S.V. Nerush, D.G. Chubov, D.I. Sukhov, Yu.Yu. Kaplanskiy Relationship between microstructure, creep mechanisms and stress‑rupture strength of the VZhS1 and VZhS3 nickel‑based superalloys produced by selective laser melting // Proceedings of VIAM. 2026. No. 7. DOI: 10.18577/2307-6046-2026-0-7-43-62. URL: https://viam-works.ru/index%2ephp/en/journal/2026/7/4

Relationship between microstructure, creep mechanisms and stress‑rupture strength of the VZhS1 and VZhS3 nickel‑based superalloys produced by selective laser melting

S.V. Nerush, D.G. Chubov, D.I. Sukhov, Yu.Yu. Kaplanskiy
Abstract

Isothermal creep tests in the range from 850 to 950 °C yielded a matrix stress exponent n = 6,24 and an effective activation energy Q ≈ 613 kJ/mol, indicating that creep is governed by dislocation mechanisms with a dominant contribution of dislocation climb past coherent γ′ precipitates. For the alloys developed, Q exceeds the nickel self-diffusion energy by 329 kJ/mol, which corresponds to the level of cast IN738LC. In terms of stress-rupture strength the VZhS1 alloy surpasses IN939, whereas at 1000 °C the highly alloyed VZhS3 alloy (σ100 ≈ 130 MPa) approaches cast VZhL12U (~140 MPa) and exceeds the superalloys currently used in additive manufacturing

Keywords
selective laser melting, nickel-based superalloys, creep, stress-rupture strength, activation energy, Larson–Miller parameter, γ′-phase, VZhS1, VZhS3
Reference list
  1. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New-generation materials and digital additive technologies for the production of resource parts FSUE «VIAM». Part 3. Adaptation and creation of materials. Electrometallurgiya, 2022, no. 4, pp. 15–25.
  2. Kablov E.N., Evgenov A.G., Petrushin N.V., Bakradze M.M., Nerush S.V., Shurtakov S.V., Mazalov I.S. Selective laser melting: materials and technologies for the synthesis of resource parts: textbook. Moscow: NRC «Kurchatov Institute» – VIAM, 2024, 512 p.
  3. Logunov A.V. Heat-resistant nickel alloys for gas turbine blades and disks. Moscow: Moscow Textbooks, 2018, 592 p.
  4. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders. Trudy VIAM, 2015, no. 2, pp. 8–15. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  5. Evgenov A.G., Gorbovec M.A., Prager S.M. Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  6. Mazalov I.S., Evgenov A.G., Prager S.M. Perspectives of heat resistant structurally stable alloy VZh159 application for additive production of high-temperature parts of GTE. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 3–7. DOI: 10.18577/2071-9140-2016-0-S1-3-7.
  7. Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective laser manufacture. Trudy VIAM, 2021, no. 8 (102), pp. 3–11. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2021-0-8-3-11.
  8. Kablov E.N., Nerush S.V., Chubov D.G., Suhov D.I., Filonova E.V., Pahomkin S.I. Structural instability of heat-resistant nickel-based superalloys with high content of the gamma prime phase obtained by selective laser melting method. Trudy VIAM, 2025, no. 8 (150), pp. 3–13. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2025-0-8-3-13.
  9. Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 43–51. Available at: http://www.journal.viam.ru (accessed: July 04, 2026). DOI: 10.18577/2713-0193-2022-0-2-43-51.
  10. Sukhov D.I., Nerush S.V., Efimochkin I.Yu., Karachevchev F.N., Bogachev I.A. Production of MMC based on VZh159 alloy by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), pp. 62–72. Available at: http://www.journal.viam.ru (accessed: July 04, 2026). DOI: 10.18577/2713-0193-2021-0-2-62-72.
  11. Rickenbacher L., Etter T., Hövel S., Wegener K. High Temperature Material Properties of IN738LC Processed by Selective Laser Melting (SLM) Technology. Rapid Prototyping Journal, 2013, vol. 19, no. 4, pp. 282–290. DOI: 10.1108/13552541311323281.
  12. Wilkes J., Hoopes K., Helfand J. Creep and Tensile Properties of Direct Metal Laser Sintered (DMLS) Inconel 738LC Coupons and Comparison to Cast Properties. The 6th International Supercritical CO2 Power Cycles Symposium. Pittsburgh, 2018, paper 168. Available at: https://sco2symposium.com/papers2018/materials/168_Paper.pdf (accessed: July 04, 2026).
  13. Xu J., Gruber H., Deng D. et al. Short-Term Creep Behavior of an Additive Manufactured Non-Weldable Nickel-Base Superalloy Evaluated by Slow Strain Rate Testing. Acta Materialia, 2019, vol. 179, pp. 142–157. DOI: 10.1016/j.actamat.2019.08.018.
  14. Bridges A., Shingledecker J., Torkaman A., Houck L. Metallurgical Evaluation of an Additively Manufactured Nickel-Base Superalloy for Gas Turbine Guide Vanes. ASME Turbo Expo 2020: Turbomachinery Technical Conference and Exposition. New York: ASME, 2020, vol. 8: Industrial and Cogeneration; Manufacturing Materials and Metallurgy; Marine; Microturbines, Turbochargers, and Small Turbomachines, art. GT2020-15363. DOI: 10.1115/GT2020-15363.
  15. Pröbstle M., Neumeier S., Hopfenmüller J. et al. Superior Creep Strength of a Nickel-Based Superalloy Produced by Selective Laser Melting. Materials Science and Engineering: A, 2016, vol. 674, pp. 299–307. DOI: 10.1016/j.msea.2016.07.061.
  16. Popovich V.A., Borisov E.V., Heurtebise V. et al. Creep and Thermomechanical Fatigue of Functionally Graded Inconel 718 Produced by Additive Manufacturing. TMS 2018: 147th Annual Meeting & Exhibition Supplemental Proceedings. The Minerals, Metals & Materials Series. Cham: Springer, 2018. DOI: 10.1007/978-3-319-72526-0_9.
  17. Kuo Y.-L., Horikawa S., Kakehi K. Effects of Build Direction and Heat Treatment on Creep Properties of Ni-Base Superalloy Built up by Additive Manufacturing. Scripta Materialia, 2017, vol. 129, pp. 74–78. DOI: 10.1016/j.scriptamat.2016.10.035.
  18. Nerush S.V., Chubov D.G., Kaplanskiy Yu.Yu., Suhov D.I. Investigation of experimental nickel-based heat-resistant alloy obtained by selective laser melting method. Trudy VIAM, 2025, no. 7 (149), pp. 3–12. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2025-0-7-3-12.
  19. Nerush S.V., Sukhov D.I., Kaplanskiy Yu.Yu., Chubov D.G. Regularities of the kinetics of creep and long-term strength of heat-resistant nickel alloy VZhS1. Coll. Reports of XVIII All-Rus. Conf. on Testing and Research of Materials Properties «TESTMAT» on the topic: «Modern approaches and trends in the development of structural-phase, chemical-analytical methods of analysis». Moscow: NRC «Kurchatov Institute» – VIAM, 2026, pp. 334–345.
  20. Shang S.L., Zacherl C.L., Fang H.Z. et al. Effects of Alloying Element and Temperature on the Stacking Fault Energies of Dilute Ni-Base Superalloys. Journal of Physics: Condensed Matter, 2012, vol. 24, no. 50, art. 505403. DOI: 10.1088/0953-8984/24/50/505403.
  21. Frost H.J., Ashby M.F. Deformation-Mechanism Maps: The Plasticity and Creep of Metals and Ceramics. Oxford: Pergamon Press, 1982, 166 p.
  22. Sawada K., Kimura K., Abe F. et al. Data Sheets on the Elevated-Temperature Properties of Nickel Based 16Cr–8,5Co–3,5Al–3,5Ti–2,6W–1,8Mo–0,9Nb Superalloy Casting for Gas Turbine Components. NIMS Creep Data Sheet No. 49A. Tsukuba: National Institute for Materials Science, 2012. DOI: 10.11503/nims.1053.
  23. Chen K., Dong J., Yao Z. Creep Failure and Damage Mechanism of Inconel 718 Alloy at 800–900 °C. Metals and Materials International, 2021, vol. 27, no. 5, pp. 970–984. DOI: 10.1007/s12540-019-00447-4.
  24. Epishin A.I., Fedelich B., Viguier B. et al. Creep of Single-Crystals of Nickel-Base γ-Alloy at Temperatures between 1150 °C and 1288 °C. Materials Science and Engineering: A, 2021, vol. 825, art. 141880. DOI: 10.1016/j.msea.2021.141880.
  25. Li Q., Tian S., Yu H. et al. Effects of Carbides and Its Evolution on Creep Properties of a Directionally Solidified Nickel-Based Superalloy. Materials Science and Engineering: A, 2015, vol. 633, pp. 20–27. DOI: 10.1016/j.msea.2015.02.056.
  26. Furillo F.T., Davidson J.M., Tien J.K., Jackman L.A. The Effects of Grain Boundary Carbides on the Creep and Back Stress of a Nickel-Base Superalloy. Materials Science and Engineering, 1979, vol. 39, pp. 267–273. DOI: 10.1016/0025-5416(79)90065-X.
  27. He L.Z., Zheng Q., Sun X.F. et al. Effect of Carbides on the Creep Properties of a Ni-Base Superalloy M963. Materials Science and Engineering: A, 2005, vol. 397, no. 1–2, pp. 297–304. DOI: 10.1016/j.msea.2005.02.038.
  28. Monkman F.C., Grant N.J. An Empirical Relationship between Rupture Life and Minimum Creep Rate in Creep-Rupture Tests. Proceedings of ASTM, 1956, vol. 56, pp. 593–620.
  29. Larson F.R., Miller J. A Time-Temperature Relationship for Rupture and Creep Stresses. Transactions of the ASME, 1952, vol. 74, pp. 765–771.
  30. Shaw S.W.K. Response of IN-939 to Process Variations. Superalloys 1980. Warrendale: The Metallurgical Society of AIME, 1980, pp. 275–284.
  31. Engineering Properties of Alloy 713C. Toronto: Nickel Institute. Publication No. 337. Available at: https://nickelinstitute.org/media/2487/alloys-713c_337.pdf (accessed: July 04, 2026).