Hydrogen influence on high-strength corrosion-resistant steel VNS65-Sh properties and ways of elimination of hydrogen embrittlement

Voznesenskaya N.M., Tonysheva О.А., Leonov A.V., Dulnev K.V.
Voznesenskaya N.M., Tonysheva О.А., Leonov A.V., Dulnev K.V. Hydrogen influence on high-strength corrosion-resistant steel VNS65-Sh properties and ways of elimination of hydrogen embrittlement // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-3-9. URL: https://viam-works.ru/en/journal/2018/10/1
Keywords
high strength steel, corrosion-resistant steel, diffusion mobility hydrogen, reduction of area, plasticity, heat treatment, surface cold working.
Abstract

High strength corrosion-resistant steel VNS65-Sh is the transitional class steel. This steel is used for manufacturing of the high-loaded power details and nodes for aviation engineering. The results of diffusion mobility hydrogen (DMH) influence on steel plasticity characteristics are shown in this article. The negative influence of surface cold working on removal of DMH during heat treatment is shown. The different modes of heat treatment providing the minimum content of DMH in samples and recovery of steel plasticity of are investigated. Positive influence of heat treatment in vacuum furnace on recovery of steel plasticity is shown.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnyye napravleniya razvitiya tekhnologiy proizvodstva zharoprochnykh materialov dlya aviatsionnogo dvigatelestroyeniya [Priority directions of development of technologies for the production of heat-resistant materials for aircraft engine industry] // Problemy chernoy metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  3. Gromov V.I., Voznesenskaya N.M., Pokrovskaya N.G., Tonysheva O.A. Vysokoprochnye konstrukcionnye i korrozionnostojkie stali FGUP «VIAM» dlya izdelij aviacionnoj tehniki [High-strength constructional and corrosion-resistant steels developed by VIAM for aviation engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 159–174. DOI: 10.18577/2071-9140-2017-0-S-159-174.
  4. Tonysheva O.A., Voznesenskaya N.M. Perspektivnyye vysokoprochnyye korrozionnostoykiye stali, legirovannyye azotom (sravnitel'nyy analiz) // Aviatsionnyye materialy i tekhnologii. 2014. №3. S. 27–32. DOI: 10.18577/2071-9140-2014-0-3-27-32.
  5. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  6. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resursosberegayushchiye tekhnologii vyplavki perspektivnykh liteynykh i deformiruyemykh superzharoprochnykh splavov s uchetom pererabotki vsekh vidov otkhodov [Resource-saving technologies for smelting promising casting and wrought superhigh-strength alloys with regard to processing all types of waste] // Elektrometallurgiya. 2016. №9. S. 30–41.
  7. Voznesenskaya N.M., Potak Ya.M., Kachanov E.B., Shalin R.E., Grashchenkov P.M., Zhabina V.A., Shvedova L.V. Vliyaniye vodoroda na kachestvo vysokoprochnykh korrozionnostoykikh staley [The influence of hydrogen on the quality of high-strength corrosion-resistant steels] // Novoye v metallurgii staley i splavov. Ser.: Aviacionnyye materialy. 1979. Vyp. 2. S. 120–129.
  8. Krivonogov G.S., Kablov E.N. Staticheskaya treshchinostoykost' navodorozhennykh vysokoprochnykh staley [Static crack resistance of hydrogen-reinforced high-strength steels] // Aviacionnyye materialy i tehnologii. 2000. Vyp. 2. S. 25–32.
  9. Geld P.V., Ryabov R.A. Vodorod v metallakh i splavakh [Hydrogen in metals and alloys]. M.: Metallurgiya, 1974. 271 s.
  10. Moroz L.S., Chechulin B.B. Vodorodnaya khrupkost metallov [Hydrogen brittleness of metals]. M.: Metallurgiya, 1967. 256 s.
  11. Sklyuyev P.V. Vodorod i flokeny v krupnykh pokovkakh [Hydrogen and flocs in large forgings]. M.: Mashgiz, 1963. 188 s.
  12. Kotrell A.F. Struktura metallov i svoystva [Metal structure and properties]. M.: Metallurgizdat, 1957. 134 s.
  13. Kablov E.N., Krivonogov G.S. Rabotosposobnost korrozionnostoykikh staley pri vozdeystvii vodoroda [The efficiency of corrosion-resistant steels under the influence of hydroge] // Metally. 2002. №1. S. 42–51.
  14. Bratukhin A.G., Demchenko O.F., Dolzhenkov N.N., Krivonogov G.S. Vysokoprochnyye korrozionnostoykiye stali sovremennoy aviatsii [High-strength corrosion-resistant steel of modern aviation]. M.: MAI, 2006. 654 s.
  15. Mak-Magon K., Braynt K., Benerdzhi S. Vliyaniye vodoroda i primesey na khrupkoye razrusheniye stali [Effect of hydrogen and impurities on steel brittle fracture] // Mekhanika razrusheniya, razrusheniye materialov. 1979. №17. S. 109–133.