Butuzov A.V. Preceramic polymers for the production of ceramic products by vat photopolymerization. Part 2. Composition and methods of obtaining photo-curable polymer preceramic compounds // Proceedings of VIAM. 2026. No. 1 (155). С. 102–123. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-1-102-123.

Preceramic polymers for the production of ceramic products by vat photopolymerization

Part 2. Composition and methods of obtaining photo-curable polymer preceramic compounds
Butuzov A.V.
Abstract

The second part of the review examines the compositions and methods for obtaining photocurable polymer pre-ceramic compositions for the manufacture of ceramics using vat photopolymerization. The main types of photocurable organosilicon polymers, active diluents, photoinitiators, and special additives are considered. The mechanisms of radical and cationic photopolymerization of photocurable polymer pre-ceramic compositions are presented. The effect of filler addition into the composition on the properties of ceramics is indicated.

Keywords
preceramic polymers, vat photopolymerization, polyorganosiloxanes, polyorganocarbosilanes, polyorganosilazanes, photo-curable polymer preceramic compounds, polymer derived ceramics
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Rosso M. Ceramic and metal matrix composites: Кoutes and properties. Journal of Materials Processing Technology, 2006, vol. 175, pp. 364–375. DOI: 10.1016/j.jmatprotec.2005.04.038.
  3. Bill J., Wakai F., Aldinger F. Precursor-derived ceramics: Synthesis, Structure and High-Temperature Mechanical Properties. Weinheim: Wiley-VCH, 2008, 313 p.
  4. Kablov E.N. The Present and Future of Additive Technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  5. Kablov E.N. Additive Technologies – the Dominant Focus of the National Technological Initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  6. Turchenko M.V., Lebedeva Yu.E., Belyachenkov I.O., Prokofiev V.A. Obtaining of ceramic materials by stereolithography method. Trudy VIAM, 2023, no. 9 (127), pp. 79–89. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2023-0-9-79-89.
  7. Lacelle T., Sampson K.L., Sarvestani H.Y. et al. Additive manufacturing of polymer derived ceramics: Materials, methods, and applications. APL Materials, 2023, vol. 11, pp. 1–29. DOI: 10.1063/5.0151661.
  8. Camargo I.L., Morais M.M., Fortulan C.A., Branciforti M.C. A review on the rheological behavior and formulations of ceramic suspensions for vat photopolymerization. Ceramics International, 2021, vol. 47, pp. 11906–11921. DOI: 10.1016/j.ceramint.2021.01.031.
  9. Bae C.J., Ramachandran A., Chung K., Park S. Ceramic stereolithography: Additive manufacturing for 3D complex ceramic structures. Journal of the Korean Ceramic Society, 2017, vol. 54, pp. 470–477. DOI: 10.4191/kcers.2017.54.6.12.
  10. Rasaki S.A., Xiong D., Xiong S. et al. Photopolymerization-based additive manufacturing of ceramics: A systematic review. Journal of advanced ceramics, 2021, vol. 10, no. 3, pp. 442–471. DOI: 10.1007/s40145-021-0468-z.
  11. Nowak D., Ortyl J., Kamińska-Borek I. et al. Photopolymerization of hybrid monomers: Part I: Comparison of the performance of selected photoinitiators in cationic and free-radical polymerization of hybrid monomers. Polymer Testing, 2017, vol. 64, pp. 313–320. DOI: 10.1016/j.polymertesting.2017.10.020.
  12. Mucci V., Vallo C. Efficiency of 2,2-dimethoxy-2-phenylacetophenone for the photopolymerization of methacrylate monomers in thick sections. Journal Applied Polymer Science, 2012, vol. 123, pp. 418–425. DOI: 10.1002/app.34473.
  13. Babkin O.E. 3D modeling: technologies, equipment, materials. St. Petersburg: Publ. House of St. Petersburg State Univ. of Cinematography and Television, 2013, 97 p.
  14. Sarychev I.A., Butuzov A.V., Serkova E.A., Dolgova E.V. Photocurable acrylate compositions (review). Trudy VIAM, 2022, no. 9 (115), pp. 68–82. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2022-0-9-68-82.
  15. Green W.A. Industrial Photoinitiators: A Technical Guide. Boca Raton: CRC Press, 2010, 302 p.
  16. Rapid Prototyping Resin Compositions: pat. 8293810 US; appl. 29.08.05; publ. 23.10.12.
  17. Photopolymerizable Compositions Containing an Alkylbisacylphosphine Oxide: pat. 5472992 US; appl. 28.04.94; publ. 05.12.95.
  18. Wloka T., Gottschaldt M., Schubert U.S. From light to structure: Photo initiators for radical two-photon polymerization. Chemistry – A European Journal, 2022, no. 28, pp. 1–54. DOI: 10.1002/chem.202104191.
  19. Boddapati A., Rahane S.B., Slopek R.P. et al. Gel Time Prediction of Multifunctional Acrylates Using a Kinetics Model. Polymer, 2011, no. 52, pp. 866–873. DOI: 10.1016/j.polymer.2010.12.024.
  20. Wayner D.D.M., Clark K.B., Rauk A. et al. C-H Bond Dissociation Energies of Alkyl Amines: Radical Structures and Stabilization Energies. Journal of the American Chemical Society, 1997, no. 119, pp. 8925−8932. DOI: 10.1021/ja971365v.
  21. Crivello J.V. The Discovery and Development of Onium Salt Cationic Photoinitiators. Journal of Polymer Science. Part A: Polymer Chemistry, 1999, no. 37, pp. 4241−4254. DOI: 10.1002/(sici)1099-0518(19991201)37:233.0.co;2-r.
  22. Fouassier J.-P., Lalevee J. Photoinitiators for Polymer Synthesis: Scope, Reactivity, and Efficiency. Weinheim: Wiley-VCH Verlag and Co. KGaA, 2012, 490 p.
  23. Lenshina N.A., Shurygina M.P., Chesnokov S.A. Photoreduction reaction of carbonyl-containing compounds in the synthesis and modification of polymers. Vysokomolekulyarnye soedineniya. Ser.: B, 2021, vol. 63, no. 6, pp. 383–418. DOI: 10.31857/S2308113921060139.
  24. Yagci Y. Wavelength flexibility in photoinitiated cationic polymerization. Macromolecular Symposia, 2004, vol. 215, no. 1, pp. 267–280. DOI: 10.1002/masy.200451121.
  25. Ligon S.C., Liska R., Stampfl J. et al. Polymers for 3D printing and customized additive manufacturing. Chemical Reviews, 2017, vol. 117, pp. 10212–10290. DOI: 10.1021/acs.chemrev.7b00074.
  26. Bagheri A., Jin J. Photopolymerization in 3D Printing. ACS Applied Polymer Materials, 2019, vol. 1, pp. 593–611. DOI: 10.1021/acsapm.8b00165.
  27. Zhiganshina E.R., Arsenyev M.V., Chesnokov S.A. Two-photon stereolithography – optical nanolithography. Vysokomolekulyarne soedineniya. Ser.: B, 2023, vol. 65, no. 3, pp. 163–188. DOI: 10.31857/S2308113923700468.
  28. Brigo L.L., Schmidt J.E.M., Gandin A. et al. 3D Nanofabrication of SiOC Ceramic Structures. Advanced Science, 2018, no. 5, pp. 1–8. DOI: 10.1002/advs.201800937.
  29. Bauer J., Crook C., Izard A.G. et al. Additive manufacturing of ductile, ultrastrong polymer-derived nanoceramics. Matter, 2019, vol. 1 (6), pp. 1547–1556. DOI: 10.1016/j.matt.2019.09.009.
  30. Barroso G., Li Q., Bordia R.K., Motz G. Polymeric and ceramic silicon-based coatings – A review. Journal of Materials Chemistry, 2019, vol. 7 (5), pp. 1936–1963. DOI: 10.1039/C8TA09054H.
  31. Al-Ajrash S.M.N., Browning C., Eckerle R., Cao L. Initial development of preceramic polymer formulations for additive manufacturing. Materials Advances, 2021, no. 2, pp. 1083–1089. DOI: 10.1039/d0ma00742k.
  32. Dory H., Miele P., Salameh C. UV-curable inorganic precursorsenable direct 3D printing of SiOC ceramics. International Journal of Applied Ceramic Technology, 2023, no. 20, pp. 141–152. DOI: 10.1111/ijac.14173.
  33. Ligon-Auer S.C., Schwentenwein M., Gorsche C. et al. Toughening of Photo-Curable Polymer Networks: A Review. Polymer Chemistry, 2016, no. 7, pp. 257–286. DOI: 10.1039/C5PY01631B.
  34. Husar B., Ligon S.C., Wutzel H. et al. The Formulator’s Guide to Anti-Oxygen Inhibition Additives. Progress Organic Coatings, 2014, no. 77, pp. 1789−1798. DOI: 10.1016/j.porgcoat.2014.06.005.
  35. Wang X., Schmidt F., Hanaor D. et al. Additive manufacturing of ceramics from preceramic polymers: A versatile stereolithographic approach assisted by thiol-ene click chemistry. Additive Manufacturing, 2019, vol. 27, pp. 80–90. DOI: 10.1016/j.addma.2019.02.012.
  36. Dufaud O., Marchal P., Corbel S. Rheological properties of PZT suspensions for stereolithography. Journal of the European Ceramic Society, 2002, vol. 22, pp. 2081–2092. DOI: 10.1016/S0955-2219(02)00036-5.
  37. Zhang J., Wei L., Meng X. et al. Digital light processing stereolithography three-dimensional printing of yttria-stabilized zirconia. Ceramics International, 2020, vol. 46, pp. 8745–8753. DOI: 10.1016/j.ceramint.2019.12.113.
  38. Shestakov A.M. Ceramics based on organosilicon polymers-precursors: methods of preparation and properties (review). Trudy VIAM, 2020, no. 11 (93), pp. 76–92. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2020-0-11-76-92.
  39. Wang D., Klein J., Mejia E. Catalytic systems for the cross-linking of organosilicon polymers. Chemistry – An Asian Journal, 2017, vol. 12 (11), pp. 1180–1197. DOI: 10.1002/asia.201700304.
  40. Butuzov A.V., Semina A.V. Preceramic polymers for the production of ceramic products by vat photopolymerization. Part 1. Methods of production and properties. Trudy VIAM, 2025, no. 3 (145), pp. 70–88. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2025-0-3-70-88.
  41. Schmidt J., Colombo P. Digital light processing of ceramic components from polysiloxanes. Journal of the European Ceramic Society, 2018, vol. 38, pp. 57–66. DOI: 10.1016/j.jeurceramsoc.2017.07.033.
  42. Brigo L.L., Schmidt J.E.M., Gandin A. et al. 3D Nanofabrication of SiOC Ceramic Structures. Advanced Science, 2018, no. 5, pp. 1–8. DOI: 10.1002/advs.201800937.
  43. Zanchetta E., Cattaldo M., Franchin G. et al. Stereolithography of SiOC ceramic microcomponents. Advanced Materials, 2016, vol. 28, pp. 370–376. DOI: 10.1002/adma.201503470.
  44. He C., Ma C., Li X. et al. Polymer-derived SiOC ceramic lattice with thick struts prepared by digital light processing. Additive Manufacturing, 2020, vol. 35, pp. 1–8. DOI: 10.1016/j.addma.2020.101366.
  45. Yang J., Yu R., Li X. et al. Silicon carbide whiskers reinforced SiOC ceramics through digital light processing 3D printing technology. Ceramics International, 2021, vol. 47, pp. 18314–18322. DOI: 10.1016/j.ceramint.2021.03.152.
  46. Tarasova E.M., Butuzov А.V., Cherkasova A.A., Ivanov P.V. Study of chemical assembly of macromolecules in polycondensation of difunctional dimethylsilanes. Tonkie khimicheskie tekhnologii, 2016, vol. 11, no. 1, pp. 59–66. DOI: 10.32362/2410-6593-2016-11-1-59-66.
  47. Shitov R.О., Butuzov А.V. Commercial silicone resin (review). Part 1. Trudy VIAM, 2023, no. 2 (120), pp. 3–19. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2023-0-2-3-19.
  48. Hazan Y., Penner D. SiC and SiOC ceramic articles produced by stereolithography of acrylate modified polycarbosilane systems. Journal of the European Ceramic Society, 2017, vol. 37, pp. 5205–5212. DOI: 10.1016/j.jeurceramsoc.2017.03.021.
  49. Wang X., Schmidt F., Hanaor D. et al. Additive manufacturing of ceramics from preceramic polymers: A versatile stereolithographic approach assisted by thiol-ene click chemistry. Additive Manufacturing, 2019, vol. 27, pp. 80–90. DOI: 10.1016/j.addma.2019.02.012.
  50. Li Z., Chen Z., Liu J. et al. Additive manufacturing of lightweight and high-strenght polymer-derived SiOC ceramics. Virtual and Physical Protyping, 2020, vol. 15, no. 2, pp. 1–15. DOI: 10.1080/17452759.2019.1710919.