UDC
669.15:621.787
DOI
10.18577/2307-6046-2026-0-1-19-29
Article PDF (Russian)
(911.08 KB)
How to cite
Laptev A.B., Zagorskikh O.A., Fedorov A.S., Golubev I.A. Optimization of the surface hardening parameters for 12X18H10T steel pipes using a regression model // Proceedings of VIAM. 2026. No. 1 (155). С. 19–29. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-1-19-29.
Optimization of the surface hardening parameters for 12X18H10T steel pipes using a regression model
Abstract
During the operation of turbojet engines, the pipelines of the external systems are subject to fatigue failure caused by fretting corrosion. The article presents the results of developing a model describing the change in the resistance of 8×1 mm pipes made of 12X18H10T steel to fretting corrosion after various types of processing. It is shown that maximum resistance to fretting corrosion is achieved at: microhardness HV0,025 = 2510 МPа, modified layer depth greater than 44 microns, average compressive residual stresses greater than 208,5 MPa and roughness, Ra less than 1,18 microns.
Keywords
fretting corrosion, fretting fatigue, stainless steel, surface hardening, optimization, regression model
Reference list
- Mystkowska J., Lysik D., Klekotka M. Effect off Saliva and Mucin-Based Saliva Substitutes on Fretting Processes of 316 Austenitic Stainless Steel. Metals, 2019, vol. 9, p. 178.
- Petukhov A.N. Fretting corrosion and fretting fatigue in low-mobility joints. Vestnik SGAU im. akademika S.P. Koroleva, 2006, no. 2-1 (10), pp. 115–120.
- Muboyadzhyan S.A., Konnova V.I., Gorlov D.S., Alexandrov D.A. The study of steel EP866Sh fretting resistance. Trudy VIAM, 2015, no. 7, pp. 3–7. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2015-0-7-1-1.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik RAN, 2020, vol. 90, no. 4, pp. 331–334.
- Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
- Kablov E.N. Trends and Guidelines for Innovative Development of Russia: Collection of Scientific and Information Materials; 3rd ed., rev. and enl. Moscow: VIAM, 2015, 720 p.
- Maksarov V.V., Krasnyy V.A. Friction Mechanisms of Thin-Film Coatings under Fretting Corrosion Conditions. Nauchno-tekhnicheskiye vedomosti SpbGPU, 2015, no. 3 (226). pp. 111–120.
- Lyubimov R.V. Forecasting and Technological Support of Performance Properties of GTE Parts Operating under Fretting Corrosion Conditions: thesis, Cand. Sc. (Tech.). Rybinsk, 2000, 202 p.
- Terentyev V.F., Korableva S.A. Metal Fatigue. Moscow: Nauka, 2015, 484 p.
- Ostrovsky M.S. Fretting as a Cause of Reduced Reliability of Mining Machines. Gornyy informatsionno-analiticheskiy byulleten, 2011, no. S3, pp. 315–331.
- Khaing Min, Petukhov A.N., Pavlov Yu.I. Ensuring the Load-Bearing Capacity of Lock Joints of Aircraft Engine Compressor Blades under the Effect of Fretting Corrosion. Aviatsionnaya promyshlennost, 2012, no. 1, p. 12.
- Ivanova V.S., Gurevich S.E., Kopyev I.M. et al. Fatigue and Brittleness of Metallic Materials. Moscow: Nauka, 1968, 219 p.
- Aslanyan I.R., Semenov V.I., Shuster L.Sh. Determination of factors significantly influencing fretting wear of electrolytic NiP coatings. Vestnik UGATU, 2012, vol. 16, no. 1 (46), pp. 57–61.
- Aslanyan I.R., Selis Zh.P., Shuster L.Sh. Effect of silicon carbide SiC additives on wear of electrolytic NiP coatings. Trenie i iznos, 2010, vol. 31, no. 5, pp. 353–361.
- Zagorskikh O.A., Laptev A.B. Features of fretting corrosion of stainless austenitic steels (review). Actual problems of corrosion protection of oil and gas equipment and pipelines (CORROSION–2023): collection of materials of the I Int. scientific and technical conf. Ufa, 2023, pp. 40–42.
- Aslanian I.R., Schuster L.Sh. Wear of electrolytic NiP coatings at fretting. Aviacionnye materialy i tehnologii, 2015, no. 3 (36), pp. 38–43. DOI: 10.18577/2071-9140-2015-0-3-38-43.
- Aslanyan I.R. Improving the efficiency of wear-resistant electrolytic coatings: thesis abstract, Dr. Sc. (Tech.). Ufa, 2014, 39 p.
- Aslanyan I.R., Krioni N.K., Shuster L.Sh. Tribological characteristics of electrolytic coatings under various friction conditions. Vestnik UGATU, 2013, vol. 17, no. 8 (61), pp. 24–28.
- Dokshanin S.G. Influence of lubricating compositions with ultradispersed additives on fretting fatigue processes. Vestnik SIBGAU, 2014, no. 3 (55), pp. 198–201.
- Shevelya V.V., Oleksandrenko V.P. Rheological aspects of the influence of fretting on stress-corrosion cracking of steel. Vestnik dvigatelestroyeniya, 2006, no. 1, pp. 95–100.
- Zabirov F.Sh., Mansurov R.R. On the Negative Impact of Fretting Corrosion in a Rubber-Metal Bearing of a Turbodrill Spindle. Alleya nauki, 2017, vol. 2, no. 9, pp. 412–414.
- Petukhov A.N. Fretting and Fretting Fatigue of Structural Materials and Components. Aviatsionnaya promyshlennost, 2014, no. 4, pp. 5–50.
- Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: April 07, 2024). DOI: 10.18577/2713-0193-2023-0-1-30-50.
- Pogonyshev V.A., Tishchenko S.V. Method for Increasing Fretting Resistance of Machine Parts by Improving Their Damping Properties. Current Trends in Science, Technology, and Education: Coll. of Scientific Papers Based on the Proceedings of the III Int. Res. and Pract. Conf.: in 2 Parts (March 31, 2018, Smolensk). Smolensk: NOVALENSO, 2018, part 2, pp. 77–80.
- Smyslov A.M., Selivanov K.S. Development and Research of Technological Methods for Improving Fretting Resistance of Titanium Alloy Working Blades. Vestnik UGATU, 2007, vol. 9, no. 1 (19), pp. 77–83.
- Fridman Z.G., Veitsman M.G. The influence of mechanical and thermal treatment on the cyclic strength of sheets of 1X18N9 steel. Fatigue of metals and alloys: coll. of materials of the 5th Conference on metal fatigue. Moscow: Nauka, 1971, p. 123.
- Fouvry S., Kapsa P., Vincent L. Quantification of fretting damage. Wear, 1996, vol. 200, pp. 186–205. DOI: 10.1016/j.wear.2009.09.012.
- Loto R.T. Assessment of pitting corrosion of austenitic stainless steel type 304 in an acid-chloride environment. Journal of Materials and Environmental Sciences, 2013, vol. 4 (4), pp. 448–459.
- Dabrowski J.R., Klekotka M., Sidun J. Fretting and fretting corrosion of 316L implantation steel in the oral cavity environment. Eksploatacja i Niezawodnosc – Maintenance and Reliability, 2014, vol. 16, pp. 441–446. DOI: 10.3390/ma13071561.
- Laptev A.B., Zakirova L.I., Zagorskikh O.A., Pavlov M.R. Methods of investigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review). Part 1. Investigation of corrosion-mechanical destruction of steels. Trudy VIAM, 2022, no. 4 (110), pp. 118–130. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2022-0-4-118-130.
- Laptev A.B., Zakirova L.I., Zagorskikh O.A., Pavlov M.R., Gorbovets M.A. Methods of in-vestigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review). Part 2. Formation of passive films and hydrogen sulfide cracking of steels. Trudy VIAM, 2022, no. 5 (111), pp. 138–146. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2022-0-5-138-146.
- Zagorskikh O.A., Laptev A.B. Prevention of fretting corrosion of austenitic alloy steel by forming a hardened layer on the surface. Bulletin PNIPU. Ser.: Mechanical Engineering, Materials Science, 2024, vol. 26, no. 4, pp. 5–18. DOI: 10.15593/2224-9877/2024.4.01.