Modern trends in the development of galvanic protective coating that can operate at temperatures up to 600 °С

Vasiliev A.S., Vdovin A.I., Zakirova L.I., Koltsova M.А.
Vasiliev A.S., Vdovin A.I., Zakirova L.I., Koltsova M.А. Modern trends in the development of galvanic protective coating that can operate at temperatures up to 600 °С // Proceedings of VIAM. 2026. No. 4. DOI: 10.18577/2307-6046-2026-0-4-121-132. URL: https://viam-works.ru/en/journal/2026/4/10
Keywords
galvanic coating, high-temperature corrosion, composite electrolytic coating, functional coating
Abstract

This article presents a review of international scientific and technical literature on galvanic protective coatings used at temperatures up to 600 °C. According to the review, over 60 % of the research is devoted to the production of composite coatings based on nickel and its alloys. The most common alloying systems for composite electrolytic coatings based on nickel are identified. It is noted that the production of nickel-cobalt composites by electrodeposition is a promising approach, but it is primarily limited to laboratory experiments, and scaling up for industrial mass production remains a significant obstacle.

Reference list
  1. Yemets N.E., Belova I.V., Mikhalko L.V., Markova S.A. Technology of Materials and Coatings: in 2 parts: a textbook. Komsomolsk-on-Amur: KnAGTU Publ. House, 2013, part 2, 111 p.
  2. Lobanov M.L., Kardonina N.I., Rossina N.G., Yurovskikh A.S. Protective Coatings. a textbook. Ekaterinburg: Ural Univ. Publ. House, 2014, 200 p.
  3. Giurlani W., Zangari G., Gambinossi F. Electroplating for Decorative Applications: Recent Trends in Research and Development. Coatings, 2018, no. 8, p. 260.
  4. State Standard 9.303–84. Unified System of Protection against Corrosion and Aging. Metallic and Non-Metallic Inorganic Coatings. General Selection Requirements. Moscow: Standartinform, 2008, 34 p.
  5. Industry standard 90171–83. Metallic and Non-Metallic Inorganic Coatings. Selection of Types and Thicknesses. Moscow: Experimental Printing Enterprise TsNIITEIlegprom, 1983, 95 p.
  6. Salakhova R.K., Tikhoobrazov A.B. Thermal resistance of electrolytic chromium coatings. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 60–67. DOI: 10.18577/2071-9140-2019-0-2-60-67.
  7. Okonkwo B.O., Jeong C., Jang C. Advances on Cr and Ni Electrodeposition for Industrial Applications ‒ A Review. Coatings, 2022, no. 12, p. 1555.
  8. Walsh F.C., Wang S., Zhou N. The electrodeposition of composite coatings: Diversity, applications and challenges. Current Opinion in Electrochemistry, 2020, no. 20, pp. 8–19.
  9. Vinokurov E.G., Margolin L.N., Farafonov V.V. Electrodeposition of composite coatings. Khimiya i khimicheskaya tekhnologiya, 2020, vol. 63, pp. 4–38.
  10. Saini A., Singh G., Mehta S. et al. A review on mechanical behaviour of electrodeposited Ni-composite coatings. International Journal on Interactive Design and Manufacturing, 2023, no. 17, pp. 2247–2258.
  11. Zellele D.M., Yar-Mukhamedova G.S., Rutkowska-Gorczyca M. A Review on Properties of Electrodeposited Nickel Composite Coatings: Ni‒Al2O3, Ni‒SiC, Ni‒ZrO2, Ni‒TiO2 and Ni–WC. Materials, 2024, no. 17, p. 5715.
  12. Petukhova P.M., Bushueva E.G., Novgorodtseva O.N., Kizimov V.D. Electrodeposition of Ni–WC composite coatings: formation, structure and properties. Chimica Techno Acta, 2024, vol. 11 (4), pp. 1–7. DOI: 10.15826/chimtech.2024.11.4.08.
  13. Zhachkin S.Yu., Trifonov G.I., Sidorkin O.A., Pustovetov A.V. Wear resistance of nickel composite coatings with micron and submicron SiC particles. Inzhenernye tekhnologii i sistemy, 2024, vol. 34, no. 4, pp. 629–647.
  14. Parida G., Chaira D., Basu A. Ni–ZrO2 Composite Coating by Electro-Co-Deposition. Transactions of the Indian Institute of Metals, 2013, no. 66 (1), pp. 5–11.
  15. Bhogal S.S., Kumar V., Dhami S.S., Pabla B.S. Preparation and properties of electrodeposited Ni‒TiO2 composite coating. Journal of Electrochemical Science and Engineering, 2015, no. 5 (1), pp. 37–45.
  16. Mahidashti Z., Aliofkhazraei M., Lotfi N. Review of Nickel-Based Electrodeposited Tribo-Coatings. The Indian Institute of Metals – IIM, 2017, no. 71 (2), pp. 123–162.
  17. Hamidouche M., Walsh F.C. Mechanical and tribological characterization of electrolytically elaborated (Ni and Ni‒Co) deposits: Thesis for PhD. Sétif, 2021, p. 149.
  18. Mazalov P.B., Suhov D.I., Sulyanova E.A., Mazalov I.S. Heat-resistant cobalt-based alloys. Aviation materials and technologies, 2021, no. 3 (64), pp. 3‒10. Available at: http://www.journal.viam.ru (accessed: August 18, 2025). DOI: 10.18577/2713-0193-2021-0-3-3-10.
  19. Lai L., Qian F., Bi Y. et al. Advancements in the Preparation and Application of Ni‒Co System (Alloys, Composites, and Coatings): A Review. Nanomaterials, 2025, no. 15, p. 312.
  20. Karimzadeh A., Aliofkhazraei M., Walsh F.C. A review of electrodeposited Ni‒Co alloy and composite coatings: Microstructure, properties and applications. Surface & Coatings Technology, 2019, no. 372, pp. 463–498.
  21. Wang G.F., Jiang S.S., Lu Z., Zhang K.F. Preparation and tensile properties of Al2O3/Ni‒Co nanocomposites. Transactions of Nonferrous Metals Society of China, 2011, no. 21, pp. 374–379.
  22. Tian Y., Chengzhang P., Wei X. Ni–Co–Cr alloy co-deposition process. Journal of Hunan University Science and Technology (Natural Sciences Edition), 2015, no. 30, pp. 36–40.
  23. Li B., Zhang W., Li D. Synthesis and properties of a novel Ni–Co and Ni–Co/ZrO2 composite coating by DC electrodeposition. Journal of Alloys and Compounds, 2019, no. 821, p. 153258.
  24. Zhang Z.Q., Jiang C.H., Ma N.H. Electrodeposition and mechanical property of Ni–Co–ZrC coatings. Materials Research Innovations, 2015, vol. 19, no. 2, pp. 133–139.
  25. Torabinejad V., Aliofkhazraei M., Rouhaghdam A.S., Allahyarzadeh M.H. Tribological properties of Ni‒Fe‒Co multilayer coatings fabricated by pulse electrodeposition. Tribology International, 2017, no. 106, pp. 34–40.
  26. Kumaraguru S., Gnanamuthu R.M. An efficient corrosion protection activity of electrodeposited Ni/Ni‒Co‒Mn oxide composite for surface modification of steel. Materials Letters, 2021, no. 295, p. 129804.
  27. Ghazanlou S.I., Farhood A.H.S., Hosouli S. et al. Pulse and direct electrodeposition of Ni–Co/micro and nanosized SiO2 particles. Materials and Manufacturing Processes, 2018, no. 33, pp. 1067–1079.
  28. Xu W., Xu T., Wang X.L. et al. Effect of Diamond Particle Size on the Microstructure and Wear Resistance of Ni‒Co. Diamond Composite Coating. Equipment Manufacturing Technology, 2015, no. 6, pp. 9–11.
  29. Ilyin V.A. Nanotechnology for applying cluster galvanic coatings. Aviatsionnye materialy i technologii, 2009, no. 2, pp. 3–7.
  30. Nickel plating electrolyte: pat. 2293803C1 Rus. Federation; appl. 01.08.05; publ. 20.02.07.
  31. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  32. Kireev S.Yu., Kireeva S.N., Kozlov G.V., Kirilina Yu.N., Yangurazova A.Z. Development of the technology for electroplating composite Ni–WC coatings as an alternative to Co–WC coatings for aerospace components. Aviation materials and technologies, 2025, no. 3 (80), pp. 121–134. Available at: http://www.journal.viam.ru (accessed: September 18, 2025). DOI: 10.18577/2713-0193-2025-0-3-121-134.
  33. Kvyatkovskaya A.S., Saburova Yu.B., Belonogov V.A. et al. The investigation of electrodeposited Ni‒SiC coatings and the methods of its application on aluminum alloys. Aviation materials and technologies, 2024, no. 4 (77), pp. 128–139. Available at: http://www.journal.viam.ru (accessed: September 18, 2025). DOI: 10.18577/2713-0193-2024-0-4-128-139.
  34. Nagaev V.V. Study of nickel plating electrolytes containing nanopowders. Aviatsionnye materialy i technologii, 2009, no. 1, pp. 18–20.
  35. Khmeleva K.M., Kozlov I.A., Nikitin Ya.Yu., Nikiforov A.A. Modern trends of protective galvanic coatings working at high temperatures (review). Trudy VIAM, 2020, no. 12 (94), pp. 75–86. Available at: http://www.viam-works.ru (accessed: August 17, 2025). DOI: 10.18577/2307-6046-2020-0-12-75-86.