composites made therefrom: pat. US6139942; appl. 06.02.97; рubl. 31.10.00.
  35. Martinez P., Jin B.C., Nutt S. Droplet Spreading on Unidirectional Fiber Beds. Journal of Composites Science, 2021, vol. 5, pp. 13–15.
  36. Schechter S.G.K., Grunenfelder L.K., Nutt S.R. Air evacuation and resin impregnation in semi-pregs: effects of feature dimensions. Advanced manufacturing: polymer & composites science, 2020, vol. 6, is. 2, pp. 101–114.
  37. Tavares S.S., Michaud V., Månson J.A.E. Through thickness air permeability of prepregs during cure. Composites. Part A: Applied Science and Manufacturing, 2009, vol. 40, pp. 1587–1596.
  38. Edwards W.T., Martinez P., Nutt S.R. Process robustness and defect formation mechanisms in unidirectional semipreg. Advanced Manufacturing: Polymer & Composites Science, 2020, vol. 6, is. 4, pp. 198–211.
  39. Frost M., Solanki D., Mills A. Resin film infusion processing of carbon fibre composite automotive body panels. SAMPE Journal, 2003, vol. 39, is. 4, pp. 44–49.
  40. A kind of phenolic aldehyde panel honeycomb sandwich construction part forming method: pat. CN106608056B; appl. 21.11.16; рubl. 03.05.17.
  41. Ma Y., Centea T., Nutt S.R. Defect reduction strategies for the manufacture of contoured laminates using vacuum BAG-only prepregs. Polymer Composites, 2017, vol. 38, pp. 2016–2025.
  42. Levy A., Hubert P. Vacuum-bagged composite laminate forming processes: Predicting thickness deviation in complex shapes. Composites. Part A: Applied Science and Manufacturing, 2019, vol. 126, p. 105568.
  43. Naji M.I., Hoa S.V. Curing of thick angle-bend thermoset composite part: Curing process modification for uniform thickness and uniform fiber volume fraction distribution. Journal of composite materials, 2000, vol. 34, pp. 1710–1755.
  44. Hubert P., Poursartip A. A review of flow and compaction modelling relevant to thermoset matrix laminate processing. Journal of Reinforced Plastics and Composites, 1998, vol. 17, pp. 286–318.
  45. Gu Y., Li M., Li Y., Zhang Z. Pressure transfer behaviour of rubber mould and the effects on consolidation of L-shape composite laminates. Polymers and Polymer Composites, 2010, vol. 18, pp. 167–174.
  46. Hein R., Prussak R., Schmidt J. Phenomenological Analysis of Thermo-Mechanical-Chemical Properties of GFRP during Curing by Means of Sensor Supported Process Simulation. Processes, 2020, vol. 8, p. 192.
  47. Zappino E., Zobeiry N., Petrolo M. et al. Analysis of process-induced deformations and residual stresses in curved composite parts considering transverse shear stress and thickness stretching. Composite Structures, 2020, vol. 241, p. 112057.
  48. Fiorina M., Seman A., Castanié B. et al. Spring-in prediction for carbon/epoxy aerospace composite structure. Composite Structures, 2017, vol. 168, pp. 739–745.
  49. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2022-0-11-81-92.
  50. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: October 01, 2024). DOI: 10.18577/2713-0193-2021-0-1-22-33.