Prepregs and fiberglass based on VSR-3М resin and fiberglass fabrics for use in helicopter blades

Kolokoltseva T.V., Popov J.O., Lantsov I.A., Gusev Y.A.
Kolokoltseva T.V., Popov J.O., Lantsov I.A., Gusev Y.A. Prepregs and fiberglass based on VSR-3М resin and fiberglass fabrics for use in helicopter blades // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-56-65. URL: https://viam-works.ru/en/journal/2023/11/6
Keywords
carbon plastic, prepreg, helicopter blades, resin, polymer composite materials, aviation products
Abstract

This article presents the main results on the development of prepreg and carbon fiber based on the VSR-3M resin and carbon fabric grade VTkU-2.200. The process of studying prepreg, the technology of its production in an impregnation installation, and the selection of the main parameters of impregnation are described. Correct selection of impregnation parameters guarantees the production of materials with the required properties. The results of a study of the properties of prepreg obtained using the selected technological mode and carbon fiber reinforced plastic made from it are also presented. 

Reference list
  1. Haidar F. AL-Qrimli, Fadhil A. Mahdi, Firas B. Ismail. Carbon/Epoxy Woven Composite Experimental and Numerical Simulation to Predict Tensile Performance. Advances in Materials Science and Applications, 2015, vol. 4, is. 2, pp. 33–41.
  2. Polymer composite materials: structure, properties, technology: textbook. manual. Ed. A.A. Berlin. St. Petersburg: Profession, 2011, 560 p.
  3. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: August 20, 2023). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  4. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 2. Automated Fiber Placement (AFP). Aviation materials and technologies, 2021, no. 3 (64), paper no. 11. Available at: http://www.journal.viam.ru (accessed: August 20, 2023). DOI: 10.18577/2713-0193-2021-0-3-117-127.
  5. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 3. Comparison of ATL and AFP technologies. Hybrid technology of ATL/AFP. Aviation materials and technologies, 2021, no. 4 (65), paper no. 05. Available at: http://www.journal.viam.ru (accessed: August 20, 2023). DOI: 10.18577/2713-0193-2021-0-4-43-50.
  6. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  7. Kablov E.N. The formation of domestic space material science. Vestnik RFFI, 2017, no. 3,pp. 97–105.
  8. Kablov E.N. VIAM: New generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  9. Weber T.A., Ruff-Stahl H.-J.K. Advances in Composite Manufacturing of Helicopter Parts. International Journal of Aviation, Aeronautics and Aerospace, 2017, vol. 4, is. 1, pp. 1–33.
  10. Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products. Trudy VIAM, 2020, no. 12 (94), paper no. 05. Available at: http://www.viam-works.ru (accessed: September 01, 2023). DOI: 10.18577/2307-6046-2020-0-12-47-58.
  11. Handbook of compositional materials: in 2 book. Ed. J. Lubina; trans. from Engl. A.B. Geller, M.M. Helmont. Moscow: Mashinostroenie, 1988, book 1, 448 p.
  12. Qiang Liu, Yongzhou Lin, Zhijian Zong, Guangyong Sun, Qing Li. Lightweight design of carbon twill weave fabric composite body structure for electric vehicle. Composite Structures, 2013, vol. 97, pp. 231–238.
  13. HexPly Prepreg Technology. Available at: https://www.hexcel.com/user_area/content_media/raw/Prepreg_Technology.pdf (accessed: September 20, 2023).
  14. Composite Materials Handbook-17 (СМН-17). SAE International, 2012, vol. 1: Polymer matrix composites guidelines for characterization of structural materials, р. 96.
  15. Kolokoltseva T.V., Popov Yu.O., Usacheva M.N., Gromova A.A. Prepregs and fiberglass based on VSR-3М binder and fiberglass fabrics for use in helicopter blades. Trudy VIAM, 2018, no. 3 (109), paper no. 03. Available at: http://www.viam-works.ru (accessed: August 27, 2023). DOI: 10.18577/2307-6046-2022-0-3-27-34.