The production of powders by PREP method for addictive manufacturing – current situation and development prospects
Vostrikov A.V., Sukhov D.I. The production of powders by PREP method for addictive manufacturing – current situation and development prospects // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-3-3. URL: https://viam-works.ru/en/journal/2016/8/3
Keywords
AM, powder, granules, PREP.
Abstract
In this article the issue of PREP powders application in modern AM units both for SLS and DMD technologies is analyzed. The essential powder properties for these powders application in AM units are shown. The analytic forecast of development of PREP method for its most effective application in AM is made. The conclusions on its prospects and implementation in Russia are made as well. The work is executed within implementation of the complex scientific direction 10.3. «Technologies for receiving high-quality powders of alloys on different basis for the additive technologies and powders of solders for the soldering» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1].
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Chto takoe innovacii [What are innovations] // Nauka i zhizn. 2011. №11. S. 16–21.
- Kablov E.N. Materialy i tehnologii VIAM v konstrukciyakh perspektivnykh dvigatelej razrabotki OAO «Aviadvigatel» [VIAM`s materials and technologies applied in constructions of advanced engines developed by OPSC “Aviadvigatel”] // IB «Permskie aviacionnye dvigateli». 2014. №31. S. 43–47.
- Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
- Kablov E.N., Petrushin N.V., Svetlov I.L. Sovremennye litye nikelevye zharoprochnye splavy [Modern cast nickel heat-resistant alloys] // Nauchnye idei S.T. Kishkina i sovremennoe materialovedenie: sb. tr. Mezhdunar. nauch.-tekhn. konf. 2006. S. 39–55.
- Logunov A.V., Shmotin Yu.N. Sovremennye zharoprochnye nikelevye splavy dlya diskov gazovykh turbin (materialy i tehnologii) [Modern heat-resistant nickel alloys for disks of gas turbines (materials and technologies)]. M.: Nauka i tehnologii, 2013. 264 s.
- ASTM F2792−12a. Standard Terminology for Additive Manufacturing Technologies. West Conshohocken: ASTM International. 2012. DOI: 10.1520/F2792–12A.
- Shahzad K., Deckers J., Kruth J.-P., Vleugels J. Additive manufacturing of alumina parts by indirect selective laser sintering and post processing // Journal of Materials Processing Technology. 2013. P 1484–1494.
- Nerush S.V., Evgenov A.G. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava marki EP648-VI primenitelno k lazernoj LMD-naplavke, a takzhe ocenka kachestva naplavki poroshkovogo materiala na nikelevoj osnove na rabochie lopatki TVD [Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 01. Available at: http://www.viam-works.ru (accessed: November 11, 2015). DOI: 10.18577/2307-6046-2014-0-3-1-1.
- Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitelno k lazernoj LMD-naplavke [The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 04. Available at: http://www.viam-works.ru (accessed: November 11, 2015). DOI: 10.18577/2307-6046-2014-0-5-4-4.
- Available at: http://nami.ru/uploads/docs/centr_technology_docs/ 55a62fc89524bAT_metall.pdf (accessed: November 11, 2015)
- Wohlers Report. Additive Manufacturing and 3D Printing State of the Industry Annual Worldwide Progress Report. 2012. 286 p.
- Available at: http://files.lib.sfu-kras.ru/ebibl/umkd/63/u_lectures.pdf (accessed: November 11, 2015).
- Capus J.M. Metal Powders. A Global Survey of Production, Applications and Markets to 2010. 4th edition. Elsevier. 2005. 314 р.
- Dunkley J.J. Atomization // Powder Metal Technologies and Applications. ASM International Publishers. 1998. V. 7. P. 35–52.
- Lawley A., Atomization // Metal Powder Industries Federation Publishers. Princeton. 2003. 166 p.
- Smagorinski M.E., Tsantrizos P.G. Production of spherical titanium powder by plasma atomization // Proc. World Congress of PM & Particulate Matter. Metal Powder Ind. Fed. 2002. V. 3. P. 248–260.
- Sukhov D.I. Primenenie matematicheskoj modeli dlya analiza vliyaniya parametrov plazmennogo raspyleniya na krupnost granul iz titanovogo splava VT25UP [Application of mathematical model for influence analyses of plasma spraying parameters on size of grains from VT25UP titanium alloy] // Tekhnologiya legkikh splavov. 2013. №2. S. 57–68.
- Garibov G.S., Vostrikov A.V., Gric N.M., Fedorenko E.A. Razrabotka novykh granulirovannykh zharoprochnykh nikelevykh splavov dlya proizvodstva diskov i valov aviacionnykh dvigatelej [Development of new granulated heat-resistant nickel alloys for production of disks and shafts of aviation engines] // Tekhnologiya legkikh splavov. 2010. №2. S. 34–44.
- Vostrikov A.V., Garibov G.S., Ber L.B., Shlyapin S.D. Issledovanie fiziko-mekhanicheskikh svojstv i struktury granul iz novogo vysokoprochnogo nikelevogo splava, izgotovlennykh metodom PREP [Researches of physical and mechanical properties and structures of grains from new heat-resistant nickel alloy produced by PREP] // Tekhnologiya legkikh splavov. 2013. № 2. S. 69–75.
- Vostrikov A.V., Garibov G.S. Investigation in the Field of Physico-Mechanical Properties and a Structure of New Ni-Base Superalloy Powder // Proceeding HIP’14. Stockholm. 2014. P. 427–439.
- Sposob proizvodstva granul zharoprochnykh splavov: pat. 2468891 Ros. Federaciya [Method of production of grains of heat-resistant alloys]; zayavl. 18.11.11; opubl. 10.12.2012.
- Ustanovka dlya polucheniya metallicheskogo poroshka: pat. 2356696 Ros. Federaciya [Unit for production of metal powder]; zayavl. 14.09.07; opubl. 27.05.2009.
- Available at: http://www.itp-forum.ru/conf2015/documents/Section_prezentations/1_Logacheva_Kompozit.pdf (accessed: October 15, 2015).
- Garibov G.S., Gric N.M. V.I. Dobatkin i metallurgiya granul zharoprochnykh nikelevykh splavov [V.I. Dobatkin and metallurgy of grains of heat-resistant nickel alloys] // Tekhnologiya legkikh splavov. 2015. №2. S. 34–40.