E. S. Afanasyeva, A. V. Sviridov, M. D. Panteleev, K. N. Popov Research of the structure and properties of welded joints of synthesized materials based on nickel, cobalt, titanium and iron // Proceedings of VIAM. 2026. No. 10 (164). С. 14-32. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-14-32.

Research of the structure and properties of welded joints of synthesized materials based on nickel, cobalt, titanium and iron

E. S. Afanasyeva1, A. V. Sviridov1, M. D. Panteleev1, K. N. Popov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The article presents the results of argon-arc welding technology of heat-resistant nickel, cobalt, and titanium based alloys, synthesized by selective laser melting. The study addresses similar and dissimilar joints of synthesized materials with wrought alloys used in manufacture and repair of hot-section components of PD series gas turbine engines. The welding parameters were optimized for KKh28M6, Kh15N5D4B, VT6-PS alloys as well as for dissimilar joints with steel 12Kh18N10T. The microstructure and mechanical properties after repair build-up welding were analyzed. The effect of thermal cycles on welds strength was established.

Keywords
selective laser melting, heat-resistant alloys, gas turbine engine, argon-tungsten arc welding, microstructure, mechanical properties, build-up welding

Reference list
  1. Gorbovets M.A., Khodinev I.A., Monin S.A. Influence of average cycle stress on characteristics of low-cycle fatigue of high-temperature nickel alloy VZh175. Aviation materials and technologies, 2023, no. 1 (70), pp. 126–136. Available at: http://www.journal.viam.ru (accessed: August 23, 2026). DOI: 10.18577/2713-0193-2023-0-1-126-136.
  2. Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New-generation materials and digital additive manufacturing technologies for critical components at FSUE VIAM. Part 1. Materials and synthesis technologies. Elektrometallurgiya, 2022, no. 1, pp. 2–12.
  3. Min P.G., Vadeev V.E., Kolesnikov S.I., Chemov D.A. The effect of impurities on mechanical and operational properties of the cast nickel-base superalloy VZhM200. Trudy VIAM, 2024, no. 10 (140), pp. 13–23. Available at: http://www.viam-works.ru (accessed: August 23, 2026). DOI: 10.18577/2307-6046-2024-0-10-13-23.
  4. Mostafa A., Rubio I.P., Brailovski V. et al. Structure, Texture and Phases in 3D Printed IN718 Alloy Subjected to Homogenization and HIP Treatments. Metals, 2017, no. 7, pp. 196–219. DOI: 10.3390/met7060196.
  5. Narsky A.R., Deynega G.I., Kuzmina I.G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: August 23, 2026). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  6. El-Bagoury N., Hessien M.M., Alsawat M. et al. Optimization of Microstructure and Mechanical Properties of Hipped Inconel 718 by Various Heat Treatment Processes. Metallography, Microstructure, and Analysis, 2019, no. 8, pp. 642–655. DOI: 10.1007/s13632-019-00568-7.
  7. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New-generation materials and digital additive manufacturing technologies for critical components at FSUE «VIAM». Part 3. Adaptation and development of materials. Elektrometallurgiya, 2022, no. 4, pp. 15–25.
  8. Loshchinin Yu.V., Pakhomkin S.I., Razmakhov M.G. Phase transformation temperatures and calorimetric analysis of powder compositions of nickel-based superalloys. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 79–85. DOI: 10.18577/2071-9140-2020-0-1-79-85.
  9. Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New-generation materials and digital additive technologies for the production of critical service-life components at FSUE VIAM. Part 2. Compensation and control of deviations, HIP, and heat treatment. Elektrometallurgiya, 2022, no. 2, pp. 2–12.
  10. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S. New-generation materials and digital additive technologies for the production of critical service-life components at FSUE VIAM. Part 4. Development of heat-resistant materials. Elektrometallurgiya, 2022, no. 5, pp. 8–19.
  11. Knyazev A.E., Min P.G. Comparison of characteristics of VZhL718 alloy metal powder compositions produced by PREP and VEGA methods after selective laser melting. Metallurg, 2024, no. 4, pp. 48–58.
  12. Min P.G., Vadeev V.E., Rogalev A.M., Knyazev A.E. Investigation of the chemical composition, structure, and mechanical properties of EP648 alloy at various stages of additive manufacturing. Materialovedenie, 2018, no. 12, pp. 17–22.
  13. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30–41. Available at: http://www.journal.viam.ru (accessed: August 23, 2026). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  14. Weldable oxidation resistant nickel-iron-chromium-aluminium alloy: pat. 8506883 US; appl. 12.12.07; publ. 18.06.09.
  15. Nickel-chromium-iron-aluminium alloy: pat. 4671931 US; appl. 11.05.84; publ. 09.06.87.
  16. Superalloy repair welding using multiple alloy powders: pat. 8618434 US; appl. 22.03.10; publ. 22.09.11.
  17. Repaired turbine exhaust strut heat shield vanes and repair methods: pat. 8083465 US; appl. 05.09.08; publ. 11.03.10.