Features of forming pressed fiber reinforced plastic on the basis of modified phenol-formaldehyde binding
Krasnov L.L., Kirina Z.V., Еliseev O.A. Features of forming pressed fiber reinforced plastic on the basis of modified phenol-formaldehyde binding // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-5-5. URL: https://viam-works.ru/en/journal/2014/8/5
Abstract
In work dependence has been used of physical, mechanical, technological, operational properties of pressing material on length of fiber, temperature, time of drying and prepreg storage life on the basis of the modified phenolic resin and carbon-silicious filler is used.
Reference list
- Stekloplastiki [GRP] /V kn. Istorija aviacionnogo materialovedenija. VIAM-80 let: gody i ljudi /Pod obshh. red. E.N. Kablova. M.: VIAM. 2012. S. 349–355.
- Arhangel'skij B.A. Plasticheskie massy [Plastics]: Spravochnoe posobie. L. 1961.
- S. 208–232.
- Polimernye kompozicionnye materialy: svojstva, struktura, tehnologii [Polymer composite materials: properties, structure, technology] /Pod obshh. red. A.A. Berlina. SPb.: Professija. 2008. S. 358–361.
- Brocyhin E.A. Tehnologija plasticheskih mass [Plastics technology]. L.: Gos. nauch.-tehnich. izd-vo himich. lit. 1963. S. 235–237.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature and heat-insulating materials based on fibers of refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
- Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Fire safety of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
- Kiselev B.A. Stekloplastiki [GRP]. M.: Goshimizdat. 1961. S. 142–147.
- Skrjabina M.E., Pijugzhanin V.M., Frushar D. Osobennosti formovanija tekstury deformacii v magnievom splave v processe ravnokanal'nogo uglovogo pressovanija [Features molding deformation texture in the magnesium alloy during equal channel angular pressing] //Perspektivnye materialy. 2013. №11. S. 33–42.
- Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works. ru).
- Osnovnye tehnologii pererabotki plastmass [Key technology Plastics processing] /Pod red. V.N. Kuznecova, V.K. Guseva. M.: Himija. 2004. 597 s.
- Berezin N.M., Zalazinskij A.G. Opredelenie uslovij plasticheskogo techenija nekompaktnyh materialov [Determination of the conditions of plastic flow of non-compact materials] //Fundamental'nye issledovanija. 2013. №8. S. 19–20.
- Sharkeev Ju.P., Eroshenko A.Ju., Fortuna S.V., Tolmachev A.I., Fink T.A. Mikrostruk-tura i mehanicheskie svojstva posle intensivnoj plasticheskoj deformacii [Microstructure and mechanical properties after severe plastic deformation] //Izvestija vuzov. 2013. №8. S. 60–64.
- Vasil'ev V.S. O press-formovochnyh mashinah [About the press molding machines] //KOKS i himija. 2011. №4. S. 32–38.
- Vinogradov V.M., Golovin G.S., Gorohovich A.I., Gruchishkin V.A., Pervushin Ju.S. Tehnologija proizvodstva prepregov dlja polimernyh kompozicionnyh materialov [Technology for producing prepregs polymer composites]. Ufa: CGATU. 1995. 92 c.
- Ishanov G.V. Prochnost' nemetallicheskih materialov pri neravnomernom nagreve [Strength of non-metallic materials with non-uniform heating]. K.: Naukova dumka. 1971. 187 s.
- Guljaev A.S. Novye steklovoloknistye materialy [New glass fiber materials]. M.: GOSINTI. 1959. 20 s.
- Napolniteli dlja polimernyh kompozicionnyh materialov [Fillers for polymer composites] /Pod red. P.G. Babaevskogo. M.: Himija. 1981. S. 19–85.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing techniques of structural fibrous RMB] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Dushin M.I., Hrul'kov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovanija detalej iz polimernyh kompozicionnyh materialov [Selection of process parameters autoclave molding parts made of polymer composites] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
- Dushin M.I., Hrul'kov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Bezavtoklavnogo molding carbon fiber based prepregs obtained by mortar technology] //Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
- Donskoj A.A., Shashkina M.A. Jelastomernye ogne-teplozashhitnye i teploakkumulirujushhie materialy [Elastomeric fire-and heat-storage materials] /V sb. Aviacionnye materialy na rubezhe XX–XXI vekov: Nauch.-tehnich. sb. M.: VIAM. 1994. S. 384–390.
- Shah V. Spravochnoe rukovodstvo po ispytanijam plastmass i analizu prichin ih razrushenija [Reference Manual of Tests and plastic analysis of the causes of their destruction]. SPb.: NAT. 2009. S. 178–191.