Friction stir welding of high-strength aluminum-lithium V-1469 alloy semiproducts
Lukin V.I., Kulick V.I., Bezophen S.Ya., Lukinа E.A., Sharov A.V., Panteleev M.D., Samorukov M.L. Friction stir welding of high-strength aluminum-lithium V-1469 alloy semiproducts // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-2-2. URL: https://viam-works.ru/en/journal/2017/12/2
Keywords
friction stir welding (FSW), high-strength aluminum-lithium alloys, aluminum alloys, transmission electron microscopy (TEM), x-ray analysis, welded fuselage panel.
Abstract
The influence of heat treatment on the mechanical properties, corrosion resistance and structure of welds manufactured from high-strength aluminum-lithium V-1469 alloy pressed panels friction stir welded on the optimal welding parameters was investigated. The investigation of mechanical properties and corrosion resistance shows that the usage of technological scheme: welding+solution+ageing allows to obtain the following level of weld properties – σUTS weld≥0,83σUTS BM, KCU≥134 kJ/m2, IGC: 0,09 мм, layer corrosion of the weld: 3 point.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Lukin V.I., Ospennikova O.G. Perspektivnye alyuminievye splavy i tehnologii ih soedineniya dlya izdelij aviakosmicheskoj tehniki [Perspective aluminum alloys and technologies of their connection for products of aerospace equipment] // Tez. dokl. 2-j Mezhdunar. konf. «Alyuminij-21/Svarka i pajka». M., 2012. St. 8.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials are the base of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N., Lukin V.I., Zhegina I.P., Ioda E.N., Loskutov V.M. Osobennosti i perspektivy svarki alyuminijlitievyh splavov [Features and welding perspectives aluminum-lithium alloys] // Aviacionnye materialy i tehnologii. 2002. №4. S. 3–12.
- Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
- Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
- Fridlyander I.N., Chuistov K.V., Berezina A.L., Kolobnev N.I., Koval Yu.N. Alyuminij-litievye splavy. Struktura i svojstva [Aluminum-lithium alloys. Structure and properties]. Kiev: Naukova dumka, 1992. 192 s.
- Becofen S.Ya., Antipov V.V., Grushin I.A., Knyazev M.I., Hohlatova L.B., Alekseev A.A. Zakonomernosti vliyaniya sostava Al-Li splavov na kolichestvennoe sootnoshenie δ(Al3Li), S1(Al2MgLi) i Т1 (Al2CuLi) faz [Patterns of influence of structure of Al-Li of alloys on quantitative ratio δ(Al3Li), S1(Al2MgLi) and Т1 (Al2CuLi) of phases] // Metally. 2015. №1. C. 59–66.
- Mahin I.D., Nikolaev V.V., Petrovichev P.S. Issledovanie svarivaemosti splavov V-1469 i 01570S [Research of bondability of alloys V-1469 and 01570С] // Kosmicheskaya tehnika i tehnologii. 2014. №4. S. 69–75.
- Lukin V.I., Becofen S.Ya., Panteleev M.D., Dolgova M.I. Vliyanie termodeformacionnogo cikla STP na formirovanie struktury svarnogo soedineniya splava V-1469 [Influence of the STP thermodeformation cycle on forming of structure of welded connection of alloy V-1469] // Svarochnoe proizvodstvo. 2017. №7. S. 17–24.
- Lukin V.I., Ioda E.N., Bazeskin A.V. i dr. Osobennosti formirovaniya svarnogo soedineniya pri svarke treniem s peremeshivaniem alyuminievogo splava V-1469 [Features of forming of welded connection at friction bonding with V-1469 aluminum alloy hashing] // Svarochnoe proizvodstvo. 2012. №6. S. 30–36.
- Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Vliyanie termicheskoj obrabotki na harakteristiki svarnyh soedinenij vysokoprochnyh alyuminijlitievyh splavov [Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 06. Available at: http://www.viam-works.ru (accessed: November 10, 2017). DOI: 10.18577/2307-6046-2015-0-4-6-6.
- Malard B., De Geuser F., Deschamps A. Microstructure distribution in an AA2050 T34 friction stir weld and its evolution during post-welding heat treatment // Acta Materialia. 2015. Vol. 101. P. 90–100.
- Chong Gao, Zhixiong Zhu, Jian Han, Huijun Li. Correlation of microstructure and mechanical properties in friction stir welded 2198-T8 Al–Li alloy // Materials Science & Engineering A. 2015. Vol. 639. P. 489–499.
- Shamraj V.F., Klochkova Yu.Yu., Lazarev E.M., Gordeev A.S., Sirotkin V.P. Strukturnye sostoyaniya materiala listov alyuminij-litievogo splava 1469 [Structural conditions of material of sheets aluminum-lithium alloy 1469] // Metally. 2013. №5. S.77–84.
- Giles T.L., Oh-Ishi K., Zhilyaev A.P., Swamianathan S. et al. The Effect of Friction Stir Processing on the Microstructure and Mechanical Properties of an Aluminum Lithium Alloy // Metallurgical And Materials Transactions A. 2009. Vol. 40A. P. 104–115.
- Giummarra C., Thomas B., Rioja R.J. New aluminum lithium alloys for aerospace applications // Proceedings of the Light Metals Technology Conference. 2007. Available at: https://www.researchgate.net/publication/267374310_New_aluminum-lithium_alloys_for_aero-space_applications (accessed: November 13, 2017).
- De Geuser F., Bley F., Denquin A., Deschamps A. Mapping the microstructure of a friction-stir welded (FSW) Al–Li–Cu alloy // Journal of Physics: Conference Series. 2010. Vol. 247. P. 1–7. DOI:10.1088/1742-6596/247/1/012034.
- Chong Gao, Zhixiong Zhu, Jian Han, Huijun Li. Correlation of microstructure and mechanical properties in friction stir welded 2198-T8 Al–Li alloy // Materials Science & Engineering: A. 2015. Vol. 639. P. 489–499.
- Mishra R.S., Ma Z.Y. Friction Stir Welding and processing // Material Science and Engineering Reports. 2005. Vol. 50. No. 1–2. P. 1–78.
- Arbegast W.J. Friction stir welding. After a decade of development // Welding Journal. 2006. Vol. 85. No. 3. P. 28–35.
- Welded structural members and method and use thereof: pat. US 8.420.256 B2; publ. 16.04.13.
- Aluminum alloy products having improved property combinations and method for artificially aging same: pat. US 8.673.209 B2; publ. 18.03.14.