G.S. Sevalnev , A.V. Sheremetiev , T.G. Sevalneva , K.V. Dulnev Study of the change in electrical resistance depending on the structure evolution in austenitic nitrogen‑containing corrosion‑resistant steel VNS53‑Sh // Proceedings of VIAM. 2026. No. 7. DOI: 10.18577/2307-6046-2026-0-7-16-25. URL: https://viam-works.ru/index%2ephp/en/journal/2026/7/2
Study of the change in electrical resistance depending on the structure evolution in austenitic nitrogen‑containing corrosion‑resistant steel VNS53‑Sh
Abstract
The change in electrical resistivity of austenitic nitrogen-containing steel VNS53-Sh has been studied depending on heat treatment in the temperature range of 200–1000 °C. Using the IACS standard resistivity measurement method, the relationship between electrical resistivity and structural-phase transformations has been established, including chromium nitride precipitation, formation of discontinuous decomposition zones, and recrystallization. Threshold values of electrical resistivity for non-destructive testing of the phase composition of the steel under production conditions have been determined.
Keywords
nitrogen-containing steel, complex-alloyed austenitic steel, microstructure, phase composition, hardness, specific electrical resistivity
Reference list
- Filippov M.A., Litvinov V.S., Nemirovsky Yu.R. Steels with metastable austenite. Moscow: Metallurgiya, 1988, 256 p.
- Mushnikova S.Yu., Kostin S.K., Sagaradze V.V., Kataeva N.V. Structure, properties and resistance to stress corrosion cracking of nitrogen-containing austenitic steel strengthened by thermomechanical treatment. Fizika metallov i metallovedenie, 2017, vol. 118, no. 11, pp. 1223–1235. DOI: 10.7868/S0015323017110092.
- Svyazhin A.G., Kaputkina L.M. Nitrogen and high-nitrogen steels. Industrial technologies and properties. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya Metallurgiya, 2019, no. 62 (3), pp. 173–187. DOI: 10.17073/0368-0797-2019-3-173-187.
- Kushnereva D.S., Sapozhnikov G.V. Study of the properties of new high-strength stainless steels. Khimicheskaya fizika i mezoskopiya, 2019, vol. 21, no. 1, pp. 39–44.
- Sevalnev G.S., Druzhinina M.E., Voznesenskaya N.M. et al. Structural changes in surface layers during wear testing of high-strength austenitic steel VNS-53. Metally, 2023, no. 4, pp. 76–81.
- Parmenova O.N. Effect of Cold Deformation on the Corrosion Resistance of Austenitic Steels in Seawater. Ural School of Young Metallurgists: Coll. of Materials and Reports of the XIX Int. Scientific and Technical. Ural School-Seminar of Metallurgists – Young Scientists. Ekaterinburg: Ural Univ. Publ. House, 2018, pp. 332–333.
- Bubnov V.A. Mechanism of the Transition of Austenite to Martensite during Cold Plastic Deformation of Austenitic Steels. Izvestiya vysshikh uchebnykh zavedeniy. Mashinostroyenie, 2018, no. 11 (704), pp. 14–19.
- Kostina M.V., Kudryashov A.E., Spitsina I.V. et al. Study of the Effect of Hot Rolling and Heating Temperature for Quenching on the Structure and Hardness of Fe–13%Cr Steels Alloyed with Nitrogen, Vanadium, and Niobium. Metally, 2024, no. 3, pp. 21–31. DOI: 10.31857/S0869573324032131.
- Lukin E.I., Blinov V.M., Bannykh I.O. et al. Effect of cold rolling on the structure and mechanical properties of corrosion-resistant nitrogen-containing martensitic-austenitic-ferritic steel 03Kh17AN2F. Electrometallurgiya, 2025, no. 2, pp. 11–19. DOI: 10.31044/1684-5781-2025-0-2-11-19.
- Betsofen S.Ya., Lukin E.I., Ashmarin A.A. et al. Effect of Cold Rolling on the Phase Composition, Texture, and Residual Stresses in Steels with 15,9 and 17,7 % Mn. Russian Metallurgy (Metally), 2025, vol. 2025, no. 3, pp. 603–610. DOI: 10.1134/S0036029525700168.
- Sevalnev G.S., Dulnev K.V., Ryzhkov P.V., Leonov A.V., Voznesenskaya N.M. Optimization of heat treatment for high-strength corrosion-resistant nitrogen-containing steel to produce seamless thin-walled tubes. Trudy VIAM, 2025, no. 8 (150), pp. 41–52. Available at: http://www.viam-works.ru (accessed: October 11, 2025). DOI: 10.18577/2307-6046-2025-0-8-41-52.
- Sevalnev G.S., Gromov V.I., Dulnev K.V., Sevalneva T.G. Contact endurance of nitrogenous austenitic-martensitic steels with different hardening mechanism. Aviation materials and technologies, 2024, no. 2 (75), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: January 25, 2026). DOI: 10.18577/2713-0193-2024-0-2-3-14.
- Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
- Pichugin S.S., Shitikov V.S., Golovkov A.N. Non-destructive methods for residual stress assessment. Trudy VIAM, 2024, no. 1 (131), pp. 101–112. Available at: http://www.viam-works.ru (accessed: January 11, 2026). DOI: 10.18577/2307-6046-2024-0-1-101-112.
- Lednev I.S. Magnetic methods of non-destructive testing of aircraft parts. Aviation materials and technologies, 2024, no. 1 (74), pp. 111–120. Available at: http://www.journal.viam.ru (accessed: January 11, 2026). DOI: 10.18577/2713-0193-2024-0-1-111-120.
- Lin G., Zhang Z., Wang H. et al. Enhanced strength and electrical conductivity of Al–Mg–Si alloy by thermo-mechanical treatment. Materials Science and Engineering: A, 2016, vol. 650, pp. 210–217.
- Cui X., Wu Y., Zhang G. et al. Study on the improvement of electrical conductivity and mechanical properties of low alloying electrical aluminum alloys. Composites. Part B: Engineering, 2017, vol. 110, pp. 381–387.
- Bannykh I.O. Structural features and prospects for the application of high-nitrogen austenitic steels. Metallovedenie i termicheskaya obrabotka metallov, 2019, no. 5, pp. 22–29.
- Bannykh O.A., Blinov V.M. On the effect of discontinuous decomposition on the structure and properties of high-nitrogen steels and on methods for suppression thereof. Steel research, 1991, vol. 62, no. 1, pp. 38–45.
- Sagaradze V.V., Fomina O.V., Vikhareva T.V. et al. Features of delta-ferrite decomposition in nitrogen-containing austenitic steels. Fizika metallov i metallovedenie, 2018, vol. 119, no. 3, pp. 296–302.
- Belomyttev M.Yu. Regularities of austenite grain formation in 12% chromium heat-resistant ferritic-martensitic steels. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya Metallurgiya, 2023, vol. 66, no. 2, pp. 168–176.
- Bannykh I.O. Correlation of grain structure and mechanical properties of high-nitrogen austenitic steel 02Kh20AG10N4MFB after annealing. Deformatsiya i razrusheniye materialov, 2015, no. 12, pp. 25–29.
- Potak Ya.M. High-strength steels. Moscow: Metallurgiya, 1972, 208 p.
- Eliseev E.A., Leonov A.V., Voznesenskaya N.M., Nefedkin D.Yu. Study of structure changes under the influence of various technological factors on the properties of cold-rolled strip made of nickel-beryllium alloy grade 97NL-VI. Problemy chernoy metallurgii i materialovedeniya, 2022, no. 1, pp. 29–34.