Prospects for the use of polymer composite materials based on flax fibers

Donetskiy K.I., Khrulkov A.V., Gorodilova N.A., Melnikov D.A.
Donetskiy K.I., Khrulkov A.V., Gorodilova N.A., Melnikov D.A. Prospects for the use of polymer composite materials based on flax fibers // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-82-95. URL: https://viam-works.ru/en/journal/2023/10/8
Keywords
polymer composite materials, biopolymers, natural fiber, flax fiber, biopolymer binder, fiber adhesion, molding
Abstract

Environmental problems, primarily such as the inability to recycle materials and, consequently, the formation of uncontrolled landfills, are powerful incentives for the development of biodegradable materials. Due to its environmental and economic advantages, as well as its technical characteristics, natural fibers become a likely replacement for synthetic ones for use as fillers in polymer composite materials. Flax fibers, due to their high availability and specific properties, are the most valuable products of the bast type. Physical and chemical processing of fibers allows them to be used for structural materials as well.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  3. Kablov E.N., Erofeev V.T., Dergunova A.V., Deraeva E.V., Svetlov D.A. Influence of environmental factors on the processes of biodegradation of vinylester composites. Journal of Physics: Conference Series. «International Conference on Engineering Systems 2020», 2020, pp. 012029.
  4. Donetskij K.I., Khrulkov A.V. Application of naturals fibers for manufacturing of polymer composite materials. Trudy VIAM, 2015, no. 2, paper no. 09. Available at: http://www.viam-works.ru (accessed: July 05, 2023). DOI: 10.18577/2307-6046-2015-0-2-9-9.
  5. Popov Yu.O., Koloкoltseva T.V., Gromova A.A., Gusev Yu.A. Influence of operational factors on the main physical and mechanical properties of a fiberglass product VPS-31. Trudy VIAM, 2021, no. 11 (105), paper no. 08. Available at: http://www.viam-works.ru (accessed: January 10, 2023). DOI: 10.18577/2307-6046-2021-0-11-82-90.
  6. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: February 01, 2023). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  7. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: January 10, 2023). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  8. Donetskiy K.I., Bystrikova D.V., Karavaev R.Yu., Timoshkov P.N. Application of polymeric composite materials for creation of elements of transmissions of aviation engineering (review). Trudy VIAM, 2020, no. 3 (87), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 19, 2023). DOI: 10.18577/2307-6046-2020-0-3-82-93.
  9. Gonzalo M., Fangueiro R. PLA Composites Reinforced with Flax and JuteFibers–A Review of Recent Trends, Processing Parameters and Mechanical Properties. Polymers, 2020, no. 12 (2373), pp. 1–29.
  10. Mohamad Midani M., Elseify L.A. Natural Fiber Composites: Practical Guide for Industrial Utilization. International Fiber Journal, 2022, no. 2, pp. 26–29.
  11. Shekar H.S., Ramachandra M. Green Composites: A Review. Materials Today Proceedings, 2018, no. 5, pp. 2518–2526.
  12. Mulhaupt R. The Use of Renewable Resources–Possibilities and Limitations. Energies, 1996, no. 50, pp. 191–198.
  13. Siakeng R., Jawaid M., Ariffin H. et al. Natural fiber reinforced polylactic acid composites: A review. Polymer Composites, 2019, vol. 40, is. 2, pp. 446–463. DOI: 10.1002/pc.24747.
  14. McMullen P. Fiber/resin composites for aircraft primary structures: A short history. Composites, 1984, no. 15, pp. 222–230.
  15. Bristol Blenheim. Available at: http://www.pilotfriend.com/photo_albums/timeline/ww2/Bristol%20Blenheim.htm (accessed: August 24, 2023).
  16. Middleton D.H. Composite Developments in Aircraft Structures – Part 1. Aircraft Engineering and Aerospace Technology, 1992, vol. 64, no. 5, pp. 2–8. DOI: 10.1108/eb037234.
  17. Sáez A. Industrial Applications of Natural Gas. InTech Open, 2010, no. 9, pp. 11–28.
  18. Bos H.L. The potential of flax fibres as reinforcement for composite materials. Technische Universiteit Eindhoven, 2004. DOI: 10.6100/IR575360.
  19. Xie Y., Hill C.A.S., Xiao Z. et al. Silane coupling agents used for natural fiber/polymer composites: A review. Polymer Composites, 2010, no. 41, pp. 806–819.
  20. Pacheco-Torgal F., Jalali S. Cementitious building materials reinforced with vegetable fibers: A review. Polymer Composites, 2011, no. 25, pp. 575–581.
  21. Sidorina A.I. Natural reinforcing fillers for polymer composite materials (review). Khimicheskie volokna, 2023, no. 1, pp. 56–65.
  22. Jawaid M., Khalil H.A. Cellulosic/synthetic fiber reinforced polymer hybrid composites: A review. Polymer Composites, 2011, no. 86, pp. 1–18.
  23. Hart A., Summerscales J. Effect of time at temperature for natural fibers. Procedia Engineering, 2017, no. 200, pp. 269–275.
  24. Mohanty A.K., Misra M., Dreal L.T. Surface Modifications of Natural Fibers and Performance of the Resulting Biocomposite // Composite Interfaces, 2001, no. 8, pp. 313–343.
  25. Cruz J., Fangueiro R. Surface Modification of Natural Fibers: A Review. Procedia Engineering, 2016, no. 155, pp. 285–288.
  26. Cho D., Lee H.S., Han S.O. Effect of Fiber Surface Modification on the Interfacial and Mechanical Propertiesof Kenaf Fiber-Reinforced Thermoplastic and Thermosetting Polymer Composites. Composite Interfaces, 2009, no. 16, pp. 711–729.
  27. Ferreira D.P., Cruz J., Fangueiro R. Surface Modification of Natural Fibers in Polymer Composites // Composite Interfaces, 2019, no. 6, pp. 30–41.
  28. Herrmann A., Nickel J., Riedel U. Construction materials based upon biologically renewable resources–From components to finished parts. Procedia Engineering, 1998, no. 59, pp. 251–261.
  29. Pickering K.L., Efendy M.A., Le T.M. A review of recent developments in natural fiber composites and their mechanical performance. Composite Interfaces, 2016, no. 83, pp. 98–112.
  30. Netravali A.N. Advanced green composites: New directions. Advanced Composite Materials, 2019, no. 8, pp. 32–38.
  31. Netravali A.N., Huang X., Mizuta K. Advanced «Green» Composites. Advanced Composite Materials, 2018, no. 7, pp. 12–24.
  32. Chow W.S., Ishak Z.A.M. Smart polymer nanocomposites: A review. Procedia Engineering, 2020, no. 14, pp. 16–35.
  33. Zhang N., Khan T., Guo H., Shi S., Zhong W., Zhang W. Functionally Graded Materials: An Overview of Stability, Buckling and Free Vibration Analysis. Advances in Materials Science and Engineering, 2019, no. 5, pp. 1–18.
  34. Singh R., Bhavar V., Kattire P., Thakare S., Patil S., Singh R.K.P. A Review on Functionally Gradient Materials (FGMs) and Their Applications. Procedia Engineering, 2017, no. 229, pp. 22–36.
  35. Pereira J.F., Ferreira D.P., Pinho E., Fangueiro R. Chemical and Biological Warfare Protection and Self-Decontaminating Flax Fabrics Based on CaO Nanoparticles. Key Engineering Materials, 2019, no. 812, pp. 75–83.
  36. Costa S.M., Ferreira D.P., Ferreira A., Vaz F., Fangueiro R. Multifunctional Flax Fibers Based on the Combined Effect of Silver and Zinc Oxide (Ag/ZnO) Nanostructures. Nanomaterials, 2018, no. 8, pp. 10–30.
  37. Njuguna J., Nassiopoulos E. Development of flax-reinforced bio-composites for high-load bearing automotive parts. Composite Materials, 2012, no. 4, pp. 17–30.
  38. Torterat C. Flax fiber, the material that will replace fiberglass in boat building? Boats news: International Boats magazine. Available at: https://www.boatsnews.com/story/39468/flax-fiber-the-material-that-will-replace-fiberglass-in-boat-building (accessed: July 12, 2023).
  39. Gladunova O. Bridge made of flax and bioresin in the Netherlands. Available at: https://compositeworld.ru/articles/app/id627b59b50e5c8f00199ab8d6 (дата обращения: 24.08.2023).
  40. Mishkin S.I., Raskutin A.E., Evdokimov A.A., Gulyaev I.N. Technologies and the main stages of construction of the arch bridge first in Russia from composite materials. Trudy VIAM, 2017, no. 6 (54), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 05, 2023). DOI: 10.18577/2307-6046-2017-0-6-5-5.
  41. Crosse J. Amplitex, which consists of woven fabric made of flax fibres, could be an alternative to carbon-fibre. Available at: https://www.autocarindia.com/auto-features/fun-flax-an-eco-friendly-alternative-to-carbon-fibre-419419 (accessed: July 13, 2023).
  42. Ignatieva A. Tatneft brought to the market composite profiles using eco-material. Available at: https://neftegaz.ru/news/Oborudovanie/726857-tatneft-vyvela-na-rynok-kompozitnye-profili-s-ispolzovaniem-eko-materiala/ (accessed: July 12, 2023).
  43. Achieve carbon neutrality: Tatneft began production of flax composites. Available at: https://www.tatar-inform.ru/news/dostic-uglerodnoi-neitralnosti-tatneft-nacala-vypusk-kompozitov-iz-lna-5856880 (accessed: July 12, 2023).