Peculiarities of technology production specimens of PCM on CNC machines (review)
Minibaev M.I., Raskutin A.E., Goncharov V.A. Peculiarities of technology production specimens of PCM on CNC machines (review) // Proceedings of VIAM. 2019. No. 1. DOI: 10.18577/2307-6046-2019-0-1-105-114. URL: https://viam-works.ru/en/journal/2019/1/11
Keywords
production of samples from PCM, cutting tools for PCM, milling of composites, tool wear, CNC machine, vacuum table, diamond-like coating.
Abstract
The polymer composite materials industry is in constant development, however, PCM processing technologies must be developed, and the effects of mechanical processing on the properties of the material after processing should be investigated. Manufacturers of tools offer special cutters, differing in the materials from which they are made, geometry, grinding angles, etc. It is necessary to conduct research for each brand of material in order to designate the optimal cutting mode. The design of the equipment should provide reliable protection of personnel and take into account the properties formed during the processing of chips.
Reference list
- Kablov E.N., Kondrashov S.V., Yurkov G.Y. Prospects of using carbonaceous nanoparticles in binders for polymer composites // Nanotechnologies in Russia, 2013. Vol. 8. No. 3–4. P. 163–185.
- Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Russia needs new generation materials] // Redkiye zemli. 2014. №3. S. 8–13.
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials] // Polimernyye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Boychuk A.S., Generalov A.S., Stepanov A.V. Nerazrushayushhij kontrol ugleplastikov na nalichie nesploshnostej s ispolzovaniem ultrazvukovyh fazirovannyh reshetok [NDT monitoring of CFRP structural health by ultrasonic phased array technique] //Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 84–89. DOI: 10.18577/2071-9140-2015-0-3-84-89.
- Murashov V.V., Trifonova S.I. Kontrol kachestva polimernyh kompozicionnyh materialov ultrazvukovym vremennym sposobom velosimetricheskogo metoda [Quality control of polymer composite materials using ultrasonic time-of-flight velocimetric technique] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 86–90. DOI: 10.18577/2071-9140-2015-0-4-86-90.
- Boychuk A.S., Generalov A.S., Dikov I.A. Kontrol detaley i konstruktsiy iz polimernykh kompozitsionnykh materialov s primeneniyem tekhnologii ultrazvukovykh fazirovannykh reshetok [FRP parts and structures testing by phased array technique] // Aviacionnyye materialy i tehnologii. 2017. №1 (46). S. 45–50. DOI: 10.18577/2071-9140-2017-0-1-45-50.
- Nerazrushayushchiy kontrol: spravochnik / pod obshch. red. V.V. Klyuyeva [Non-Destructive Testing: Reference / gen. ed. By V.V. Klyuev]. M.: Mashinostroyeniye, 2006. T. 3: Ultrazvukovoy kontrol / I.N. Ermolov, Yu.V. Lange. 864 s.
- Antyufeyeva N.V., Stolyankov Yu.V., Iskhodzhanova I.V. Issledovaniye i otsenka svoystv polimernykh kompozitsionnykh materialov po metodikam, garmonizirovannym s mezhdunarodnymi standartami [Research and evaluation of the properties of polymeric composite materials by methods harmonized with international standards] // Konstruktsii iz kompozitsionnykh materialov. 2013. №3. S. 41–45.
- ASTM D5687/D5687M-95. Standard guide for preparation of flat composite panels with processing guidelines specimen preparation. ASTM International, West Conshohocken, PA, 2015. Available at: http://astm.org (accessed: October 01, 2018). DOI: 10.1520/D5687_D5687M-95R15.
- Abrão A.M., Rubio J.C.C., Faria P.E., Davim J.P. The effect of cutting tool geometry on thrust force and delamination when drilling glass fibre reinforced plastic composite // Materials and Design, 2008. Vol. 29. Is. 2. P. 508–513. Available at: https://www.scopus.com (accessed: October 18, 2018). DOI: 10.1016/j.matdes.2007.01.016.
- Caggiano A., Improta I., Nele L. Characterization of a new dry drill-milling process of Carbon Fibre Reinforced Polymer laminates // Materials. 2018. Vol. 11. Is. 8. P. 1470. Available at: https://www.scopus.com (Available at). DOI: 10.3390/ma11081470.
- Wang H., Sun J., Li J. et al. Evaluation of cutting force and cutting temperature in milling carbon fiber-reinforced polymer composites // International Journal of Advanced Manufacturing Technology. 2016. Vol. 82. Is. 9–12. P. 1517–1525. Available at: https://www.scopus.com (accessed: October 18, 2018). DOI: 10.1007/s00170-015-7479-2.
- Gao C., Xiao J., Xu J, Ke Y. Factor analysis of machining parameters of fiber-reinforced polymer composites based on finite element simulation with experimental investigation // International Journal of Advanced Manufacturing Technology. 2016. Vol. 83. Is. 5–8. P. 1113–1125. Available at: https://www.scopus.com (accessed: October 19, 2018). DOI: 10.1007/s00170-015-7592-2.
- Garant ToolScout: spravochnik po obrabotke rezaniyem [Garant ToolScout: handling Guide]. Hoffmann Group, 2013. S. 152–153.
- Tekhnologiya naneseniya almazopodobnykh pokrytiy [The technology of applying diamond-like coatings]. Available at: http://www.dlc.ru (accessed: October 20, 2018).
- Tikhomirov R.A., Nikolayev V.I. Mekhanicheskaya obrabotka plastmass [Mechanical processing of plastics]. L., 1975. 208 s.