Evaluation of the effectiveness of various methods of applying powder developers during capillary control

Kulichkova S.I., Golovkov A.N., Kudinov I.I., Skorobogatko D.S.
Kulichkova S.I., Golovkov A.N., Kudinov I.I., Skorobogatko D.S. Evaluation of the effectiveness of various methods of applying powder developers during capillary control // Proceedings of VIAM. 2022. No. 10. DOI: 10.18577/2307-6046-2022-0-10-116-127. URL: https://viam-works.ru/en/journal/2022/10/10
Keywords
non-destructive testing, fluorescent penetrant testing, sensitivity, control samples, powder developer, electrostatic spray, vortex application method
Abstract

Analyzes the effectiveness of various methods of applying a powder developer included in a penetrant materials with level I sensitivity for automated penetrant testing. The technologies of penetrant testing with the application of a powder developer using the electrostatic spraying unit and the automatic storm-camera. The results of comparative tests of two technologies on samples with low-cycle fatigue cracks of various sizes are presented, as well as a graph of the probability of detecting a defect characterizing a specific control technology.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  3. Podzhivotov N.Yu. The minimum samples amounts for an assessment of the initial moments of distribution of tensile ultimate strength for the samples of structural metallic materials. Aviation materials and technologies, 2021, no. 2 (63), paper no. 11. Available at: http://www.journal.viam.ru (accessed: July 4, 2022). DOI: 10.18577/2713-0193-2021-0-2-103-114.
  4. Klyuev V.V., Evlampiev A.I., Popov E.D. at al. Non-destructive control and diagnostics: a reference book. Moscow: Mashinostroenie, 2003, 656 p.
  5. Beda P.I., Vybornov B.I., Glazkov Yu.N. at al. Non-destructive control of metals and products. Moscow: Mashinostroenie, 1976, 456 p.
  6. Caturano G., Cavaccini G., Ciliberto A., Pianese V. Probability of Detection for Penetrant Testing in Industrial Environment. Applied and Industrial Mathematics, 2010, vol. 3, no. 3, pp. 186–195.
  7. Lively J.A. Fluorescent penetrant inspection probability of detection demonstrations performed for space propulsion. Review of Quantitative Nondestructive Evaluation, 2003, vol. 22, pp. 1891–1898.
  8. Rummel W.D., Matzkanin G.A. Nondestructive evaluation (NDE) capabilities data book. Third ed. Austin: TRI Austin, 1997, 598 p.
  9. Rentala V.K., Mylavarapu Ph., Gautam J., Kumar V. NDE Reliability using Laboratory Induced Natural Fatigue Cracks. 7th European-American Workshop on Reliability of NDE. Potsdam, 2017, pp. 1–8. Available at: https://www.ndt.net/search/docs.php3?showForm=off&id=21793 (accessed: September 4, 2022).
  10. Migun N.P., Gnusin A.B. Thermal effects in capillary non-destructive testing. Minsk: Belarus Navuka, 2011, 131 p.
  11. Industry Standard 1 90243–83. Capillary methods of non-destructive testing. Marking. Moscow: VIAM, 1983, 38 p.
  12. Kulichkova S.I., Golovkov A.N., Kudinov I.I., Laptev A.S. Modern flaw detection materials, equipment and automation of the process of capillary non-destructive testing. Kontrol. Diagnostika, 2019, no. 2, pp. 52–57. DOI: 10.14489/td.2019.02.pp052-057.
  13. Kudinov I.I., Golovkov A.N., Kulichkova S.I., Skorobogatko D.S. Evaluation of the effectiveness of the application of various methods of intensifying the process of capillary control using a domestic set of flaw detection materials. Defektoskopiya, 2019, no. 11, pp. 59–66. DOI: 10.1134/S0130308219110071.
  14. Mubarakshin R.M. Optimization of technology and equipment for producting disks of gas turbine engines and units. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 11–18. DOI: 10.18577/2071-9140-2018-0-4-11-18.
  15. State Standard 18442–80. Unbrakable control. capillary methods. Moscow: Publishing house of standards, 1987, 24 p.
  16. State Standard R ISO 3452-3-2009. The control is non-destructive. Penetrating control. Part 3: Test specimens. Moscow: Standartinform, 2011, 12 p.
  17. IndustryStandard1 90282–79. Product quality. Unbrakable control. capillary methods. Moscow: VIAM, 1979, 50 p.
  18. Kablov E.N., Ospennikova O.G., Kudinov I.I., Golovkov A.N., Generalov A.S., Knyazev A.V. Estimation of the probability of detecting operational defects in aircraft parts made of heat-resistant alloys using domestic and foreign flaw detection liquids. Defektoskopiya, 2021, no. 1, pp. 64–71. DOI: 10.31857/SO130308221010073.
  19. Chertishchev V.Yu. The estimation of the probability of defects detection by the acoustic methods, depending on their size in constructions from PCM for output control data in the form of binary. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 65–79. DOI: 10.18577/2071-9140-2018-0-3-65-79.
  20. Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https: //journal.viam.ru (accessed: July 4, 2022). DOI: 10.18577/2713-0193-2021-0-2-115-122.