Abstract
This review considers the biological damage of thermoplastic and thermoset reinforced polymer composite materials, carbon and glass fibers and resins by microorganisms and fungi. It is shown that biodegradation affects the structural integrity of the material, physical and mechanical properties. The conditions for the favorable development of microorganisms, the mechanism of biodegradation, some types of bacteria and fungi that affect polymer composite materials and the mechanisms of biofilm formation are considered.
Reference list
- Buznik V.M., Kablov E.N. Materials for the development of the Arctic and cold territories. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 21.
- Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: January 24, 2022). DOI: 10.18577/2713-0193-2021-0-2-51-61.
- Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 2. Automated Fiber Placement (AFP). Aviation materials and technologies, 2021, no. 3 (64), paper no. 11. Available at: http://www.journal.viam.ru (accessed: January 24, 2022). DOI: 10.18577/2713-0193-2021-0-3-117-127.
- Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 3. Comparison of ATL and AFP technologies. Hybrid technology of ATL/AFP. Aviation materials and technologies, 2021, no. 4 (65), paper no. 11. Available at: http://www.journal.viam.ru (accessed: January 24, 2022). DOI: 10.18577/2713-0193-2021-0-4-43-50.
- Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
- Khrulkov A.V., Timoshkov P.N., Yazvenko L.N., Usacheva M.N. Composite materials for medical and biological purposes (review). Novosti materialovedeniya. Nauka i tekhnika, 2018, no. 3–4 (30), paper no. 05. Available at: http://www.materialsnews.ru (accessed: January 27, 2022).
- Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of the structure and reinforcement transmission shafts made of polymer composite materials (review). Trudy VIAM, 2021, no. 1 (95), paper no. 9. Available at: http://www.viam-works.ru (accessed: January 24, 2022). DOI: 10.18577/2307-6046-2021-0-1-85-96.
- Agarwal B.D., Broutman L.T. Analysis and Performance of Fiber Composites. New York: John Wiley & Sons Inc., 1990, 562 p.
- Gu J.D., Ford T.E., Throp K.E.G., Mitchell R. Microbial Degradation of Polymeric Materials. Tri-Service Conference on Corrosion. Orlando, 1994, pp. 1–12.
- Rose A.H. Microbial Biodeterioration. New York: Academic Press, 1981, 516 p.
- Little B.J., Wagner P., Maki J.S. et al. Factors influencing the adhesion of microorganisms to surfaces. Journal of Adhesion, 1986, vol. 20, pp. 187–210.
- Gu J.-D., Mitchell R. Biodeterioration. The Prokaryotes. Ed. E. Rosenberg. New York: Springer-Verlag, 2013, pp. 309–342.
- Flemming H.C. Relevance of bioflms for the biodeterioration of surfaces of polymeric materials. Polymer Degradation and Stability, 1998, vol. 59, pp. 309–315.
- Thorp K.E.G., Crasto A.S., Gu J.-D., Mitchell R. Biodegradation of composite materials. Proceedings of the Tri-Service Conference on Corrosion. Washington: U.S. Government Printing House, 1994, pp. 303–314.
- Davies P., Mazeas F., Csari P. Sea water aging of glass reinforced composites: shear behavior and damage modeling. Journal of Composite Materials, 2001, vol. 35, pp. 1343–1372.
- Gu J.-D., Ford T.E., Thorp K.E.G., Mitchell R. Microbial Growth on Fiber Reinforced Composite Materials. International Biodeterioration and Biodegradation, 1996, vol. 39, pp. 197–204.
- Stroganov V.F., Kukoleva D.A., Akhmetshin A.S., Stroganov I.V. Biodeterioration of Polymers and Polymer Composite Materials. Polymer Science: Series D. Glues and Sealing Materials, 2009, vol. 2, no. 3, pp. 164–166.
- Little B., Ray R., Wagner P. et al. Impact of biofouling on the electrochemical behavior of stainless steels in natural seawater. Biofouling, 1991, vol. 3, pp. 45–59.
- Wagner P., Little B., Kevin R.H., Ray R.I. Biodegradation of Composite Materials. International Biodeterioration and Biodegradation, 1996, vol. 38, pp. 125–132.
- Pendrys J.P. Microbially induced degradation of P55 graphite fibers. Journal of The Electrochemical Society, 1989, vol. 136, pp. 113.
- Gu J.-D., Ford T.E., Thorp K.E.G., Mitchell R. Microbial deterioration of fiber reinforced composite materials. International Conference on Microbial Induced Corrosion, NACE International, 1995, pp. 439–460.
- Gu J.-D., Roman M., Esselman T., Mitchell R. The role of microbial bioflms in deterioration of space station candidate materials. International Biodeterioration & Biodegradation, 1998, vol. 41, pp. 25–33.
- Gu J.-D., Lu C., Thorp K.E.G. et al. Fiber-reinforced polymeric composites are susceptible to microbial degradation. Journal of Industrial Microbioilogy & Biotechnology, 1997, vol. 18, pp. 364–369.
- Upsher F.J. Microbial attack on materials. Proceedings The Royal Australian Chemical Institute, 1976, vol. 43–44, pp. 173–176.
- Tucker W.C., Brown R. Blister formation on graphite/polymer composites galvanically coupled with steel in seawater. Journal of Composite Materials, 1989, vol. 23, pp. 389–395.
- Belik E.S., Rudakova L.V., Kulikova Yu.V. Evaluation of the effectiveness of biodegradation of polymer composite materials. Vestnik NVGU, 2017, no. 4, pp. 111–118.
- Sakaeva E.Kh., Kulikova Yu.V., Rudakova L.V. Biodegradation of polymeric composite materials by microscopic fungi. Teoreticheskaya i prikladnaya ekologiya, 2018, no. 4, pp. 68–75.
- Imam M.A., Breister A.M., Zhou Zh. et al. Elucidatind the Impact of Microbial Interactions on Fiber-Reinforced Polymer Composites. 35th Technical Conference of the American Society for Composites, 2020, vol. 1, pp. 475–486.
- Kablov E.N., Erofeev V.T., Zotkina M.M., Dergunova A.V., Moiseev V.V., Rimshin V.I. Plasticized epoxy composites for manufacturing of composite reinforcement. Journal of Physics: Conference Ser.: International Conference on Engineering Systems 2020, 2020, pp. 12–31.
- Kablov E.N., Erofeev V.T., Dergunova A.V., Deraeva E.V., Svetlov D.A. Influence of environmental factors on the processes of biodegradation of vinylester composites. Journal of Physics: Conference Ser.: International Conference on Engineering Systems 2020, 2020, pp. 12–29.
- Wagner P., Ray R., Hart K., Little B. Microbiological degradation of stressed fiber-reinforced polymeric composites. Materials Perfomance, 1996, vol. 35, pp. 79–82.
- Breister A.M., Imam M.A., Zhichao Zho et al. Soil microbiomes mediate degradation of vinyl ester-based polymer composites. Communication Materials, 2020, vol. 1 (101), pp. 1–15.
- Wagner P.A., Ray R.I., Little B.J. Microbiologically Influenced Degradation of Fiber Reinforced Polymeric Composites. Materials Perfomance, 1996, vol. 33, no. 4, pp. 46–49.
- Gu J.D. Microbial colonization of polymeric materials for space applications and mechanisms of biodeterioration: A review. International Biodeterioration & Biodegradation, 2007, vol. 59, pp. 170–179.
- Gu J.-D., Gu J.-G., Liu J., Cheng S.-P. Sensitive Detection on Polyimides Degradation by Microorganisms Using Electrochemical Impedance Spectroscopy. Microbes and Environments, 2002, vol. 17, no. 2, pp. 105–112.
- Gu J.-D. Biodeterioration of synthetic polymeric materials: A review. International Biodeterioration & Biodegradation, 2003, vol. 52, pp. 69–91.
- Mitchell R. A Study of Microbial Deterioration of Fiber Reinforced Composites and Protective Coatings. Washington DC: Air Force Office of Scientific Research, 1998, 22 p.
- Triverdi J.P., Chatterjee R.C. Biodeterioration of aramid fibre by Anthrenus flavipes. Journal of Materials Science Letters, 1989, vol. 8, pp. 605–607.
- Solovskii M.V., Dubkova V.I., Krutko N.P. Antimicrobial activity of carbon fiber tissues modified with a polymeric complex of the antibiotic gentamicin. Prikladnaya biokhimiya i mikrobiologiya, 2009, vol. 45, no. 2, pp. 248–251.
- Zhukovsky V.A., Khokhlova V.A., Anushchenko T.Yu. Silver-containing antimicrobial materials based on carbon and polyvinylidene fluoride fibers. Rossiyskiy khimicheskiy zhurnal, 2011, vol. 55, no. 3, pp. 24–27.
- Ezeonu I.M., Noble J.A., Simmons R.B. et al. Effect of relative humidity on fungal colonization of fiberglass insulation. Applied and Environmental Microbiology, 1994, vol. 60, pp. 2149–2151.
- Krivushina A.A., Sevastyanov D.V., Shein E.A., Daskovsky M.I., Usagawa Z., Avilleira G.P., Ba-tista M.G. Study for destructive influence of micromycete strains, isolated under climatic conditions of the Republic of Сuba, on polymer film materials. Trudy VIAM, 2021, no. 4 (98), paper no. 12. Available at: http://www.viam-works.ru (accessed: January 31, 2021). DOI: 10.18577/2307-6046-2021-0-4-141-150.
- Krivushina A.A., Startsev V.O. Micromycetes-destructors of polymeric materials among extremophilic microorganisms (review). Trudy VIAM, 2022, no. 1 (107), paper no. 12. Available at: http://www.viam-works.ru (accessed: 31 January, 2022). DOI: 10.18557/2307-6046-2022-0-1-123-134.