Disadvantages of waveguide techniques for measurement of radar-absorbing material characteristics

Romanov A.M., Beljaev А.А., Bespalova E.E.
Romanov A.M., Beljaev А.А., Bespalova E.E. Disadvantages of waveguide techniques for measurement of radar-absorbing material characteristics // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-11-11. URL: https://viam-works.ru/en/journal/2015/3/11
Abstract

It was shown in the paper that the measurement results of reflection ratios of radar-absorbing materials performed in the waveguide for each frequency corresponded to the results of measurements at a certain angle of incidence in case of polarization of the electric vector perpendicular to the plane of incidence; thus, they do not correspond to the measurements at normal incidence. Material permittivity measurement errors caused by a gap between a specimen and waveguide wall were estimated. A simplified expression for estimation of the relative error of permittivity measurements and some examples of errors calculation for the above two cases are given in the paper.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Beljaev A.A., Kondrashov S.V., Lepeshkin V.V., Romanov A.M. Radiopogloshhajushhie materialy [Radio-absorbing materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 348–352.
  5. Beljaev A.A., Bespalova E.E., Romanov A.M. Pozharobezopasnye radiopogloshhajushhie materialy dlja bezjehovyh kamer [Fireproof materials for radio-anechoic chambers] //Aviacionnye materialy i tehnologii. 2013. №1. S. 53–55.
  6. Agafonova A.S., Beljaev A.A., Kondrashov Je.K., Romanov A.M. Osobennosti formirovanija monolitnyh konstrukcionnyh radiopogloshhajushhih materialov na osnove kompozitov, napolnennyh rezistivnym voloknom [Features of formation of monolithic structural radar absorbing materials based composites filled with resistive fiber] //Aviacionnye materialy i tehnologii. 2013. №3. S. 56–59.
  7. Brandt L.A. Issledovanija dijelektrikov na sverhvysokih chastotah [Studies dielectrics at microwave frequencies]. M.: Gos. izd-vo fiz.-mat. lit. 1963. S. 191–201.
  8. Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik steklosotoplasta volnovodnym metodom [Study of the dielectric characteristics of the waveguide method steklosotoplasta] //Aviacionnye materialy i tehnologii. 2013. №4. S. 62–68.
  9. Beljaev A.A., Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik monolitnyh stekloplastikov radiotehnicheskogo naznachenija [The study of dielectric properties of monolithic fiberglass radio engineering] //Kompozitnyj mir. 2014 (v pechati).
  10. Bespalova E.E., Beljaev A.A., Romanov A.M., Shirokov V.V. Issledovanie dijelektricheskih harakteristik sloev mnogoslojnogo radiopogloshhajushhego materiala dlja bezjehovyh kamer na osnove vspenennogo asbesta, napolnennogo nauglerozhennym voloknom [Study of the dielectric characteristics of radar absorbing layers of the multilayer material for anechoic chambers on the basis of foam asbestos filled with carbonized fiber] //Trudy VIAM. 2014. №8. St. 12 (viam-works.ru).
  11. Lushina M.V., Parshin S.G., Rzhevskij A.A. Sovremennye jekranirujushhie i radiopogloshhajushhie materialy [Modern shielding and radio absorbing materials] //Sistemy upravlenija i obrabotka informacii. 2011. №22.S. 208–214, 223.
  12. Nikol'skij V.V., Nikol'skaja T.I. Jelektrodinamika i rasprostranenie radiovoln [Electrodynamics and Propagation]. M.: URSS. 2012. S. 44, 163–164.
  13. Bibikov S.B., Titov A.N., Cherepanov A.K. Sintez materiala s zadannym kojefficientom otrazhenija v shirokom diapazone chastot i uglov padenija [Synthesis of a material with a specified reflectivity in a wide range of frequencies and angles of incidence] /V sb. dokl. XV Mezhdunarodnoj nauch.-tehnich. konf. «Radiolokacija. Navigacija. Svjaz'». Voronezh. 2009. S. 1578–1584.
  14. Korn G.A., Korn T.M. Spusk s vychisleniem koordinat gradient [Descent from the calculation of the coordinates of the gradient]: Spravochnik po matematike. M.: Nauka. 1984. 660 s.
  15. Rosenbrock H.H. An automatic method for finding the greatest or least value of a function //The Computer Journal. 1960. V. 3. Р. 175–184.
  16. Brehovskih A.M. Volny v sloistyh sredah [Waves in layered media]. M.: Nauka. 1957. S. 52–56.
  17. Odelevskij V.I. Raschet obobshhennoj provodimosti geterogennyh struktur. 1-matrichnye dvuhfaznye sistemy s nevytjanutymi vkljuchenijami [Calculation of generalized conductivity heterogeneous structures. 1-matrix two-phase system with unstretched inclusions] //ZhTF. 1951. T. XXI. №5. S. 668–676.
  18. Fal'kovskij O.I. Tehnicheskaja jelektrodinamika [Technical electrodynamics]. SPb.: Lan'. 2009. 244 s.
  19. Kolosov Ju.A., Levkov F.E. Tochnostnye harakteristiki volnovodnogo metoda opredelenija jelektricheskih parametrov dijelektrikov [Performance characteristics of the waveguide method for determining the parameters of electrical insulators] //Voprosy radiojelektroniki. Ser. Obshhie voprosy radiojelektroniki. 1985. №12. S. 18–33.
  20. Kolosov Ju.A., Levkov F.E. O volnovodnom metode opredelenija jelektricheskih parametrov dijelektrikov [About waveguide method for determining the electrical parameters of dielectrics] //Voprosy radiojelektroniki. Ser. Obshhie voprosy radiojelektroniki. 1986. №1. S. 41–45.