D.G. Chubov , S.V. Nerush Generalized crack-resistance criterion nickel-based superalloys for selective laser melting // Proceedings of VIAM. 2026. No. 7. DOI: 10.18577/2307-6046-2026-0-7-26-42. URL: https://viam-works.ru/index%2ephp/en/journal/2026/7/3

Generalized crack-resistance criterion nickel-based superalloys for selective laser melting

D.G. Chubov , S.V. Nerush
Abstract

A generalized dimensionless crack-resistance criterion $\Xi$ for nickel-based superalloys processed by selective laser melting is proposed – the ratio of the plastic relaxation functional to the damage accumulation functional, combining solidification cracking, strain-age cracking and grain-boundary embrittlement with the $\gamma'$ precipitation kinetics. Defect-free synthesis corresponds to $\Xi > \Xi_{\text{cr}}$ with $\Xi_{\text{cr}} = 1$. The criterion accounts for 94 % of the experimental crack density variance against 41–74 % for known criteria. The VZhS1 (adjusted $R^2 = 0{,}88$ for six fitted parameters) and VZhS3 alloys designed with it were synthesized crack-free.

 

Keywords
selective laser melting, nickel-based superalloys, crack-resistance criterion, γ′-phase, CALPHAD, inverse alloy design, VZhS1, VZhS3
Reference list
  1. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New-generation materials and digital additive technologies for the production of resource parts FSUE «VIAM». Part 3. Adaptation and creation of materials. Electrometallurgiya, 2022, no. 4, pp. 15–25.
  2. Kablov E.N., Evgenov A.G., Petrushin N.V., Bakradze M.M., Nerush S.V., Shurtakov S.V., Mazalov I.S. Selective laser melting: materials and technologies for the synthesis of resource parts: textbook. Moscow: NRC «Kurchatov Institute» – VIAM, 2024, 512 p.
  3. Sukhov D.I., Nerush S.V., Belyakov S.V., Mazalov P.B. Study of surface layer roughness parameters and manufacturing accuracy of additive manufactured products. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Mashinostroyenye, 2017, no. 9 (690), pp. 73–84. DOI 10.18698/0536-1044-2017-9-73-84.
  4. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders. Trudy VIAM, 2015, no. 2, pp. 8–15. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  5. Evgenov A.G., Gorbovec M.A., Prager S.M. Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  6. Mazalov I.S., Evgenov A.G., Prager S.M. Perspectives of heat resistant structurally stable alloy VZh159 application for additive production of high-temperature parts of GTE. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 3–7. DOI: 10.18577/2071-9140-2016-0-S1-3-7.
  7. Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture. Trudy VIAM, 2021, no. 8 (102), pp. 3–11. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2021-0-8-3-11.
  8. Sukhov D.I., Nerush S.V., Efimochkin I.Yu., Karachevchev F.N., Bogachev I.A. Production of MMC based on VZh159 alloy by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), pp. 62–72. Available at: http://www.journal.viam.ru (accessed: July 04, 2026). DOI: 10.18577/2713-0193-2021-0-2-62-72.
  9. Min P.G., Vadeev V.E., Sukhov D.I., Raevskikh A.N. Structure and mechanical properties of a corrosion-resistant heat-resistant nickel alloy obtained by selective laser melting. Materialovedenie, 2021, no. 12, pp. 3–10. DOI 10.31044/1684-579X-2021-0-12-3-10.
  10. Petrushin N.V., Evgenov A.G., Zavodov A.V., Trennikov I.A. Structure and strength of heat-resistant nickel alloy ZhS32-VI obtained by selective laser melting on a single-crystal substrate. Materialovedenie, 2017, no. 11, pp. 19–26.
  11. Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 43–51. Available at: http://www.journal.viam.ru (accessed: July 04, 2026). DOI: 10.18577/2713-0193-2022-0-2-43-51.
  12. Kablov E.N., Nerush S.V., Chubov D.G., Suhov D.I., Filonova E.V., Pahomkin S.I. Structural instability of heat-resistant nickel-based superalloys with high content of the gamma prime phase obtained by selective laser melting method. Trudy VIAM, 2025, no. 8 (150), pp. 3–13. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2025-0-8-3-13.
  13. Nerush S.V., Chubov D.G., Kaplanskiy Yu.Yu., Suhov D.I. Investigation of experimental nickel-based heat-resistant alloy obtained by selective laser melting method. Trudy VIAM, 2025, no. 7 (149), pp. 3–12. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI: 10.18577/2307-6046-2025-0-7-3-12.
  14. Ghoussoub J.N., Tang Y.T., Panwisawas C., Németh A.A.N., Reed R.C. On the Influence of Alloy Chemistry and Processing Conditions on Additive Manufacturability of Ni-based Superalloys. Superalloys 2020. Eds S. Tin et al. Cham: Springer, 2020, pp. 153–162. DOI 10.1007/978-3-030-51834-9_15.
  15. Pollock T.M., Clarke A.J., Babu S.S. Design and Tailoring of Alloys for Additive Manufacturing. Metallurgical and Materials Transactions A, 2020, vol. 51, no. 12, pp. 6000–6019. DOI 10.1007/s11661-020-06009-3.
  16. Messe O.M.D.M., Muñoz-Moreno R., Illston T. et al. Metastable Carbides and Their Impact on Recrystallisation in IN738LC Processed by Selective Laser Melting. Additive Manufacturing, 2018, vol. 22, pp. 394–404. DOI 10.1016/j.addma.2018.05.030.
  17. ASM Specialty Handbook: Nickel, Cobalt, and Their Alloys / ed. J.R. Davis. Materials Park, OH: ASM International, 2000, 442 p. ISBN 0-87170-685-7.
  18. Prager M., Shira C.S. Welding of Precipitation-Hardening Nickel-Base Alloys. Welding Research Council Bulletin. New York: Welding Research Council, 1968, no. 128, p. 55.
  19. Haußmann L., Burbaum B., Stöhr B. et al. Crack-Free Welding of a Co-Base Superalloy with High \(\gamma^{\prime}\) Precipitate Fraction. Advanced Engineering Materials, 2022, vol. 24, art. 2200609. DOI: 10.1002/adem.202200609.
  20. Rappaz M., Drezet J.-M., Gremaud M. A New Hot-Tearing Criterion. Metallurgical and Materials Transactions A, 1999, vol. 30, no. 2, pp. 449–455. DOI 10.1007/s11661-999-0334-z.
  21. Kou S. A Criterion for Cracking during Solidification. Acta Materialia, 2015, vol. 88, pp. 366–374. DOI 10.1016/j.actamat.2015.01.034.
  22. Tang Y.T., Panwisawas C., Ghoussoub J.N. et al. Alloys-by-design: Application to New Superalloys for Additive Manufacturing. Acta Materialia, 2021, vol. 202, pp. 417–436. DOI: 10.1016/j.actamat.2020.09.023.
  23. Crudden D.J., Mottura A., Warnken N. et al. Modelling of the Influence of Alloy Composition on Flow Stress in High-Strength Nickel-Based Superalloys. Acta Materialia, 2014, vol. 75, pp. 356–370. DOI 10.1016/j.actamat.2014.04.075.
  24. Conduit B.D., Jones N.G., Stone H.J., Conduit G.J. Design of a Nickel-Base Superalloy Using a Neural Network. Materials & Design, 2017, vol. 131, pp. 358–365. DOI: 10.1016/j.matdes.2017.06.007.
  25. Conduit B.D., Illston T., Baker S., Vadegadde Duggappa D. et al. Probabilistic Neural Network Identification of an Alloy for Direct Laser Deposition. Materials & Design, 2019, vol. 168, art. 107644. DOI 10.1016/j.matdes.2019.107644.
  26. Gao Z., Hu W., Liu Y. et al. Intelligent Design of Crack-Resistant Nickel-Based Superalloys for Additive Manufacturing by Machine Learning and Multilayer Filtering Strategy. Materials Today Communications, 2025, art. 112360. DOI 10.1016/j.mtcomm.2025.112360.
  27. Vershkov A.V., Ospennikova O.G., Nerush S.V. Developing the concept of the integrated information system on the properties of aircraft materials with the ability to calculating the characteristics of new materials being developed. Trudy VIAM, 2015, no. 5, pp. 3–6. Available at: http://www.viam-works.ru (accessed: July 04, 2026). DOI 10.18577/2307-6046-2015-0-5-1-1.
  28. Karunaratne M.S.A., Carter P., Reed R.C. On the Diffusion of Aluminium and Titanium in the Ni-Rich Ni-Al-Ti System Between 900 and 1200 °C. Acta Materialia, 2001, vol. 49, no. 5, pp. 861–875. DOI: 10.1016/S1359-6454(00)00390-6.
  29. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.
  30. Karunaratne M.S.A., Reed R.C. Interdiffusion of Niobium and Molybdenum in Nickel Between 900–1300 °C. Defect and Diffusion Forum, 2005, vol. 237–240, pp. 420–425. DOI: 10.4028/www.scientific.net/DDF.237-240.420.
  31. Engeli R., Etter T., Geiger F. et al. Effect of Si on the SLM Processability of IN738LC. Proceedings of the 26th Annual International Solid Freeform Fabrication Symposium (SFF 2015), Austin, TX. Austin: University of Texas at Austin, 2015, pp. 823–831.
  32. Cloots M., Uggowitzer P.J., Wegener K. Investigations on the Microstructure and Crack Formation of IN738LC Samples Processed by Selective Laser Melting Using Gaussian and Doughnut Profiles. Materials & Design, 2016, vol. 89, pp. 770–784. DOI: 10.1016/j.matdes.2015.10.027.
  33. Lee Y.S., Kirka M.M., Kim S. et al. Asymmetric Cracking in Mar-M247 Alloy Builds During Electron Beam Powder Bed Fusion Additive Manufacturing. Metallurgical and Materials Transactions A, 2018, vol. 49, no. 10, pp. 5065–5079. DOI: 10.1007/s11661-018-4788-8.
  34. Siefert J.A., Shingledecker J.P., DuPont J.N., David S.A. Weldability and Weld Performance of Candidate Nickel Based Superalloys for Advanced Ultrasupercritical Fossil Power Plants. Part II: Weldability and Cross-Weld Creep Performance. Science and Technology of Welding and Joining, 2016, vol. 21, no. 5, pp. 397–427. DOI: 10.1080/13621718.2016.1143708.
  35. Ramsperger M., Roncery L.M., Lopez-Galilea I. et al. Solution Heat Treatment of the Single Crystal Nickel-Base Superalloy CMSX-4 Fabricated by Selective Electron Beam Melting. Advanced Engineering Materials, 2015, vol. 17, no. 10, pp. 1486–1493. DOI: 10.1002/adem.201500037.
  36. Karunaratne M.S.A., Carter P., Reed R.C. Interdiffusion in the Face-Centred Cubic Phase of the Ni-Re, Ni-Ta and Ni-W Systems Between 900 and 1300 °C. Materials Science and Engineering: A, 2000, vol. 281, no. 1–2, pp. 229–233. DOI: 10.1016/S0921-5093(99)00705-4.
  37. Logunov A.V. Heat-resistant nickel alloys for gas turbine blades and disks. Moscow: Moscow Textbooks, 2018, 592 p.