Petrushin N.V., Svetlov I.L., Epishin A.I., Elyutin E.S. Development of directional solidification method to solve the problems of physical metallurgy of nickel- and cobalt-based superalloys. Part 1 // Proceedings of VIAM. 2025. No. 5 (147). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-5-3-24.

Development of directional solidification method to solve the problems of physical metallurgy of nickel- and cobalt-based superalloys

Part 1
Petrushin N.V., Svetlov I.L., Epishin A.I., Elyutin E.S.
Abstract

The review considers behavior of components during segregation along the casting height when directional solidification is performed with a flat front and shows practical application of this technique to solve problems of physical metallurgy of nickel-based alloys. Such problems include precise determination of temperature and composition of peritectic and eutectic reactions in nickel-based alloys of the binary system Ni–Al; determination of the solubility of W and Re in the γʹ- and β-phases of nickel-based alloys of the ternary systems Ni–Al–W and Ni–Al–Re; the solubility of Re and Ru in the γʹ- and β-phases in the quaternary system Ni–Al–Re–Ru, determination of the lattice spacing and interdiffusion coefficients in the γ-solid solution of nickel in the binary system Ni–Re.

Keywords
directional solidification, flat growth front, macrosegregation of alloying elements, nickel-based alloys, wolfram, rhenium, ruthenium, solidus temperature and liquidus temperature, solubility of element
Reference list
  1. Cast blades of gas turbine engines. Alloys, technologies, coatings. Ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, 632 p.
  2. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: University Press, 2006, 372 p. DOI: 10.1017/CBO9780511541285.
  3. Shalin R.E., Svetlov I.L., Kachanov E.B. et al. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroenie, 1997, 336 p.
  4. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: 15.07.2024). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  5. Flemings M. Solidification processes. Trans. from Engl. Moscow: Mir, 1977, 423 p.
  6. Gigliotte M.F.X., Henry M.F. Segregation in a plane front solidified /ʹ-TaC alloy. Proceedings of Conference on in Situ Composites II. Lexington, 1976, pp. 253–265.
  7. Svetlov I.L., Petrushin N.V., Fedorov V.A., Abalakin N.P. Segregation of alloying elements in the process of directional solidification of eutectic alloys. Fizika metallov i metallovedenie, 1984, vol. 52, is. 2, pp. 342–348.
  8. Vigdorovich V.N., Volpyan A.E., Kurdyumov G.M. Directional crystallization and physicochemical analysis. Moscow: Khimiya, 1976, 200 p.
  9. Petrushin N.V., Monastyrskaya E.V. Application of directional solidification to solving problems of development and optimization of heat-resistant materials. Materialovedenie, 1998, no. 5, pp. 2–10.
  10. Somov A.I., Tikhonovsky M.A. Eutectic compositions. Moscow: Metallurgiya, 1975, 304 p.
  11. Bridgman P.W. Certain physical properties of single crystals of tungsten, antimony, bismuth, tellurium, cadmium, zinc, and tin. Proceedings of the American Academy of Arts and Sciences, 1925, vol. 60, pp. 305–383. DOI: 10.2307/25130058.
  12. Petrushin N.V., Elyutin E.S., Dzhioeva E.S., Nazarkin R.M. Structural and phase characteristics of heat-resistant eutectic composites γ/γʹ-NbC containing rhenium and ruthenium. Perspektivnye materialy, 2015, no. 03, pp. 22–33.
  13. Alexander W.O., Vaughan N.B. Investigation of phase equilibria in Al–Ni system. Journal Institute Metals, 1937, vol. 61, pp. 247–263.
  14. Hansen M., Anderko K. Structure of binary alloys: in 2 vols. Trans. from Engl. Moscow: Metallurgizdat, 1962, vol. 1, 608 p.
  15. Schramm J. Das binare Teilssystem Nickel–NiAl. Zeitschrift Metallkunde, 1941, b. 33, nu. 10, s. 347–355.
  16. Bremer F.J., Beyss M., Karthaus E. et al. Experimental analysis of the Ni−Al phase diagram. Journal Crystal Growth, 1988, vol. 87, no. 2−3, pp. 185–192. DOI: 10.1016/0022-0248(88)90163-7.
  17. Hilpert K., Kobertz D., Venugopal V. et al. Phase diagramm studies on the Al−Ni system. Zeitschrift Naturforschung, 1987, vol. 42a, pp. 1327−1332. DOI: 10.1515/zna-1987-1117.
  18. Verhoeven J.D., Lee J.H., Laabs F.C., Jones L.L. The phase equilibria of Ni3Al evaluated by directional solidification and diffusion couple experiment. Journal Phase Equilibria, 1991, vol. 12, no. 1, pp. 15–23. DOI: 10.1007/BF02663666.
  19. Udovsky A.L., Oldakovskii I.V., Moldavskii V.G. On the revision of the phase diagram of the nickel-aluminum system. Doklady AN SSSR, 1991, vol. 317, no. 1, pp. 161−165.
  20. Akshentsev Yu.N., Stepanova N.N., Sazonova V.A., Rodionov D.P. Growth structure of Ni3Al single crystals alloyed with a third element. Fizika metallov i metallovedenie, 1997, vol. 84, is. 3, pp. 130−137.
  21. Petrushin N.V., Bronfin M.B., Chabina E.B., Dyachkova L.A. Phase transformations and structure of directionally crystallized intermetallic alloys Ni−Al−Re. Metally, 1994, no. 3, pp. 85–93.
  22. Petrushin N.V., Elyutin E.S., Chabina E.B. Phase and structural transformations in directionally solidified with plant front intermetallic eutectic Ni-based alloys. Trudy VIAM, 2020, no. 3 (87), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2020-0-3-13-29.
  23. Webber J.G., Van Aken D.C. Studies of a quasi-binary β-NiAl and α-Re eutectic. Scripta Metallurgica, 1989, vol. 23, no. 2, pp. 193–196. DOI: 10.1016/0036-9748(89)90409-2.
  24. Elyutin Е.S., Petrushin N.V., Karachevtsev F.N., Chabina E.B. Solubility of rhenium and ruthenium in the γ′-phase and physicochemical properties of nickel alloys of the Ni–Al‒Re‒Ru system. Trudy VIAM, 2023, no. 6 (124), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2023-0-6-3-14.
  25. Petrushin N.V., Elyutin E.S., Visik E.M., Golynets S.A. Development of a single-crystal heat-resistant nickel alloy of the 5th generation. Metally, 2017, no. 6, pp. 38–51.
  26. Sluytman J.V., Fontaine A.L., Cairney J.M., Pollock T.M. Elemental portioning of platinum metal containing Ni-base superalloys using electron microprobe analysis and atom probe tomography. Acta Materialia, 2010, vol. 58, pp. 1952–1962. DOI: 10.1016/J.ACTAMAT.2009.11.038.
  27. Reed R.C., Yeh A.C., Tin S. et al. Identification of the partitioning characteristics of ruthenium in single crystal superalloys using atom probe tomography. Scripta Materialia, 2004, vol. 51, pp. 327‒333. DOI: 10.1016/j.scriptamat.2004.04.019.
  28. Miracle D.B., Lark K.A., Srinavasan V., Lipsitt H.A. Nickel-Aluminium-Molybdenum phase equilibria. Metallurgical Transactions A, 1984, vol. 15A, no. 3, pp. 481−486. DOI: 10.1007/BF02644971.
  29. Udovsky A.L., Oldakovskiy I.V., Moldavskiy V.G. Theoretical and experimental studies of phase equilibria of the Ni−NiAl−W system in the range of 900−1500 °C. Metally, 1991, no. 4, pp. 112−123.
  30. Willemin P., Duque O., Durand-Charre M., Davidson J.H. Experimental determination of nickel-rich corner of Ni–Al–Ta phase diagram. Materials Science and Technology, 1986, vol. 2, no. 4, pp. 344−348. DOI: 10.1179/mst.1986.2.4.344.
  31. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 15, 2024). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  32. Huang M., Zhu J. An overview of rhenium effect in single-crystal superalloys. Rare Metals, 2016, vol. 35, no. 2, pp. 127–139. DOI: 10.1007/s12598-015-0597-z.
  33. Neubauer C.M., Mari D., Dunand D.C. Diffusion in nickel-rhenium system. Scripta Metallugica at Materialia, 1994, vol. 31, no. 1, pp. 99−104. DOI: 10.1016/0956-716X(94)90102-3.
  34. Karunaratne M.S.A., Carter P., Reed R.C. Interdiffusion in the face-centred cubic phase of the Ni−Re, Ni−Ta and Ni–W systems between 900 and 1300 °C. Materials Science and Engineering A, 2000, vol. A281, pp. 229–233. DOI: 10.1016/S0921-5093(99)00705-4.
  35. Campbell C.E., Boettinger W., Kattner U.R. Development of a diffusion mobility database for Ni-base superalloys. Acta Materialia, 2002, vol. 50, pp. 775–792. DOI: 10.1016/S1359-6454(01)00383-4.
  36. Murata Y., Sakurai S., Mabruri E., Koyama T. Cross interdiffusion coefficients in Nickel- and Iron-based ternary alloys. Defect and Diffusion Forum, 2008, vol. 273−276, pp. 419−424. DOI: 10.4028/www.scientific.net/DDF.273-276.419.
  37. Sakurai S., Mabruri E., Murata Y., Koyama T. Diffusion of refractory elements in Ni−X−Y (X, Y: Co, Re, Ru, W) ternary alloys. Defect and Diffusion Forum, 2008, vol. 273−276, pp. 572−576. DOI: 10.4028/www.scientific.net/DDF.273-276.572.
  38. Zeng Q., Ma S.W., Zheng Y.R., Liu S.Z. A study of Re and Al diffusion in Ni. Journal of Alloys and Compounds, 2009, vol. 480, pp. 987–990. DOI: 10.1016/j.jallcom.2009.02115.
  39. Bokshteyn B.S. Diffusion in metals. Moscow: Metallurgiya, 1978, 248 p.
  40. Epishin A.I., Rodin A.O., Bokshteyn B.S., Svetlov I.L. Mutual diffusion in binary alloys of the Ni−Re system. Fizika metallov i metallovedenie, 2015, vol. 116, no. 2, pp. 184–190. DOI: 10.7868/S0015323015020138.
  41. Karunaratne M.S.A., Cox D.C., Carter P., Reed R.C. Modelling of the microsegregation in CMSX-4 superalloy and its homogenisation during heat treatment. Superalloys 2000. TMS, 2000, pp. 263–272.
  42. Janotti A., Krčmar M., Fu C.L., Reed R.C. Solute diffusion in metals: larger atoms can move faster. Physical Review Letters, 2004, vol. 92, no. 8, p. 085901. DOI: 10.1103/PhysRewLett.92.085901.
  43. Epishin A., Brückner U., Portella P.D., Link T. Influence of small rhenium additions on the lattice spacing of nickel solid solution. Scripta Materialia, 2003, vol. 48, no. 4, pp. 455–459. DOI: 10.1016/S1359-6462(02)00436-0.
  44. Caron P. High γʹ solvus new generation nickel-based superalloys for single crystal turbine blade applications. Superalloys 2000, TMS, 2000, pp. 737‒746.
  45. Petrushin N.V., Svetlov I.L., Samoylov A.I., Morozova G.N. Physicochemical properties and creep strength of a single crystal of nickel-base superalloy containing rhenium and ruthenium. International Journal of Materials Research (formerly Zeitschrift Metallkunde), 2010, vol. 101, no. 5, pp. 594–600. DOI: 10.3139/146.110313.
  46. Properties of elements: a reference book in 2 parts. 2nd ed. Moscow: Metallurgiya, 1976, part 1: Physical properties, 600 p.
  47. Villars P., Calvert L.D. Pearson’s Handbook of crystallographic data for intermetallic phases. Ohio: ASM International, 1991, vol. 4, 5366 p.
  48. Epremian E., Harker D. The crystal structure of Ni4W. Journal of Metals, 1949, vol. 1, no. 4, pp. 267−273.
  49. Ochiai S., Mishima Y., Suzuki T. Lattice parameter data of Ni (γ), Ni3Al (γ') and Ni3Ga (γ') solid solutions. Bulletin of Research Laboratory of Precision Machinery and Electronics, 1984, vol. 53, pp. 15‒28.
  50. Kornilov N.I., Snetkov A.Ya. Lattice periods of limited solid solutions of some elements in nickel. Research on heat-resistant alloys: in 10 vols. Moscow: USSR Academy of Sciences, 1961, vol. 7, pp. 106‒111.