A. G. Gunyaeva, O. N. Klimenko, S. I. Mishkin, A. I. Tkachuk, G. A. Akomelkov Polymer film coating with an integrated metal layer for protection against lightning discharges of helicopter equipment elements made of polymer composite material (PCM) // Proceedings of VIAM. 2026. No. 10 (164). С. 185-196. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-185-196.

Polymer film coating with an integrated metal layer for protection against lightning discharges of helicopter equipment elements made of polymer composite material (PCM)

A. G. Gunyaeva1, O. N. Klimenko1, S. I. Mishkin1, A. I. Tkachuk1, G. A. Akomelkov2

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
2Separate Division of a Joint-Stock Company «31 State Design Institute for Special Construction» «Research Center 26 Central Research Institute», Saint Petersburg, Russia; op26cnii@gmpi.spb.ru

Abstract

The article considers various approaches to lightning protection of helicopters structures made of PCM. A new development of the Kurchatov Institute – VIAM is presented: a lightning-protection coating of VMZP-3 grade, which is a leveling composite film with an integrated metal layer. It can be used with perforated foils or knitted wire sieves of various surface densities, including those with a glass fabric substrate. The main properties of the developed VMZP-3 lightning-protection coating and the results of tests of elementary samples for lightning resistance are given.

Keywords
lightning protection, polymer composite materials, carbon fiber reinforced plastic (CFRP), carbon filler, perforated metal foils, knitted metal wire sieve, composite leveling films, helicopter



Reference list
  1. Kablov E.N. Marketing in Materials Science, Aircraft Manufacturing, and Industry: Present and Future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. The Role of State Scientific Centers of the Russian Federation in Ensuring National Security. Perspektivnyye tekhnologii dlya sistem bezopasnosti, 2023, no. 1, pp. 4–9.
  4. Kablov E.N., Antipov V.V. The Role of New-Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  5. Kablov E.N. New-Generation Materials and Digital Technologies for Their Processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  6. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  7. Sazhenkov N.A., Sazhenkov A.N. Lightning protection coatings for engine nacelles made of polymer composite materials. Part 1. Analysis of existing types of lightning protection. Vestnik PNIPU. Aerokosmicheskaya tekhnika, 2021, no. 67, pp. 43–55.
  8. Chursova L.V., Panina N.N., Grebeneva T.A., Vishnyakov L.R. Materials for lightning protection systems for polymer composite materials. Manufacturing specifics (review, Part I). Vse materialy. Entsiklopedicheskiy spravochnik, 2023, no. 9, pp. 25–33.
  9. Mishkin S.I., Klimenko O.N., Gunyaeva A.G. Materials for the lightnings protection of aviation engineering. Trudy VIAM, 2023, no. 7 (125), pp. 84–92. Available at: http://www.viam-works.ru (accessed: September 09, 2026). DOI: 10.18577/2307-6046-2023-0-7-84-92.
  10. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  11. Kablov E.N., Gunyaev G.M., Krivonos V.V. et al. Increasing the transverse conductivity of structural carbon-fiber-reinforced plastics modified with fulleroid nanoparticles. Nanocomposites: Research, Production, Application. Moscow: TorusPress, 2004, pp. 20–23.
  12. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: September 01, 2026). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  13. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), pp. 82–92. Available at: http://www.journal.viam.ru (accessed: July 04, 2026). DOI: 10.18577/2713-0193-2023-0-1-82-92.
  14. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: July 04, 2026). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  15. Gulyaev I.N., Klimenko O.N., Lonskii S.L., Slavin A.V., Cherfas L.V. Determination of the composition and structure of polymer composite materials. Aviation materials and technologies, 2025, no. 4 (81), pp. 32–47. Available at: http://www.journal.viam.ru (accessed: August 01, 2026). DOI: 10.18577/2713-0193-2025-0-4-32-47.
  16. Veshkin E.A., Slavin A.V., Postnova M.V., Apalkova A.V. The role of temperature-time curing conditions in the formation of unidirectional and equally strong carbon fiber plastics properties. Aviation materials and technologies, 2025, no. 2 (79), pp. 59–71. Available at: http://www.journal.viam.ru (accessed: September 01, 2026). DOI: 10.18577/2713-0193-2025-0-2-59-71.
  17. Gunyaeva A.G., Kurnosov A.O., Slavin A.V. Experience in the use of polymer composite materials developed by NRC «Kurchatov Institute» – VIAM in engines for civil aircraft. Aviation materials and technologies, 2024, no. 4 (77), pp. 82–94. Available at: http://www.journal.viam.ru (accessed: September 01, 2026). DOI: 10.18577/2713-0193-2024-0-4-82-94.
  18. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.