V. G. Prokopenkov, A. G. Zagora, A. L. Shosheva, E. V. Dolgova, A. O. Kurnosov Influence of post-curing on properties of glass-reinforced plastics based on bismaleimide binder // Proceedings of VIAM. 2026. No. 10 (164). С. 118-132. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-118-132.

Influence of post-curing on properties of glass-reinforced plastics based on bismaleimide binder

V. G. Prokopenkov1, A. G. Zagora1, A. L. Shosheva1, E. V. Dolgova1, A. O. Kurnosov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

Post-curing of GFRP based on a bismaleimide binder was carried out by varying the post-curing temperature and time. The thermophysical properties of the material were determined by DSC and DMA methods. The mechanical properties of the material were determined by flexural and interlaminar shear strength (ILSS) tests. The shift of curing reaction peak, visual changes in the material, and changes in its mechanical properties with the increase of the curing temperature and time were studied. Recommendations for selecting the operating temperature of the material and proposals for further research are provided.

Keywords
polymer composite, glass fiber reinforced plastic (GFRP), thermal treatment, ene reaction, Diels–Alder reaction, polymer three-dimensional cross-linking, DSC, DMA, flexure, interlaminar shear strength (ILSS)


Reference list
  1. Kablov E.N. Materials: The Foundation of Any Endeavor. Delovaya Slava Rossii, 2013, no. 2, pp. 4-9.
  2. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122-144. Available at: http://www.journal.viam.ru (accessed: August 03, 2026). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  3. Malaya E.V., Savvin A.I. Composite Materials in Modern Aviation. Aktualnye issledovaniya, 2022, no. 49 (128), part I, pp. 6-9. Available at: https://apni.ru (accessed: August 03, 2026).
  4. Gulyaev I.N., Klimenko O.N., Lonskii S.L., Slavin A.V., Cherfas L.V. Determination of the composition and structure of polymer composite materials. Aviation materials and technologies, 2025, no. 4 (81), pp. 32-47. Available at: http://www.journal.viam.ru (accessed: August 03, 2026). DOI: 10.18577/2713-0193-2025-0-4-32-47.
  5. Gusev Yu.A., Usacheva M.N., Parakhin I.V., Kovalenko A.V., Vasyukov A.N. Application of composite materials and polymer filler in a helicopter blade design. Trudy VIAM, 2025, no. 9 (151), pp. 50-62. Available at: http://www.viam-works.ru (accessed: August 03, 2026). DOI: 10.18577/2307-6046-2025-0-9-50-62.
  6. Kablov E.N. What Is the Future Made Of? Next-Generation Materials and Technologies for Their Production and Processing as the Foundation for Innovation. Krylya Rodiny, 2016, no. 5, p. 8-18.
  7. Shosheva A.L. Bismaleimide resins (review). Part 1. Trudy VIAM, 2022, no. 10 (116), pp. 23-41. Available at: http://www.viam-works.ru (accessed: August 03, 2026). DOI: 10.18577/2307-6046-2022-0-10-23-41.
  8. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Kudryavtseva A.N. Application of bismaleimide VST-57 binder for obtaining heat-resistant dimensionally stable molds from polymer composite materials. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 32-40. DOI: 10.18577/2071-9140-2020-0-2-32-40.
  9. Prokopenkov V.G., Kolpachkov E.D., Shosheva A.L. Influence of glass fiber-reinforced bismaleimide composition on the level of its properties. Trudy VIAM, 2023, no. 4 (122), pp. 49-59. Available at: http://www.viam-works.ru (accessed: August 03, 2026). DOI: 10.18577/2307-6046-2023-0-4-49-59.
  10. Nacharkina A.V., Valueva M.I., Zelenina I.V., Shosheva A.L. High-temperature carbon fiber reinforced plastics based on bismaleinimide binders. Aviation materials and technologies, 2024, no. 4 (77), pp. 43–61. Available at: http://www.journal.viam.ru (accessed: August 03, 2026). DOI: 10.18577/2713-0193-2024-0-4-43-61.
  11. Evsyukov S., Pohlmann T., Wiel M. Modern approaches to the processing of bismaleimide resins. Current Trends in Polymer Science, 2020, no. 20, pp. 1–28.
  12. Fink J.K. Reactive Polymers: Fundamentals and Applications. Third Ed. Elsevier, 2018, pp. 367–402. DOI: 10.1016/B978-0-12-814509-8.00011-7.
  13. Prasanaa Iyer N., Arunkumar N. Review on Fiber reinforced/modified Bismaleimide resin composites for Aircraft Structure Application. IOP Conference Series: Materials Science and Engineering, 2020, vol. 923, p. 12051. DOI: 10.1088/1757-899X/923/1/012051.
  14. Anandan S., Dhaliwal G., Samaranayake V. et al. Influence of cure conditions on out-of-autoclave bismaleimide composite laminates. Journal of Applied Polymer Science, 2016, no. 133 (38). DOI: 10.1002/app.43984.
  15. Stelter C., Park C., Chu S.-H., Hudson T. Dynamic Mechanical Analysis of Post-Cured Bismaleimide Resins for Composite-Overwrapped Combustion Chambers Cycled From Cryogenic to High Temperatures: Technical Memorandum: NASA/TM-20240012459. URL: https://ntrs.nasa.gov (accessed: August 03, 2026).
  16. Seris A., Feve M., Méchin F., Pascault J. Thermally and anionically initiated cure of bismaleimide monomers. Journal of Applied Polymer Science, 1993, no. 48 (2), pp. 257–269.
  17. Shin E., Morgan R., Zhou J., Lincoln J. Hygrothermal Durability and Thermal Aging Behavior Prediction of High-Temperature Polymer-Matrix Composites and Their Resins. Journal of Thermoplastic Composite Materials, 2000, no. 13 (1), pp. 40–57. DOI: 10.1177/089270570001300104.
  18. Shibulal G., Adityan S., Mohit P., Akheela N., Kasilingam R. Processing, Curing and After-Cure Dynamic Properties of a Thermally Polymerizable Bismaleimide-Filled Natural Rubber Formulation. Journal of Applied Polymer Science, 2025, no. 143. DOI: 10.1002/app.57995.
  19. Yu S., Feng Y., Wang W. et al. Curing Kinetics of Bismaleimide Resin and High-Temperature Tribological Properties of Fabric-Reinforced Composites. ACS Applied Polymer Materials, 2026, no. 8 (12), pp. 9662–9672. DOI: 10.1021/acsapm.6c01293.
  20. Eliseyeva I.I., Yuzbashev M.M. General Theory of Statistics: Textbook. 5th ed. Moscow: Finansy i Statistika, 2004, 656 p.