Borisova E.A., Pavlukovich N.G., Ivanov M.S., Morozova V.S., Mekalina I.V. Vibration absorbing materials for aviation.. Part 2. The influence of external factors on damping properties of polymer materials in a viscoelastic state // Proceedings of VIAM. 2026. No. 8 (162). С. 68-81. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-8-68-81.
Vibration absorbing materials for aviation.
Part 2. The influence of external factors on damping properties of polymer materials in a viscoelastic state
Abstract
A comprehensive analysis of the factors determining the vibration-absorbing capacity of polymers in the viscoelastic state has been carried out. The influence of temperature and frequency on the relaxation properties of polymers has been studied, and the application of the time-temperature equivalence principle for predicting material behavior over a wide frequency range has been substantiated. To control dissipative properties, such polymer modification strategies as the combination of several polymers, the creation of the phase structure, and the reinforcement of the polymer with fillers are described.
Keywords
viscoelastic state, vibration absorption, damping, dissipation, relaxation, vibration-damping materials, temperature-time equivalence principle, Deborah criterion
Reference list
- Mikhailin Yu.A. Structural polymer composite materials. 2nd ed. St. Petersburg: Scientific Foundations and Technologies, 2010, 822 p.
- Ionov A. V. Means of reducing vibration and noise on ships. St. Petersburg: Krylov Central Research Institute, 2000, 368 p.
- Kablov E. N., Antipov V. V. The role of new-generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiskyok akademii nauk, 2023, vol. 93, no. 10, pp. 907-916.
- Bert C.W. Composite materials: a survey of damping capacity of fiber reinforced composites. Damping Applications for Vibration Control. Ed. P.J. Torvik. New York, 1980, pp. 53-63.
- Gibson R.F. Dynamic mechanical properties of advanced composite materials and structures: a Review. Shock & Vibration Digest. 1987, vol. 19, no. 7, pp. 13-22.
- Zinoviev P.A., Ermakov Yu.N. Characteristics of energy dissipation during vibrations in structural elements made of fiber composites (review). Moscow: Central Research Institute of Scientific and Technical Information, 1989, 76 p.
- Corcaro R.D., Sperling L.H. Relation of polymer chemical composition to acoustic damping. Sound and vibration damping with polymers: ACS Symposium series. Washington: American Chemical Society, 1990, vol. 424, pp. 317-345. DOI: 10.1021/bk-1990-0424.
- Mohan D. Rao Recent applications of viscoelastic damping for noise control in automobiles and commercial airplanes. Journal of Sound and Vibration, 2003, vol. 262, is. 3, pp. 457-474. DOI: 10.1016/S0022-460X(03)00106-8.
- Kuleznev V.N., Shershnev V.A. Chemistry and physics of polymers. 2nd ed., rev. and add. Moscow: KolosS, 2007, 367 p.
- Kolesnikov V.I., Chernyshev S.L., Kolesnikov I.V. et al. Modernization of the low-amplitude friction damper with vacuum ion-plasma coating of friction working surfaces. Aviation materials and technologies, 2024, no. 3 (76), pp. 106-118. Available at: http://www.journal.viam.ru (accessed: January 28, 2026). DOI: 10.18577/2713-0193-2024-0-3-106-118.
- Pavlukovich N.G., Ivanov M.S., Borisova E.A., Morozova V.S., Bolshakov V.A., Mekalina I.V. Vibration absorbing materials for aircraft. Part 1. Mechanism and research methods for damping of polymeric materials. Trudy VIAM, 2026, no. 3 (157), pp. 85-96. Available at: http://www.viamworks.ru (accessed: May 30, 2026). DOI: 10.18577/2307-6046-2026-0-3-85-96.
- Ivanov M.S., Kuleznev V.N. Drop weight testing of polyethylene pipe grades. Plasticheskie massy, 2016, no. 11-12, pp. 23-26.
- Smirnov S.V., Myasnikova M.V. Adaptation of elastic-viscoplastic model for description of rheology of polymer coating material during indentation. Aviation materials and technologies, 2023, no. 3 (72), pp. 78-89. Available at: http://www.journal.viam.ru (accessed: January 28, 2026). DOI: 10.18577/2713-0193-2023-0-3-78-89.
- Nashif A., Jones D., Henderson J. Damping of Vibrations. Trans. from Engl. Moscow: Mir, 1988, 448 p.
- Jones D.I.G. On temperature-frequency analysis of polymer dynamic mechanical behaviour. Journal of Sound and Vibration, 1990, vol. 140, is. 1, pp. 85-102.
- Skuratova T.B., Kirillov S.E., Syatkovsky A.I. Dissipative properties of polymer films and composite materials based on polyvinyl acetate. Zhurnal prikladnoy khimii, 2019, vol. 92, no. 7, pp. 881-887. DOI: 10.1134/S0044461819070090.
- Ivanov M.S., Kuleznev V.N. Method of mechanical spectroscopy of pipe grades of polyethylene. Trudy VIAM, 2016, no. 11 (47), pp. 68-76. Available at: http://www.viam-works.ru (accessed: February 18, 2026). DOI: 10.18577/2307-6046-2016-0-11-9-9.
- Komova N.N., Potapov E.E., Gruskov A.D., Zaikov G.E. Features of the principle of temperature-time equivalence in low-density polyethylene filled with shungite. Vestnik MITKhT, 2013, vol. 8, no. 1, pp. 24-35.
- Malkin A.Ya., Isaev A.I. Rheology: concepts, methods, applications. St. Petersburg: Profession, 2010, 557 p.
- Physical acoustics: in 7 vols. Ed. W. Mason. Moscow: Mir, 1969, vol. 2, part B: Properties of polymers and nonlinear acoustics, 420 p.
- Babkina N.V., Tkalich M.G., Brovko A.A. The Role of Reference Temperature in Constructing Generalized Viscoelastic Functions for Predicting the Damping Properties of Epoxy Polymers. Polimernyy zhurnal, 2015, vol. 37, no. 1, pp. 34-40.
- Ferry J. Viscoelastic Properties of Polymers. Moscow: Foreign Literature Publ. House, 1963, 536 p.
- Syatkovsky A.I., Skuratova T.B., Trofimov D.N., Mazur A.S. Influence of the Parameters of Polyvinyl Acetate-Based Composite Materials on Their Dissipative Properties. Zhurnal prikladnoy khimii, 2020, vol. 93, is. 4, pp. 575-580. DOI: 10.31857/S004446182004012X.
- Syatkovsky A.I. Thermoplastic film materials for damping engineering structures. Plasticheskie massy, 2023, no. 9-10, pp. 48-50. DOI: 10.35164/0554-2901-2023-9-10-48-52.
- Chakraborty B.C., Ratna D. Polymer for vibration damping applications. Elsevier, 2020, 348 p.
- Sagomonova V.A., Sytyi Yu.V., Kislyakova V.I., Dolgopolov S.S. Investigation of the damping properties of vibration-absorbing materials based on thermoplastic elastomers. Aviacionnye materialy i tehnologii, 2014, no. S3, pp. 5-10. DOI: 10.18577/2071-9140-2014-0-s3-5-10.
- Chen R., Luo H., Wang H., Zhou W. Topology optimization of partial constrained layer damping treatment on plate for maximizing modal loss factors. Composites and Advanced Materials, 2021, vol. 30, pp. 1-19.
- Samoryadov A.V., Kalugina E.V., Bitt V.V., Parshikov Yu.G., Ergashev A.T. Development and research of the properties of composite materials based on thermoplastic hybrid polymer matrix. Aviation materials and technologies, 2024, no. 3 (76), pp. 51-68. Available at: http://www.journal.viam.ru (accessed: January 28, 2026). DOI: 10.18577/2713-0193-2024-0-3-51-68.
- Sheyanov D.A. Methods for regulating vibration-absorbing properties of polymeric materials. Nauchnyy aspekt, 2024, vol. 43, no. 1, pp. 5615-5621.
- Sagomonova V.A., Tselikin V.V. Vibration damping material with perforated constraining layer. Aviation materials and technologies, 2023, no. 3 (72), pp. 125-133. Available at: http://www.journal.viam.ru (accessed: January 28, 2026). DOI: 10.18577/2713-0193-2023-0-3- 125-133.
- Manson J., Sperling L. Polymer Mixtures and Composites. Moscow: Khimiya, 1979, 440 p.
- Sagomonova V.A., Ivanov M.S., Platonov M.M. et al. Effect of Carbon Nanosized Fillers on the Mechanical Loss Coefficient of Thermoplastic Polyurethane Composites. Vse materialy. Entsiklopedicheskiy spravochnik, 2017, no. 1, pp. 9-14.
The article was submitted
2026-04-17
approved and accepted for publication after reviewing
2026-05-10