M. D. Panteleev, A. V. Sviridov, Z. S. Dementev, A. M. Rogalev, M. V. Lobanova Features of laser cleaning of aluminum alloy // Proceedings of VIAM. 2026. No. 10 (164). С. 54-64. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-54-64.

Features of laser cleaning of aluminum alloy

M. D. Panteleev1, A. V. Sviridov1, Z. S. Dementev1, A. M. Rogalev1, M. V. Lobanova1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

This article considers features of laser surface cleaning of the aluminum alloy. A metallographic assessment of the surface layer structure was carried out, and roughness parameters were measured under various laser exposure conditions. The thickness of the layer removed per laser beam pass was determined. Based on the obtained experimental data, a graph of the roughness dependence on power was plotted, which made it possible to identify the optimal cleaning modes providing minimal roughness at stable material removal depth. It has been shown that laser cleaning is an effective method for surface finishing.

Keywords
aluminum alloy, laser cleaning, selective laser melting, metallography, surface roughness, thickness of the removed layer
Reference list
  1. DeBroy T., Wei H.L., Zuback J.S. et al. Additive manufacturing of metallic components - Process, structure and properties. Progress in Materials Science, 2018, vol. 92, pp. 112-224. DOI: 10.1016/j.pmatsci.2017.10.001.
  2. Dobrynin D.A., Pavlova T.V. Electrolyte-plasma polishing of parts made by selective laser sintering from metal powder composition of aluminum alloy grade VAS1. Part 1. Trudy VIAM, 2023, no. 12 (130), pp. 19-27. Available at: http://www.viam-works.ru (accessed: August 20, 2026). DOI: 10.18577/2307-6046-2023-0-12-19-27.
  3. Herzog D., Seyda V., Wycisk E. et al. Additive manufacturing of metals. Acta Materialia, 2016, vol. 117, pp. 371-392. DOI: 10.1016/j.actamat.2016.07.019.
  4. Kozlov I.A., Volkov I.A., Fomina M.A., Zakharov K.E. Features of chemical oxidation of semi-finished products obtained by selective laser melting from a metal powder composition of the alloy VAS1. Trudy VIAM, 2023, no. 11 (129), pp. 90-98. Available at: http://www.viam-works.ru (accessed: August 21, 2026). DOI: 10.18577/2307-6046-2023-0-11-90-98.
  5. Shiganov I.N., Kuleshov S.S., Smirnova N.A. Application of laser additive surfacing in the manufacture of aluminum alloy components. Svarozhnye proizvodstvo, 2018, no. 7, pp. 27-32.
  6. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3-11. DOI: 10.18557/2071-9140-2020-0-4-3-11.
  7. Veiko V.P., Dyshlovenko S.S. Laser Microstructuring of Surfaces. Nauchno-tekhnicheskiy vestnik Sankt-Peterburgskogo gosudarstvennogo instituta tochnoy mekhaniki i optiki, 2001, no. 4, p. 119.
  8. Gogoleva V.D., Kuznetsova P.E., Kuko I.S., Mazalova T.A., Bogachev I.A. Structure and properties investigations of the synthesized steel material of Fe-Cr-Ni-Co-Mo system, obtained by selective laser melting after different heat treatments. Trudy VIAM, 2026, no. 7 (161), pp. 63-75. Available at: http://www.viam-works.ru (accessed: August 21, 2026). DOI: 10.18577/2307-6046-2026-0-7-63-75.
  9. Effect of surface cleaning technology on porosity in welds of Al-Mg alloy sheets. Zagotovitelnye proizvodstva v mashinostroyenii, 2026, no. 1, pp. 7-13.
  10. Cui Z., Xu J., Xiong Y. et al. A Review of Laser Cleaning Technology: Mechanisms, Applications, and Performance Analysis. Journal of Physics: Conference Series, 2026, vol. 3270, art. 012025. DOI: 10.1088/1742-6596/3270/1/012025.
  11. Dozhdelev A.M., Lavrentyev A.Yu., Kakorin D.D., Tulyaev I.P. Laser cleaning of metal products. International Journal of Humanities and Natural Sciences, 2022, vol. 12-2 (75), pp. 123-125. DOI: 10.24412/2500-1000-2022-12-2-123-125.
  12. Zhu G., Xu Z., Jin Y. et al. Mechanism and application of laser cleaning: A review. Optics and Lasers in Engineering, 2023, vol. 162, art. 107426. DOI: 10.1016/j.optlaseng.2022.107426.
  13. Lee J.M., Watkins K.G., Steen W.M. Laser cleaning of aluminum alloy surface. Applied Surface Science, 2000, vol. 154-155, pp. 523-528. DOI: 10.1016/S0169-4332(99)00445-5.
  14. Turner M.W., Crouse P.L., Li L. Comparison of mechanisms and effects of Nd:YAG and excimer laser cleaning. Applied Surface Science, 2006, vol. 252, no. 13, pp. 4792-4802. DOI: 10.1016/j.apsusc.2005.07.024.
  15. Zhou Y., Li Q., Zhang H. et al. Advances in laser cleaning technology for aluminum alloys. Journal of Materials Research and Technology, 2023, vol. 24, pp. 5678-5695. DOI: 10.1016/j.jmrt.2023.04.150.
  16. Li Y., Guo L., Jiang P. et al. Experimental Study on Surface Morphology Changes of Aluminum Alloy Using Laser Cleaning and Optimization of Process Parameters. Chinese Journal of Lasers, 2021, vol. 48, no. 22, art. 2202016. DOI: 10.3788/CJL202148.2202016.
  17. Grigoryants A.G., Shiganov I.N., Misyurov A.I. Laser Processing Technologies. Moscow: Bauman Moscow State Techn. Univ., 2018, 664 p.
  18. Wang W., Kou J., Zhong J. et al. Effect of Scanning Speed on Surface Quality and Corrosion Resistance of 7075 Aluminum Alloy in Laser Cleaning. Metals and Materials International, 2026, vol. 32, no. 7, p. 2357. DOI: 10.1007/s12540-025-02026-2.
  19. Gu Z., Wang T., Feng W. et al. Experimental and process parameter optimization study of laser cleaning of aluminum alloy surface paint layers. Journal of Optoelectronics Laser, 2025, vol. 36, no. 2, pp. 208.
  20. Shoshev F.L., Bogachev I.A., Suhov D.I. The features of processing an aluminum matrix composite material by selective laser melting. Trudy VIAM, 2023, no. 11 (129), pp. 66–76. Available at: http://www.viam-works.ru (accessed: August 21, 2026). DOI: 10.18577/2307-6046-2023-0-11-66-76.
  21. Razab M.K.A.A., Noor A.M., Jaafar M.S. et al. A review of incorporating Nd:YAG laser cleaning principal in aerospace industry. Journal of Radiation Research and Applied Sciences, 2018, vol. 11, no. 1, pp. 1–10. DOI: 10.1016/j.jrras.2017.08.001.
  22. Sukhov D.I., Nerush S.V., Efimochkin I.Yu., Karachevchev F.N., Bogachev I.A. Production of MMC based on VZh159 alloy by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), pp. 62–72. Available at: http://www.journal.viam.ru (accessed: August 24, 2026). DOI: 10.18577/2713-0193-2021-0-2-62-72.
  23. State Standard R ISO 25178-2–2014. Geometrical product specifications (GPS). Surface texture: areal. Part 2. Terms, definitions and surface texture parameters. Moscow: Standartinform, 2014, 25 p.
  24. State Standard 2789–73. Surface roughness. Parameters and characteristics. Moscow: Standartinform, 1973, 10 p.
  25. Yao D., Ma Y., Zhao S., Shan Y. Effect of laser incidence angle on the removal of non-uniform paint surface of 6061 aluminum alloy. Laser Technology, 2025, vol. 49, no. 3, p. 424.
  26. Daurelio G., Chita G., Cinquepalmi M. Laser surface cleaning of aluminum alloys. Journal of Materials Processing Technology, 1998, vol. 75, no. 1–3, pp. 1–6. DOI: 10.1016/S0924-0136(97)00272-2.
  27. Kumar A., Sapp M., Ott J. et al. Laser cleaning of aerospace aluminum alloys: An experimental study. Journal of Laser Applications, 2020, vol. 32, no. 2, art. 022013. DOI: 10.2351/7.0000065.