M. V. Turchenko, Yu. E. Lebedeva, A. V. Butuzov, A. S. Chaynikova, M. V. Gamazina, K. I. Svetogorov Production of zirconium oxide-based ceramics by stereolithography // Proceedings of VIAM. 2026. No. 10 (164). С. 197-207. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-197-207.

Production of zirconium oxide-based ceramics by stereolithography

M. V. Turchenko1, Yu. E. Lebedeva1, A. V. Butuzov1, A. S. Chaynikova1, M. V. Gamazina1, K. I. Svetogorov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The potential of laser stereolithography for producing zirconium oxide-based ceramics is considered. A highly filled (83 % by weight) photocurable zirconium oxide-based ceramic paste has been developed, enabling the production of complex ceramic products using laser stereolithography (SLA). The physicochemical and thermophysical properties of the ceramics produced from the zirconium oxide-based paste by SLA are comparable to those of ceramics produced by traditional methods.

Keywords
3D printing, laser stereolithography, zirconium oxide, additive manufacturing, ceramic pastes, dense ceramics



Reference list
  1. Zhitnyuk S.V., Medvedev P.N., Sorokin O.Yu., Kachaev A.A. Formation of crystallographic texture in polycrystalline ceramics as a way to enhance properties (review). Trudy VIAM, 2022, no. 5 (111), pp. 74-86. Available at: http://www.viam-works.ru (accessed: April 08, 2026). DOI: 10.18577/2307-6046-2022-0-5-74-86.
  2. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025-2035 (review). Trudy VIAM, 2022, no. 11 (117), pp. 81-92. Available at: http://www.viam-works.ru (accessed: April 08, 2026). DOI: 10.18577/2307-6046-2022-0-11-81-92.
  3. Butuzov A.V., Lebedeva Yu.E., Semina A.V., Serkova E.A., Lonskii S.L. Influence of the nature and concentration of the wetting-dispersing additive on the rheological properties and stability of highly filled ceramic slurries based on aluminum oxide. Trudy VIAM, 2026, no. 4 (158), pp. 85-103. Available at: http://www.viam-works.ru (accessed: April 08, 2026). DOI: 10.18577/2307-6046-2022-0-4-85-103.
  4. Tolmachev Ya.V., Zavarzin S.V., Loshchinina A.O., Knyazev A.V. High temperature oxide corrosion of ceramic materials in turbine engines. Trudy VIAM, 2023, no. 7 (125), pp. 69-83. Available at: http://www.viam-works.ru (accessed: April 08, 2026). DOI: 10.18577/2307-6046-2023-0-7-69-83.
  5. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and properties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54-63. DOI: 10.18577/2071-9140-2020-0-1-54-63.
  6. Kablov E.N. Dominant of the national technological initiative. Metally Eurazii, 2017, no. 3, pp. 2-6.
  7. Bellini A., Shor L., Gueri S.I. New developments in fused deposition modeling of ceramics. Rapid Prototyping Journal, 2005, vol. 11, pp. 214-220.
  8. Gonzalez J.A., Mireles J., Lin Y. et al. Characterization of ceramic components fabricated using binder jetting additive manufacturing technology. Ceramic International, 2016, vol. 42, pp. 10559-10564.
  9. Kirihara S. Additive manufacturing of ceramic components using laser scanning stereolithography. Welding in the World, 2016, vol. 60, pp. 697-702.
  10. Faes M., Vleugels J., Vogeler F. et al. Extrusion-based additive manufacturing of ZrO2 using photoinitiated polymerization. Journal of Manufacturing Science and Technology, 2016, vol. 14, pp. 28-34.
  11. Zhou W., Li D., Chen Z. The influence of ingredients of silica suspensions and laser exposure on uv-curing behavior of aqueous ceramic suspensions in stereolithography. The International Journal of Advanced Manufacturing Technology, 2011, vol. 52, pp. 575-582.
  12. Witkowski S., Lange R. Stereolithography as an additive technique in density. Schweiz Monatsschr Zahmed, 2003, vol. 113 (8), pp. 868-884.
  13. Pfaffinger M., Mitteramskogler G., Gmeiner R. et al. Thermal debinding of ceramic-filled photopolymers. Materials Science Forum, 2015, vol. 825, pp. 75-81.
  14. Xu G., Zhao W., Lu B. Fabrication of microstructures using high-resolution stereolithography system. Journal of Mechanical Engineering, 2005, vol. 9, pp. 86-89.
  15. Xing H., Zou B., Li S. et al. Study on surface quality, precision and mechanical properties of 3D printed ZrO2 ceramic components by laser scanning stereolithography. Ceramics International, 2017, vol. 43 (18), pp. 16340–16347.
  16. Chen Z., Li Z., Li J. et al. 3D printing of ceramics: a review. Journal of the European Ceramic Society, 2019, vol. 39 (4), pp. 130–145.
  17. Zocca A., Colombo P., Gomes C.M. et al. Additive manufacturing of ceramics: issues, potentialities, and opportunities. Journal of the American Ceramic Society, 2015, vol. 98, pp. 1983–2001.
  18. Xu Y., Wu X., Guo X. et al. The boom in 3D-printed sensor technology. Sensors, 2017, vol. 17, pp. 2439–2441.
  19. Wu Z., Liu W., Wu H. et al. Research into the mechanical properties, sintering mechanism and microstructure evolution of Al2O3–ZrO2 composites fabricated by a stereolithography-based 3D printing method. Materials Chemistry and Physics, 2018, vol. 207, pp. 1–10.
  20. Dehurtevent M., Robberecht L., Hornez J.C. et al. Stereolithography: A new method for processing dental ceramics by additive computer-aided manufacturing. Dental Materials, 2017, vol. 33, pp. 477–485.
  21. Falkowski P., Grzelak A. Effect of solvents on curing process of photopolymerizable ceramic suspensions. Archives Metallurgy and Materials, 2013, vol. 58, pp. 1411–1414.
  22. Weng Z., Zhou Y., Lin W. et al. Structure-property relationship of nano enhanced stereolithography resin for desktop SLA 3D printer. Composites, 2016, vol. 88, pp. 234–242.
  23. Griffith M.L., Halloran J.W. Freeform fabrication of ceramics via stereolithography. Journal of the American Ceramic Society, 2005, vol. 79, pp. 2601–2608.
  24. De Camargo I.L., Morais M.M., Fortulan C.A. A review on the rheological behavior and formulations of ceramic suspensions for vat photopolymerization. Ceramics International, 2021, vol. 47, pp. 11906–11921.
  25. Zakeri S., Vippola M., Levanen E. A comprehensive review of the photopolymerization of ceramic resins used in stereolithography. Additive Manufacturing, 2020, vol. 35, pp. 101–177.
  26. Manapat J.Z., Chen O., Ye P. et al. 3D printing of polymer nanocomposites via stereolithography. Macromolecular Materials and Engineering, 2017, vol. 302 (9), pp. 1–13.