Modification of the surface of carbon reinforcing fillers for polymer composite materials by electrochemical treatment (review)
Sidorina A.I. Modification of the surface of carbon reinforcing fillers for polymer composite materials by electrochemical treatment (review) // Proceedings of VIAM. 2022. No. 4. DOI: 10.18577/2307-6046-2022-0-4-61-74. URL: https://viam-works.ru/en/journal/2022/4/7
Keywords
carbon fibers, reinforcing fillers, adhesion, interphase interaction, modification, polymer matrices, composite material, carbon plastic, carbon composite, electrochemical treatment, electrochemical oxidation
Abstract
A method for increasing the adhesive interaction at the interface between a carbon fiber reinforcing filler and a polymer matrix in polymer composite materials by modifying the filler surface by electrochemical treatment is considered. The methods used to characterize the surface of the origin and modified fibers are listed. The features of the electrochemical oxidation process of carbon fibers are shown. The main advantages and disadvantages of this modification method are given. An overview of the results of studies of electrochemical oxidation of carbon reinforcing filler use to improve the mechanical characteristics of carbon plastics is given.
Reference list
- Varshavsky V.Ya. Carbon fibres. Moscow: Varshavsky V.Ya., 2007, 496 p.
- Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
- Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 18, 2021). DOI: 10.18577/2713-0193-2021-0-3-105-116.
- Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products. Trudy VIAM, 2020, no. 12 (94), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 8, 2021). DOI: 10.18577/2307-6046-2020-0-12-47-58.
- Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Meleshko A.I., Polovnikov S.P. Carbon, carbon fibers, carbon composites. Moscow: Science-press, 2007, 192 p.
- Zhelezina G.F., Solovieva N.A., Kulagina G.S., Shuldeshova P.M. Study of the possibility of increasing the impact resistance of thin-sheeted carbon fiber-reinforced plastics due to clading with aramid organoplastics. Aviation materials and technologies, 2021, no. 4 (65), paper no. 04. Available at: http://www.journal.viam.ru (accessed: October 20, 2021). DOI: 10.18577/2713-0193-2021-0-4-35-42.
- Sidorina A.I., Gunyaeva A.G. Modification of Surface of Reinforsing Carbon Fillers for Polymeric Composite Materials by Plasma Treatment (Review). Fibre Chemistry, 2017, vol. 49, no. 1, pp. 24–27.
- Mikhailin Yu.A. Structural polymeric composite materials. Moscow: Nauchnye osnovy i tekhnologii, 2008, 822 p.
- Carbon fibers and carbon composites. Ed. E. Fitzer. Moscow: Mir, 1988, 338 p.
- Zhang X., Pei X., Jia Q., Wang Q. Effects of CFs surface treatment on the tribological properties of 2D woven carbon fabric/polyimide composites. Applied Physics A, 2009, vol. 95, pp. 793–799.
- Tiwari S., Bijwe J. Surface treatment of carbon fibers – a review. Procedia Technology, 2014, vol. 14, pp. 505–512.
- Vautard F., Ozcan S., Meyer H. Properties of thermos-chemically surface treated carbon fibers and their epoxy and vinyl ester composites. Composites: Part A, 2012, vol. 43, pp. 1120–1133.
- Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
- Zhang J. Different surface treatments of carbon fibers and their influence on the interfacial properties of carbon fiber/epoxy composites. Paris, 2012. Available at: https://tel.archives-ouvertes.fr/tel-01146459 (accessed: July 15, 2021).
- Mahltig B., Kyosev Y. Inorganic and Composite Fibers: Production, Properties, and Applications. Woodhead Publishing, 2018. 343 p.
- Garifullin A.R., Abdullin I.Sh. The current state of the problem of surface treatment of carbon fibers for their subsequent use in polymer composites as a reinforcing element. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2014, no. 7. Available at: https://cyberleninka.ru/article/sovremennoe-sostoyanie-problemy-poverhnostnoy-obrabotki-uglerodnyh-volokon-dlya-posleduyushego-ih-prime-neniya-v-polimernyh (accessed: June 08, 2021).
- Eyckens D.J., Arnold C.L., Simon Z. et al. Covalent sizing surface modification as a route to improved interfacial adhesion in carbon fiber-epoxy composites. Composites: Part A, 2021, vol. 140, pp. 1–7.
- Yuan X., Zhu B., Cai X. et al. Influence of different surface treatments on the interfacial adhesion of graphene oxide/carbon fiber/epoxy composites. Applied Surface Science, 2018, vol. 458, pp. 996–1005.
- Park S.-J., Kim M.-H. Effect of acidic anode treatment on carbon fibers for increasing fiber-matrix adhesion and its relationship to interlaminar shear strength of composites. Journal of Material Science, 2000, vol. 35, pp. 1901–1905.
- Comprehensive Composite Materials. Еd. T.-W. Chow. Oxford: Pergamon Press, 2000, vol. 1: Fiber reinforcements and general theory of composite, 824 p.
- Ma Y.J., Wang J.L., Cai X.P. The Effect of Electrolyte on Surface Composite and Microstructure of Carbon Fiber by Electrochemical Treatment. International Journal of Electrochemical Science, 2013, vol. 8, pp. 2806–2815.
- Gulyas J., Foldes E., Lazar A., Pukanszky B. Electrochemical oxidation of carbon fibers: surface chemistry and adhesion. Composites: Part A, 2001, vol. 32, pp. 353–360.
- Wang Y.Q., Zhang F.Q., Sherwood P.M. Interfacial interactions between polyvinyl alcohol and carbon fiber electrochemically oxidized in nitric acid solution. Chemistry of Materials, 1999, vol. 11, pp. 2573–2583.
- Bismarck A., Kumru M.E., Springer J., Simitzis J. Surface properties of PAN-based carbon fibers tuned by anodic oxidation in different alkaline electrolyte systems. Applied Surface Science, 1999, vol. 143, pp. 45–55.
- Qian X., Zhi J., Chen L. et al. Effect of low current density electrochemical oxidation on the properties of carbon fiber-reinforced epoxy resin composites. Surface and Interface Analysis, 2012, vol. 45, pp. 937–942.
- Waseem S.F., Gardner S.D., He G.R. et al. Adhesion and surface analysis of carbon fibres electrochemically oxidized in aqueous potassium nitrate. Journal of Materials Science, 1998, vol. 33, pp. 3151–3162.
- Gubanov A.A. Development of the process of electrochemical modification of the surface of carbon fiber in order to increase the strength of carbon fiber: thesis, Cand. Sc. (Tech.). Moscow, 2015. Available at: https://diss.muctr.ru/author/82/ (аccessed: September 8, 2021).
- Liu J., Tian Y., Chen Y., Liang J. Interfacial and mechanical properties of carbon fibers modified by electrochemical oxidation in (NH4HCO3)/(NH4)2C2O4·H2O aqueous compound solution. Applied Surface Science, 2010, vol. 256, pp. 6199–6204.
- Guo Y., Liu J., Liang J. Surface state of carbon fibers modified by electrochemical oxidation. Journal of Materials Science and Technology, 2005, vol. 21, pp. 371–375.
- Bondaletova L.I., Bondaletov V.G. Polymer composite materials: textbook. Tomsk: Tomsk Publishing House Polytechnic University, 2013, part 1, 118 p.
- Moshonov A., Li H., Muzzy J.D. Electrochemical surface treatment of carbon fibers. 36th Int. SAMPE Symposium, 1991, vol. 36, pp. 1787–1801.
- Donnet J.B., Bansal R.C. Carbon Fibers. 2nd ed. New York: Marcel Dekker, 1990. 470 p.
- Borman V.D., Varshavsky V.Ya., Kvanin A.L. Segregation of impurities on the surface of carbon fiber during electrochemical processing. Kompozity i nanostruktury, 2011, no. 3, pp. 24–35.
- Ma Q., Gu Y., Li M., Wang S., Zhang Z. Effects of surface treating methods of high-strength carbon fibers on interfacial properties of epoxy resin matrix composite. Applied Surface Science, 2016, vol. 379, pp. 199–205.
- Raphael N., Namratha K., Chandrashekar B.N. et al. Surface modification and grafting of carbon fibers: A route to better interface. Progress in Crystal Growth and Characterization of Materials, 2018, vol. 64, pp. 75–101.
- Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.