Obtaining the prototype of not cooled nozzle turbine blade from ceramic composite material

Lebedeva Yu.E., Shchegoleva N.E., Chaynikova A.S., Voronov V.A., Shavnev A.A.
Lebedeva Yu.E., Shchegoleva N.E., Chaynikova A.S., Voronov V.A., Shavnev A.A. Obtaining the prototype of not cooled nozzle turbine blade from ceramic composite material // Proceedings of VIAM. 2020. No. 3. DOI: 10.18577/2307-6046-2020-0-3-58-65. URL: https://viam-works.ru/en/journal/2020/3/6
Keywords
spark plasma agglomeration, ceramic composite material, silicon carbide, consolidation, treshchinostoykost, nozzle blade.
Abstract

Not cooled nozzle turbine blade prototype from ceramic composite material of SiC-SiCw–B4C–AlN system was obtained by the method of spark plasma sintering. The received prototype combines low values of density (3,4 g/cm3) and CTE (α=(5,3–5,4)10-6 K-1) with high level of mechanical and thermal characteristics: microhardness (25–26 GPa), flexural strength (413 MPa), crack resistance (6,2–6,9 MPa√м) and heat resistance at 1500 °C (weight change is 0,72–0,77% during 600 h). The spark plasma sintering method has allowed to obtain uniform structure of not cooled nozzle turbine blade prototype from ceramic composite material.

Reference list
  1. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  2. Belyachenko I.O., Schegoleva N.E., Chaynikova A.S., Vaganova M.L., Shavnev A.A. Silicon nitride ceramic materials for aviation GTE bearings and methods of manufacturing (review). Trudy VIAM, 2019, no. 7 (79), paper no. 05. Available at: http://www.viam-works.ru (accessed: September 01, 2020). DOI: 10.18577/2307-6046-2019-0-7-42-49.
  3. Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
  4. Krenkel W., Berndt F. C/C–SiC composites for space applications and advanced friction systems. Materials Science and Engineering A, 2005, vol. 412, no. 1–2, pp. 177–181.
  5. Jacobson N.S. Corrosion of silicon-based ceramics in combustion environments. Journal of the European Ceramic Society, 1993, vol. 76, pp. 3–28.
  6. Van Roode M., Price J., Miriyala N., Leroux D. Ceramic matrix composite combustor liners: A summary of field evaluations. Journal of Engineering for Gas Turbines and Power, 2007, vol. 129, no. 1, pp. 21–30.
  7. Choi S.R., Bansal N.P. Shear Strength as a Function of Test Rate for SiCf / BSAS Ceramic Matrix Composite at Elevated Temperature. Journal of the American Ceramic Society, 2004, vol. 87, no. 10, pp. 1912–1918.
  8. Kablov E.N., Karachevtsev F.N., Stolyarova V.L., Vorozhtcov V.A., Lopatin S.I. Vaporization and thermodynamics of ceramicsin the Y2O3–ZrO2–HfO2 system. Rapid Communications in Mass Spectrometry, 2019, vol. 33, no. 19, pp. 1537–1546.
  9. Sakharov K.A., Simonenko E.P., Simonenko N.P., Vaganova M.L., Lebedeva Yu.E., Chaynikova A.S., Osin I.V., Sorokin O.Yu., Grashchenkov D.V., Sevastyanov V.G., Kuznetsov N.T., Kablov E.N. Glycol-citrate synthesis of fine-grained oxides La2−xGdxZr2O7 and preparation of corresponding ceramics using FAST/SPS process. Ceramics International, 2018, vol. 44, no. 7, pp. 7647–7655.
  10. Simonenko E.P., Simonenko N.P., Papynov E.K., Gridasova E.A., Sevastyanov V.G., Kuznetsov N.T. Obtaining ultrahigh-temperature ceramic materials HfB2–SiC (10–65 vol.% SiC) using sol-gel technology and hot pressing of the composite powder HfB2–(SiO2–SiC). Zhurnal neorganicheskoy khimii, 2018, vol. 63, no. 1, pp. 3–18.
  11. Torresillas San Millan R., Pinargote Solis N.V., Okunkova A.A., Peretyagin P.Yu. Fundamentals of the process of spark plasma sintering of nanopowders. Moscow: Technosphere, 2014, 96 p.
  12. Hasanov A.O. Development of compositions and technology for spark-plasma sintering of ceramic materials, composites based on micro- and nanopowders B4C: thesis, Cand. Sc. (Tech.). Tomsk, 2015, 201 p.
  13. Chuvildeev V.N., Boldin M.S., Nokhrin A.V., Blagoveshchensky Y.V., Sakharov N.V., Shotin S.V., Kotkov D.N., Panov D.V. Structure and properties of advanced materials obtained by Spark Plasma Sintering. Acta Astronautica, 2015, vol. 109, P. 172–176.
  14. Chuvildeev V.N., Boldin M.S., Dyatlova Ya.G., Rumyantsev V.I., Ordanyan S.S. Comparative study of hot pressing and high-speed electropulse plasma sintering of Al2O3/ZrO2/Ti(C, N) powders. Russian Journal of Inorganic Chemistry, 2015, vol. 60, no. 8, pp. 987–993.
  15. Avramenko V.A., Papynov E.K., Shichalin O.O., Mayorov V.Yu., Portnyagin A.S., Sokolnitskaya T.A., Koryavets E.G. Spark plasma sintering as an innovative approach to creating a new generation of nanostructured ceramics. VI Mezhdunarodnaya konferentsiya «Nanomaterialy i tekhnologii». Ulan-Ude, 2016, pp. 82–90.
  16. Barinov V.Yu., Rogachev A.S., Vadchenko S.G., Moskovsky D.O., Kolobov Yu.R. Spark plasma sintering of complex-shaped products using quasi-isostatic pressing. International Journal of Applied and Fundamental Research, 2016, no. 1-3, pp. 312–315.
  17. Vaganova M.L., Sorokin O.Yu., Osin I.V. Joining of ceramic materials by the method of spark plasma sintering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 306–317. DOI: 10.18577 / 2071-9140-2017-0-S-306-317.
  18. Batienkov R.V., Efimochkin I.Yu., Khudnev A.A. The research of a specific electrical conductivity of Mo–W powder alloys obtained by SPS. Trudy VIAM, 2019, no. 7 (79), paper no. 06. Available at: http://www.viam-works.ru (accessed: September 01, 2020). DOI: 10.18577 / 2307-6046-2019-0-7-50-58.
  19. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  20. Ceramic composite material: pat. 2689947 Rus. Federation; filed 25.04.18; publ. 29.05.19.