Changes in the structure of oxide ceramic fibers when exposed to high temperature heats

Stepanova E.V., Maximov V.G., Ivakhnenko Yu.A.
Stepanova E.V., Maximov V.G., Ivakhnenko Yu.A. Changes in the structure of oxide ceramic fibers when exposed to high temperature heats // Proceedings of VIAM. 2022. No. 4. DOI: 10.18577/2307-6046-2022-0-4- 42-51. URL: https://viam-works.ru/en/journal/2022/4/5
Keywords
oxide ceramic fibers, structure, sol-gel method, temperature, optical microscopy, recrystallization
Abstract

Using the method of transmission optical microscopy in polarized light, changes in the internal structure of various oxide ceramic fibers under the influence of high-temperature heats were investigated. Complete restructuring of the structure of all examined fibers in the process of high-temperature exposure was revealed. Significant differences were established during recrystallization between fibers of different types. Mullite compositions showed stabilization of the recrystallization structure at the stage of formation of moderately large grains separated by stable large-angle (up to 90°) borders.

Reference list
  1. Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg: 2019, vol. 4, p. 24.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Brautmans L. Modern composite materials. Moscow: Mir, 1970, 670 p.
  5. Istomin A.V., Kolyshev S.G. Processing of wastes high-temperature heat-protective material. Trudy VIAM, 2021, no. 1 (95), paper no. 10. Available at: http://www.viam-works.ru (accessed: August 15, 2021). DOI: 10.18577/2307-6046-2021-0-1-97-104.
  6. Ermolenko I.N., Ulyanova T.M., Vityaz P.A., Fedorova I.L. Fibrous high temperature materials. Minsk: Nauka i tekhnika, 1991, 255 p.
  7. Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
  8. Babashov V.G., Varrik N.M. Zirconia fibers as a component of high temperature thermal insulation (review). Trudy VIAM, 2021, no. 10 (104). paper no. 08. Available at: http://www.viam-works.ru (accessed: November 18, 2021). DOI: 10.18577/2307-6046-2021-0-10-79-86.
  9. Chernyak M.G. Continuous glass fiber. Fundamentals of technology and properties. Moscow: Khimiya, 1965, 320 p.
  10. Kostikov V.I., Varenkov A.N. Ultra-high temperature composite materials. Moscow: Intermet Inzhiniring, 2003, 563 p.
  11. Shavnev A.A., Babashov V.G., Varrik N.M. Continuous fibers based on alumina (review). Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 27–34. DOI: 10.18577/2071-9140-2020-0-4-27-34.
  12. Afanasov I.M., Lazoryak B.I. High temperature ceramic fibers. Moscow: Lomonosov Moscow State University, 2010, 51 p.
  13. Perepelkin K.E. The fibers are inorganic. Moscow: Bolshaya rossiyskaya entsiklopediya, 2006, vol. 5. 663 p.
  14. Fibers from oxide ceramics: pat. no. 2396388 Rus. Federation; filed 10.02.10; publ. 10.08.10.
  15. Alumina fiber: pat. US 3808015A; filed. 12.05.72; publ. 30.04.74.
  16. Preparation of inorganic oxide monofilaments: pat. US3311689A; filed. 17.01.63; publ. 28.03.68.
  17. Pakshver A.B. Physical and chemical bases of technology of chemical fibers. Moscow: Khimiya, 1972, 432 p.
  18. Method for producing high-temperature fiber based on aluminum oxide: pat. no. 2212388 Rus. Federation; filed 19.11.01; publ. 20.09.03.
  19. Method for obtaining polycrystalline inorganic fibers: pat. no. 2170293 Rus. Federation; filed 16.07.99; publ. 10.07.01.
  20. Zimichev A.M., Varrik N.M., Sumin A.V. On the issue of obtaining ceramic threads based on refractory oxides. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 3, paper no. 09. Available at: http://www.materialsnews.ru (accessed: July 7, 2021).
  21. Moshnikov V.A., Tairov Yu.M., Khamova T.V., Shilova O.A. Sol-gel technology of micro- and nanocomposites: textbook. Ed. O.A. Shilova. St. Petersburg: Lan, 2013, 304 p.
  22. Maksimov A.I., Moshnikov V.A., Tairov Yu.M., Shilova O.A. Fundamentals of sol-gel technology of nanocomposites. St. Petersburg: Elmor, 2007, 255 p.
  23. Grashchenkov D.V., Balinova Yu.A., Tinyakova E.V. Ceramic fibers of aluminum oxide and materials based on them. Steklo i keramika, 2012, no. 4, pp. 32–35.
  24. Kablov E.N., Shchetanov B.V., Ivakhnenko Yu.A. Obtaining, structure and strength of Al2O3 fibers. International conf. "Theory and practice of technologies for the production of products from composite materials and new metal alloys". Moscow: Znanie, 2003, pp. 194–196.
  25. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and properties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
  26. Sirotin Yu.I., Shaskolskaya M.P. Fundamentals of crystal physics. Moscow: Nauka, 1979, 24 p.
  27. Martakov I.S. Morphology and properties of aluminum and titanium oxides obtained by template synthesis using cellulose and its derivatives: thesis, Cand. Sc. (Chem.). Syktyvkar: Institute of Chemistry, Komi Scientific Center, Ural Branch of the Russian Academy of Sciences, 2017, 133 p.
  28. Ishchenko V.V. Influence of aggregation on the evolution of the microstructure of oxide powders in the processes of synthesis, heat treatment and sintering: thesis, Cand. Sc. (Chem.). Moscow: IONKh RAN, 2000, 111 p.