Makushina M.A., Panin P.V., Kochetkov A.S. Equipment and technologies for shaped casting of titanium alloys // Proceedings of VIAM. 2025. No. 4 (146). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-4-28-41.

Equipment and technologies for shaped casting of titanium alloys

Makushina M.A., Panin P.V., Kochetkov A.S.
Abstract

This article provides an overview of foreign publications about the equipment and technologies for casting of titanium alloys. All stages of casting are considered: computer modeling of casting processes and special modeling programs; equipment and manufacturing technologies for smelted and burnt models, including those using additive technologies; materials for the manufacture of ceramic molds; traditional and fundamentally new technologies for the direct manufacture of castings. For each section, the level of development and research of the National Research Center «Kurchatov Institute» – VIAM is noted.

Keywords
titanium, casting alloys, castings, wax model, crucible, melt, investment casting
Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  3. Kablov E.N. New generation materials and digital technologies for their processing. Zhurnal neorganicheskoy khimii, 2020, vol. 65, no. 6, pp. 846–855.
  4. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  5. Novak A.V., Nochovnaya N.A., Alekseev E.B., Zavodov A.V. Influence of technological processing parameters on the morphology of the structure and mechanical properties of intermetallic titanium ortho-alloy. Reports All-Rus. scientific-technical conf. «Fundamental and applied research in the field of deformable and cast intermetallic alloys based on titanium and nickel». Moscow: VIAM, 2018, pp. 112–125.
  6. Bratukhin A.G., Kolachev B.A., Sadkov V.V. et al. Technology of production of titanium aircraft structures. Moscow: Mashinostroenie, 1995, 448 p.
  7. Agarwal A., Basile E., Bowler J. et al. Alternative technologies and design for metallic parts in aviation: the use of Titanium investment casting for aircraft structural components. Conference Paper of 5th Aircraft Structural Design Conference. Manchester, 2016, pp. 457–465.
  8. Ndukwe A.I. Review of recent findings on investment casting of titanium alloys. Academic journal of manufacturing engineering, 2022, vol. 20, is. 2, pp. 99–108.
  9. Yang J., Wang H., Wu Y. et al. Numerical calculation and experimental evaluation of counter-gravity investment casting of Ti–48Al–2Cr–2Nb alloy. The International Journal of Advanced Manufacturing Technology, 2018, vol. 96, p. 3295–3309. DOI: 10.1007/s00170-018-1784-5.
  10. Karwinski A., Lesniewski W., Wieliczko P., Małysza M. Casting of titanium alloys in centrifugal induction furnaces. Archives of metallurgy and materials, 2014, vol. 59, is. 1, pp. 403–406. DOI: 10.2478/amm-2014-0068.
  11. Taoa P., Shaoa H., Jib Z. et al. Numerical simulation for the investment casting process of a large-size titanium alloy thin-wall casing. Progress in Natural Science: Materials International, 2018, vol. 28, is. 4, pp. 520–528. DOI: 10.1016/j.pnsc.2018.06.005.
  12. Wu H., Li D., Tang Y. et al. Rapid casting of hollow turbine blades using integral ceramic moulds. Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture. 2009, vol. 223, pp. 695–702. DOI: 10.1243/09544054JEM1366.
  13. Wang J., Sama S.R., Lynch P.C., Manogharan G. Design and topology optimization of 3D-Printed wax patterns for rapid investment casting. Procedia – Manufacturing, 2019, vol. 34, pp. 683–694. DOI: 10.1016/j.promfg.2019.06.224.
  14. Mukhtarkhanov M., Perveen A., Talamona D. Application of stereolithography based 3D printing technology in investment casting. Micromachines, 2020, no. 11, pp. 946–973. DOI: 10.3390/mi11100946.
  15. Ma C., Zhang Y., Zhang H., Wu L. Manufacturing of herringbone gear model by 3D printing assisted investment casting. IOP Conference Series: Earth and Environmental Science, 2019, vol. 332, no. 4, аrt. 042045. DOI: 10.1088/1755-1315/332/4/042045.
  16. Turchenko M.V., Lebedeva Yu.E., Kolmogorov A.Yu., Gurov D.A., Chainikova A.S. Possibility of using layer-by-layer deposition technology (FDM) to produce ceramic products. Trudy VIAM, 2024, no. 8 (138), paper no. 06. Available at: http://www.viam-works.ru (accessed: September 25, 2024). DOI: 10.18577/2307-6046-2024-0-8-64-76.
  17. Turchenko M.V., Lebedeva Yu.E., Belyachenkov I.O., Prokofiev V.A. Obtaining of ceramic materials by stereolithography method. Trudy VIAM, 2023, no. 9 (127), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 27, 2024). DOI: 10.18577/2307-6046-2023-0-9-79-89.
  18. Klotz U.E., Legner C., Bulling F. et al. Investment casting of titanium alloys with calcium zirconate moulds and crucibles. The International Journal of Advanced Manufacturing Technology, 2019, no. 103, pp. 343–353. DOI: 10.1007/s00170-019-03538-z.
  19. Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Kochetkov A.S. Features of the manufacturing technology of highly refractory ceramic molds for castings from γ-TiAl alloys. Trudy VIAM, 2020, no. 2 (86), paper no. 04. Available at: http://www.viam-works.ru (accessed: October 01, 2024). DOI: 10.18577/2307-6046-2020-0-2-31-40.
  20. Uwanyuze R.S., Kanyo J.E., Myrick S.F., Schafföner S. A review on alpha case formation and modeling of mass transfer during investment casting of titanium alloys. Journal of Alloys and Compounds, 2021, vol. 865, pp. 1–19. DOI: 10.1016/j.jallcom.2020.158558.
  21. Kaliuzhnyi P., Mykhnian O.V., Voron M., Tymoshenko A. Problems of materials choice for ceramic molds to obtain titanium alloys shape castings. Casting processes, 2021, vol. 4, no. 146, pp. 55–65. DOI: 10.15407/plit2021.04.055.
  22. Makushina M.A., Kochetkov A.S., Vinogradov I.D. The influence of various modes of hot isostatic pressed and heat treatment on structure and properties of castings from the VT40L alloy. Trudy VIAM, 2023, no. 10 (128), paper no. 03. Available at: http://www.viam-works.ru (accessed: September 10, 2024). DOI: 10.18577/2307-6046-2023-0-10-24-34.
  23. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. 2nd ed., rev. and add. Moscow: VIAM, 2019, 316 p.
  24. Yang L., Chai L.H., Liang Y.F. et al. Numerical simulation and experimental verification of gravity and centrifugal investment casting low pressure turbine blades for high Nb–TiAl alloy. Intermetallics, 2015, no. 66, pp. 149–155. DOI: 10.1016/j.intermet.2015.07.006.
  25. Antipov V.V., Nochovnaya N.A., Kochetkov A.S., Panin P.V., Dzunovich D.A. Influence of technological parameters of casting on the quality of shaped castings from a new heat-resistant alloy based on TiAl. Vestnik MAI, 2018, vol. 25, no. 3, pp. 220–228.
  26. Spitans S., Bauer C., Franz H. et al. Investment castings with unique levitation melting technology FastCast. Conference Paper 68th Investment Casting Institute technical conference & expo 2021. Michigan: Investment Casting Institute, 2021, pp. 181–186.