Protective anticorrosive coating of magnets of the REM–Fe–B system

Dyomin S.A., Zavarzin S.V., Cherednichenko I.V., Kozlov I.A.
Dyomin S.A., Zavarzin S.V., Cherednichenko I.V., Kozlov I.A. Protective anticorrosive coating of magnets of the REM–Fe–B system // Proceedings of VIAM. 2022. No. 6. DOI: 10.18577/2307-6046-2022-0-6-96-107. URL: https://viam-works.ru/en/journal/2022/6/9
Keywords
permanent magnets, rare earth magnets Nd–Fe–B, electrolytic coatings, electroplating, nickel plating, corrosion protection, ion-plasma coatings
Abstract

In the current trends towards saving and increasing the efficiency of electricity use, magnetic materials of the Nd–Fe–B system are widely used in the production of fully electric vehicles: cars (Tesla), aircraft, as well as new energy sources – for example, wind turbines. Considers various methods of applying protective coatings to magnetic materials of the Nd–Fe–B system, surface preparation modes and evaluates the effect of the technology of applying anticorrosive coatings on their protective ability, the magnitude of residual induction and coercive force on the magnetization of magnetic materials.

Reference list
  1. Putsykin G.G., Pashkov P.P., Vejtsel M.Ya. Investigation of the thermophysical conditions for obtaining and the structure of crystalline anisotropic permanent magnets. Fizika metallov i metallovedenie, 1963, vol. 15, is. 4, pp. 118–123.
  2. Savchenko A.G. Nd-Fe-B magnets and promising technologies for their production. Materials of the seminar "Scientific and technological support for the activities of enterprises, institutions and firms". Moscow: MGIU, 2003, pp. 510–546.
  3. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  4. Korolev D.V., Stolyankov Yu.V., Piskorsky V.P., Valeev R.A., Bahmetiev M.V., Dvorezkaya E.V., Koplak O.V., Morgunov R.B. Magnetic properties and magnetic strip domains in micro stripes PrDyFeCoB. Aviation materials and technologies, 2021, no. 3 (64), paper no. 08. Available at: http://www.journal.viam.ru (accessed: September 03, 2022). DOI: 10.18577/2713-0193-2021-0-3-86-93.
  5. Konovalov V.V., Dubinskiy S.V., Makarov A.D., Dotsenko A.M. Research of correlation dependencies between mechanical properties of aviation materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 40–46. DOI: 10.18577/2071-9140-2018-0-2-40-46.
  6. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577 / 2071-9140-2019-0-2-3-11.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  9. Kablov E.N. Innovative development is the most important priority of the state. Metaliy Eurazii, 2010, no. 2, pp. 6–11.
  10. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  11. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  12. Lobyntsev E.S., Glushko I.M., Kuznetsov V.M. Obtaining magnets with a columnar structure by casting into honeycomb molds. Elektrotekhnicheskaya promyshlennost'. Elektrotekhnicheskiye stali, 1974, is. 9 (38), pp. 15–19.
  13. Livshits B.G., Enikeev G.Kh., Blatov V.G. Production of high-energy magnets from YUNDK35T5BA alloy under industrial conditions. IV All-Union. conf. by permanent magnets. Novocherkassk: AN SSSR, 1971, p. 38.
  14. Sklyarov A.E., Chaban I.P., Gridnev A.I., Vlasov V.G. Obtaining single crystals of alloys for permanent magnets in industrial conditions. Growing refractory rare metals. Moscow: Nauka, 1973, pp. 8–11.
  15. Pikunov M.V., Belyaev I.V., Sidorov E.V. Crystallization of alloys and directional solidification of castings. Vladimir: Vladimir State University, 2002, 213 p.
  16. Piskorsky V.P. Thermostable hard magnetic materials based on rare-earth intermetallic compounds with a tetragonal structure: thesis abstract, Dr. Sc. (Tech.). Moscow: VIAM, 2014, 36 p.
  17. Ayres R.U., Peiro L.T. Material efficiency: Rare and critical metals. Philosophical Transactions of the Royal Society A: Mathematical, Physical and Engineering Sciences, 2013, vol. 371 (1986), p. 20110563. DOI: 10.1098/rsta.2011.0563.
  18. Nakamura H., Hirota K., Shimao M. et al. Magnetic properties of extremely small Nd–Fe–B sintered magnets. IEEE Transactions on Magnetics, 2005, vol. 41, no. 10, pp. 3844–3846.
  19. Schultz L., El-Aziz A.M., Barkleit G., Mummert K. Corrosion behaviorof Nd–Fe–B permanent magnetic alloys. Materials Science and Engineering A, 1999, vol. 267, no. 2, pp. 307–313.
  20. Ishii R., Miyoshi T., Kanekiyo H., Hirosawa S. High-coercivity nanocomposite permanent magnet based on Nd–Fe–B–Ti–C with Cr addition for high-temperature applications. Journal of Magnetism and Magnetic Materials, 2007, vol. 312, no. 2, pp. 410–413.
  21. Kekalo I.B., Samarin B.A. Physical metallurgy of precision alloys. Alloys with special magnetic properties. Moscow: Metallurgiya, 1989, pp. 496–497.
  22. Dovgalevsky Ya.M. Cast magnets from Magnico alloys. Moscow: Mashinostroenie, 1964, pp. 151–152.