A. V. Nesolenov, T. V. Pavlova, O. S. Kashapov, A. R. Kondratyeva, V. S. Kalashnikov Prospects for manufacturing compressor blade group forgings from heat-resistant titanium alloys VT41 and VT46 via isothermal hot deformation // Proceedings of VIAM. 2026. No. 10 (164). С. 65-89. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-65-89.

Prospects for manufacturing compressor blade group forgings from heat-resistant titanium alloys VT41 and VT46 via isothermal hot deformation

A. V. Nesolenov1, T. V. Pavlova1, O. S. Kashapov1, A. R. Kondratyeva1, V. S. Kalashnikov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The article examines industrially applicable manufacturing processes for high-pressure compressor blades made of titanium alloys – specifically those with the most widely used dimensions and a «dovetail» root design. The article presents the results of experimental studies on the microstructure and mechanical properties of starting materials – bars and forgings (both individual and group forgings) made from heat-resistant titanium alloys VT41 and VT46, produced via various manufacturing routes. The study demonstrates the feasibility of achieving high mechanical properties and technical-economic indicators for the manufacture of high-pressure compressor blades from VT41 and VT46 alloys using group blanks.

Keywords
titanium alloys, compressor blades, machining, isothermal forging, heat treatment, mechanical properties

Reference list
  1. Krymov V.V., Eliseev Yu.S., Zudin K.I. Production of gas turbine engine blades. Moscow: Mashinostroyenie / Mashinostroyenie-Polet, 2002, 376 p.
  2. Sutyagin A.N. Modern problems of aircraft engine production technology: lecture notes. Rybinsk: RGATU, 2016, 142 p.
  3. Dyakonov G.S., Yakovleva T.V., Stotsky A.G. et al. Thermal stability and mechanical properties of ultrafine-grained titanium alloy VTSM-1. XXV Ural School of Metallurgical Thermal Scientists «Current Problems of Physical Metallurgy of Steels and Alloys»: collection of abstract report. Ekaterinburg: Ural Univ. Publ. House, 2020, pp. 17–19.
  4. Kandarov I.V., Salishchev G.A., Pankratov D.L. et al. Study of the effectiveness of using the method of intense plastic deformation in the technological process of obtaining stampings of gas turbine engine compressor blades. Fundamentalyne issledovaniya, 2016, no. 10, pp. 504-508.
  5. Kandarov I.V. Formation of a regulated structure in the VT6 alloy to improve the performance properties of gas turbine engine blades: thesis, abstract Cand. Sc. (Tech.). Naberezhnye Chelny, 2016, 18 p.
  6. Popov A.A., Popova M.A. Isothermal diagrams of the release of silicide and aluminide phases in heat-resistant titanium alloys. Metallovedenie i termicheskaya obrabotka metallov, 2016, no. 11, pp. 23-28.
  7. Zhang J., Peng N., Wang Q., Wang X. A New Aging Treatment Way for Near alpha High Temperature Titanium Alloys. Journal Material Science and Technology, 2009, vol. 25, no. 4, pp. 454-458.
  8. Bolkhovitin M.S., Korolev N.N., Monakhova V.P. Improving the efficiency of precision forging process control in the manufacture of gas turbine engine compressor blades. Trudy MAI, 2015, no. 81, pp. 1-13.
  9. Strugovets S.A., Krivosheev I.A., Galiulin R.M. et al. Development of a method for parametric diagnostics of the technical condition of gas turbine engines based on the analysis of blade erosion and compressor performance trends. Vestnik UGATU, 2010, vol. 14, no. 4 (39), pp. 3-10.
  10. Gishvarov A.S., Aitov R.R., Aitumbetov A.M. Investigation of the efficiency of dust protection devices for helicopter gas turbine engines. Vestnik UGATU, 2015, vol. 19, no. 2 (68), pp. 100-110.
  11. Korsunov K.A., Ashikhmina E.A. Analysis of certain physicochemical characteristics of the (TiZr)N ion-plasma coating on compressor rotor blades of the TV3-117 gas turbine engine. Avtomaticheskaya svarka, 2014, no. 2, pp. 49-54.
  12. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 71-81.
  13. Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Hardening of the surface of titanium alloys by ion implantation method and ionic modification. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 33-39. DOI: 10.18577/2071-9140-2018-0-2-33-39.
  14. Ratenko V.D., Simkin E.L. Operational characteristics of the TV3-117 turboshaft engine. Nauchnyi vestnik GOSNII GA, 2016, no. 15 (326), pp. 82-91.
  15. Abdelvakhid M.B. Methodology for assessing the impact of climatic conditions and erosive wear on the performance of augmented turbofan engines: thesis, Cand. Sc. (Tech.). Moscow, 2015, 175 p.
  16. Nikhamkin M.Sh., Semenova I.V. Probabilistic assessment of gas turbine engine compressor blade resistance to foreign object damage. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta im. akademika S.P. Koroleva (natsionalnogo issledovatel'skogo universiteta), 2009, no. 3-2, pp. 93-97.
  17. Valiev A.I. Comparative analysis of gas turbine engine compressor blade manufacturing. Fundamentalnye issledovaniya, 2017, no. 5, pp. 36-41.
  18. Vorobyev V.M. Precision group forging of individual gas turbine engine compressor blades with finished functional surfaces. Dvigatel, 2010, no. 4 (70), pp. 16-19.
  19. Petrov A.V., Tikhomirov V.V., Donchenko V.V. Influence of the scale factor and boundary conditions on natural frequencies and mode shapes of aviation gas turbine engine blades with various types of root attachments. Vestnik dvigatelestroeniya, 2013, no. 1, pp. 58-64.
  20. Bogdanov A.D., Kalinin N.P., Krivko A.I. TV3-117VM Turboshaft Engine (Design and Maintenance). Moscow: Vozdushny Transport, 2000, 392 p.
  21. Tetyukhin V.V., Shibanov A.S., Puzakov I.Yu. et al. Development of a manufacturing technology for titanium alloy semi-finished products that eliminates defect formation and improves material inspectability. Novosti materialovedeniya. Nauka i tekhnika, 2015, no. 6 (18), pp. 34-38. Available at: https://www.materialsnews.ru (accessed: September 28, 2026).
  22. Inagaki I., Shirai Y., Takechi T., Ariyasu N. Application and Features of Titanium for the Aerospace Industry. Technical Review. Nippon steel & sumitomo metal technical report, 2014, no. 106, pp. 22-27. Available at: https://www.nipponsteel.com/en/tech/report/nssmc/pdf/106-05.pdf (accessed: September 28, 2026).
  23. Yashin M.S., Kapitanenko D.V. Investigation of the structure and properties of the VT3-1 alloy in relation to the technology for obtaining stampings of disks and turbine blades. Trudy VIAM, 2023, no. 8 (126), pp. 52-63. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2023-0-8-52-63.
  24. Yashin M.S., Bazhenov A.R. Investigation of thermomechanical parameters of deformation and mechanical properties depending on conditions of deformation of titanium alloy VT30. Trudy VIAM, 2024, no. 3 (133), pp. 18-29. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2024-0-3-18-29.
  25. Kablov E.N. The Key Problem: Materials. Trends and Guidelines for Russia's Innovative Development. Moscow: VIAM, 2015, pp. 458-464.
  26. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3-33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  27. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a two-phase titanium alloy of the Ti–Al–Sn–Zr–Si–β-stabilizers system. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30-37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  28. Makushina M.A., Kochetkov A.S., Vinogradov I.D. Statistical evaluation of the homogeneity of the chemical composition of vacuum-arc remelting ingots from economic alloy titanium VT40L. Trudy VIAM, 2022, no. 11 (117), pp. 27-36. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2022-0-11-27-36.
  29. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Modern technologies of plastic working of metals. Trudy VIAM, 2015, no. 2, pp. 15-19. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  30. Ponomarenko D.A., Skugorev A.V., Sidorov S.A., Strokov V.V. Technological capabilities of specialized isothermal presses with forces of 6,3 and 16 MN in the production of aircraft components. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka metallov davleniyem, 2015, no. 9, pp. 36-40.
  31. Belousov M.G., Tsurkal A.A. Investigation of factors influencing damage and failure of aircraft engine compressor blades. Trudy MAI, 2013, no. 65, p. 20.
  32. Senenko S.A., Bogachev I.A., Shoshev F.L. Effect of the fractional composition of the metal-powder composition of the VT6 alloy on the surface roughness, structure and mechanical properties of the printed material obtained by selective electron beam melting. Trudy VIAM, 2024, no. 6 (136), pp. 29-41. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2024-0-6-29-41.
  33. Belyaev M.S., Khvatskiy K.K., Gorbovets M.A. Comparative analysis of national standards of RF and the USA on methods of metals fatigue testing. Trudy VIAM, 2014, no. 9, pp. 140-152. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2014-0-9-11-11.
  34. Putyarskiy S.V., Plokhikh A.I., Arislanov A.A., Naprienko S.A., Anisimova A.Yu. Study of structure and mechanical properties of the laminar structure material based on titanium alloys VT1-0 and VT47. Aviation materials and technologies, 2023, no. 2 (71), pp. 36-50. Available at: http://www.journal.viam.ru (accessed: September 29, 2026). DOI: 10.18577/2713-0193-2023-0-2-36-50.
  35. Gorbovets M.A., Khodinev I.A., Karanov V.A., Yushin V.D. Influence of the type of loading on high-cycle fatigue of heat-resistant alloys. Trudy VIAM, 2019, no. 3 (75), pp. 96-104. Available at: http://www.viam-works.ru (accessed: September 28, 2026). DOI: 10.18577/2307-6046-2019-0-3-96-104.
  36. Yang X., Guo H., Yao Z., Yuan Sh. Effect of