D. S. Gorlov, I. M. Ivanov, N. I. Artemenko Thermal spraying methods of metal-powder composites // Proceedings of VIAM. 2026. No. 9 (163). С. 149-161. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-149-161.
Thermal spraying methods of metal-powder composites
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
This paper provides an analysis of the main thermal spraying methods used to apply protective and hardening coatings based on metal powder composites. The advantages and disadvantages of various thermal spraying methods are discussed, as well as the key physical conditions and characteristics of the resulting coatings. It is shown that the most optimal thermal spraying method for applying the coating application must be selected based on a compromise between the required quality and process productivity.
Keywords
thermal spraying, protective and hardening coatings, metal powders, metal-powder composites, atmospheric plasma spraying, high velocity oxygen fuel spraying, cold spraying
Reference list
- Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Andronov A.A., Zolotukhin D.B., Salnikov S.A., Tyunkov A.V., Yushkov Yu.G. Prospects of using gadolinium zirconate as a ceramic layer of thermal protective coating (review). Aviation materials and technologies, 2026, no. 1 (82), pp. 232–254. Available at: http://www.journal.viam.ru (accessed: May 13, 2026). DOI: 10.18577/2713-0193-2026-0-1-232-254.
- Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 3 (68), pp. 108–119. Available at: http://www.journal.viam.ru (accessed: May 13, 2026). DOI: 10.18577/2713-0193-2022-0-3-108-119.
- Siegmann S., Abert C. 100 years of thermal spray: About the inventor Max Ulrich Schoop. Surface and Coatings Technology, 2013, vol. 220, pp. 3–13. DOI: 10.1016/j.surfcoat.2012.10.0134.
- Tejero-Martin D., Rezvani Rad M., McDonald A., Hussain T. Beyond Traditional Coatings: A Review on Thermal-Sprayed Functional and Smart Coatings. Journal of Thermal Spray Technology, 2019, vol. 28, no. 10, pp. 598–644. DOI: 10.1007/s11666-019-00857-1.
- Butkevich M.N., Puzyrakov A.F., Belokurov V.N. Gas-thermal spraying methods for equipment of consumer service enterprises. Servis v Rossii i za rubezhom, 2014, no. 4 (51), pp. 32–48. DOI: 10.12737/4850.
- Baldaev L.H., Sazonov E.G., Girfanova A.G., Fedorova M.O. Modification of heat-protective coatings based on stabilized ZrO2 by applying cold ceramic compositions. Aviation materials and technologies, 2025, no. 4 (81), pp. 136–142. Available at: http://www.journal.viam.ru (accessed: May 13, 2026). DOI: 10.18577/2713-0193-2025-0-4-136-142.
- Artemenko N.I. Research of the operation modes of the Metco F4 serial plasma-gun using plasma-forming gases argon and nitrogen. Trudy VIAM, 2018, no. 5 (65), pp. 76–89. Available at: http://www.viam-works.ru (accessed: March 20, 2026). DOI: 10.18577/2307-6046-2018-0-5-76-89.
- Crawmer D.E. Thermal Spray Processes. Handbook of Thermal Spray Technology. ASM International, 2013, pp. 54–76.
- Fauchais P., Vardelle M., Vardelle A., Goutier S. What do we know, what are the current limitations of suspension plasma spraying? Journal of Thermal Spray Technology, 2015, vol. 24 (7), pp. 1120–1129. DOI: 10.1007/s11666-015-0286-3.
- Young E.J., Mateeva E., Moore J.J. et al. Low Pressure Plasma Spray Coatings. International Conference on Metallurgical Coatings Thin Films, 2000, vol. 377–378, pp. 788–792. DOI: 10.1016/S0040-6090(00)01452-8.
- Trapeznikov A.V., Leonov A.A., Vlasova K.A., Chumakova E.S. Influence of coatings on the corrosion properties of AK7ch and VAL10 aluminum alloys on specimens with defects eliminated by cold spraying. Aviation materials and technologies, 2023, no. 4 (73), pp. 55–65. Available at: http://www.journal.viam.ru (accessed: May 13, 2026). DOI: 10.18577/2713-0193-2023-0-4-55-65.
- Duyunova V.A., Leonov A.A., Trofimov N.V., Mukhina I.Yu., Uridia Z.P., Tokarev M.S. Effect of gas-dynamic spraying of powder materials on the adhesion of paint coatings, corrosion, and mechanical properties of magnesium alloys. Trudy VIAM, 2026, no. 3 (157), pp. 54–65. Available at: http://www.viam-works.ru (accessed: May 13, 2026). DOI: 10.18577/2307-6046-2026-0-3-54-65.
- Bagade V.U., Duraiselvam M., Sarangi N., Parthiban K. Laser Surface Texturing to Enhance CuNiIn Anti-Fretting Coating Adhesion on Ti6Al4V Alloy for Aerospace Application. Lasers in Manufacturing and Materials Processing, 2020, vol. 7, art. 2. DOI: 10.1007/s40516-020-00114-2.
- Niu Z., Zhou W.-L., Wang C. et al. Fretting wear mechanism of plasma-sprayed CuNiIn coating on Ti–6Al–4V substrate under plane/plane contact. Surface and Coatings Technology, 2021, vol. 408, art. 126794. DOI: 10.1016/j.surfcoat.2020.126794.
The article was submitted
2026-06-18
approved and accepted for publication after reviewing
2026-06-23