Fomina M.A., Sibileva S.V., Dyomin S.A., Vasiliev A.S. Thermal indicator materials and their application // Proceedings of VIAM. 2024. No. 8 (138). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-8-77-89.
Thermal indicator materials and their application
Abstract
Thermal indicators include substances that have the ability to sharply change their color at a certain temperature, called the transition temperature. These materials are of significant interest to researchers and manufacturers as they have potential for many technological applications such as aerospace, functional coatings, military applications, printing technologies, «smart» windows, temperature sensors, etc. The nomenclature and variety of thermal indicator substances are constantly evolving, as evidenced by the annual increase in scientific and technical literature publications on this topic.
Keywords
thermal indicator coatings, thermochromism, thermal pigments, thermal indicator paints, inorganic thermochromic materials
Reference list
- Kablov E.N. Main directions of development of materials for aerospace engineering of the 21st century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
- Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
- Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
- Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https: //journal.viam.ru (accessed: May 06, 2024). DOI: 10.18577/2713-0193-2021-0-2-115-122.
- Skupov A.A., Sviridov A.V., Golev E.V., Stekolnikova E.Yu. Laser welding of heat-resistant alloy nickel base for gas turbine elements engines. Aviation materials and technologies, 2023, no. 4 (73), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 06, 2024). DOI: 10.18577/2713-0193-2023-0-4-3-13.
- Kablov E.N., Khmeleva K.M., Zavarzin S.V., Kozlov I.A., Lonskii S.L. The effect of heat treatment on the characteristics of aluminium-zinc coatings obtained by the cold spray method. Aviation materials and technologies, 2022, no. 1 (66), paper no. 07. Available at: http://www.journal.viam.ru (ассеssed: May 06, 2024). DOI: 10.18577/2713-0193-2022-0-1-78-91.
- Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021, no. 1 (62), paper no. 11. Available at: http://www.journal.viam.ru (accessed: May 06, 2024). DOI: 10.18577/2713-0193-2021-0-1-119-126.
- Hassabo A.G., Bakr M., Zayed M., Othman H.A. Chromic Dyes for SMART Textile: A Review. Letters in Applied NanoBioScience, 2023, vol. 12, is. 4, pp. 161–173.
- Durasevic V. Smart dyes for medical textiles. Advances in Smart Medical Textiles. Ed. L. van Langenhove. Cambridge: Woodhead Publishing, 2016, pp. 19–55.
- Karlessi T., Santamouris M., Apostolakis K. et al. Development and testing of thermochromic coatings for buildings and urban structures. Solar Energy, 2009, vol. 83, is. 4, pp. 538–551.
- Dawson T.L. Changing colours: now you see them, now you don’t. Coloration Technology, 2010, vol. 126 (4), pp. 177–188.
- Day J.H. Thermochromism. Chemical Review, 1963, vol. 63, is. 1, pp. 65–80.
- Kiri P., Hyett G., Binions R. Solid state thermochromic materials. Advanced Materials Letters, 2010, vol. 1, is. 2, pp. 86–105.
- Kukushkin Yu.N. Chemistry of coordination compounds. Moscow: Vysshaya shkola, 1985, 455 p.
- Abramovich V.G., Kartavtsev V.F. Color indicators of temperature. Moscow: Energiya, 1978, 216 p.
- Negussie A.H., Morhard R., Rivera J. et al. Thermochromic phantoms and paint to characterize and model image-guided thermal ablation and ablation devices: a review. Functional Composite Materials, 2024, vol. 5, аrt. 1.
- Belenkiy E.F., Riskin I.V. Chemistry and technology of pigments. Moscow: Khimiya, 1974, 625 p.
- Nikiforov A.L., Karasev E.V., Bulgakov V.V., Zhivotyagina S.N. Use of thermochromic materials as signaling means of fire prevention in electrical installations. Pozharovzryvobezopasnost, 2015, vol. 24, no. 9, pp. 41–47.
- Granqvist C.G., Lanseker P.C., Mlyuka N.R. et al. Progress in chromogenics: New results for electrochromic and thermochromic materials and devices. Solar Energy Materials and Solar Cells, 2009, vol. 93, no. 12, pp. 2032–2039.
- Alamri S.N. The temperature behavior of smart windows under direct solar radiation. Solar Energy Materials and Solar Cells, 2009, vol. 93, no. 9, pp. 1657–1662.
- Cui H.N., Costa M.F., Teixeira V. et al. Electrochromic coatings for smart windows. Surface Science, 2003, vol. 532–535, pp. 1127–1131.
- Wu S., Sun H., Duan M. et al. Applications of thermochromic and electrochromic smart windows: Materials to buildings. Cell Reports Physical Science, 2023, vol. 4, pp. 1–33.
- Choi S., Larrabee J.A. Thermochromic Tetrachlorocuprate (II): An Advanced Integrated Laboratory Experiment. Journal of Chemical Education, 1989, vol. 66, no. 9, рр. 774–776.
- Temperature indicator anti-corrosion coating: pat. 2586701 Rus. Federation; appl. 26.06.14; publ. 27.12.15.
- Method of manufacturing a temperature indicator: pat. 2579834 Rus. Federation; appl. 11.02.15; publ. 10.04.16.
- Uleva S.N., Nikiforov A.L., Nakonechny S.N., Tsirkina O.G. Problems of implementing visual control of thermal operating modes of process equipment to prevent emergency situations. Pozharnaya i avariynaya bezopasnost, 2021, no. 1 (20), pp. 32–38.
- Leonov A.P., Bolgova V.A. Visualization of Local Overheating Spots in Cable Insulation. Naukovedenie, 2014, no. 2 (21), pp. 1–8. Available at: https://naukovedenie.ru/PDF/118TVN214.pdf (accessed: May 06, 2024).
- Lagutin A., Sorokin E. Assessment of the State of Contact Joints of Outdoor Switchgear Using Thermal Indicators. Elektroenergiya. Peredacha i raspredelenie, 2023, no. 1 (28), pp. 40–43.
- Vlasov S. N., Tereshkov A. S., Klimov A. S. Monitoring the Presence of Pores Using Thermochromic Materials. Results of Modern Scientific Research and Development: XIII All-Rus. Scientific and Practical Conf. Penza, 2021, pp. 62–64.
- Pierce J.W., Goodenough J.B. Structure of Orthorhombic V0,95Cr0,05O2. Physical Review B, 1972, vol. 5, is. 10, pp. 4104–4112.
- Ivanayskiy V.V. On the Possibilities of the Temperature Indicator Method in Research of Induction Surfacing Technology. Vestnik Altayskogo gosudarstvennogo agrarnogo universiteta, 2018, no. 11 (169), pp. 108–112.
- Guzman G. Thermochromic transition-metal oxides. Sol-gel technologies for glass producers and users. Eds M.A. Aegerter, M. Mennig. New York: Springer, 2004, pp. 271–276.
- Johan O.D., Hassin M.M. Investigation on Dielectric Constant of Zinc Oxide. Modern Applied Science, 2009, vol. 3, no. 2, pp. 110–116.
- Mirnaya M.R., Ivanov K.A. Development and practical application of temperature indicator paints in a real experiment. Mir izmereniya, 2011, no. 12, pp. 26–30.
- Inorganic reversible temperature indicator: pat. 2561737 Rus. Federation; appl. 12.09.14; publ. 10.09.15.
- Hossain S., Sadoh A., Ravindra N.M. Principles, properties and preparation of thermochromic materials. Material Science & Engineering International Journal, 2023, vol. 7, is. 3, pp. 146–156.
- Jeong J., Min K.S., Kumar R.S. et al. Synthesis of novel betaine dyes for multi chromic sensors. Journal of Molecular Structure, 2019, vol. 1187, pp. 151–163.
- Abdellaoui H., Raji M., Chakchak H. et al. Thermochromic composite materials: synthesis, properties and applications. Polymer Nanocomposite-Based Smart Materials. From Synthesis to Application. Eds. R. Bouhfid, A.K. Qaiss, M. Jawaid. Cambridge: Woodhead Publishing, 2020, pp. 61–78.
- Talvenmaa P. Introduction to chromic materials. Intelligent Textiles and Clothing. Ed. H.R. Mattila. Cambridge: Woodhead Publishing, 2006, pp. 193–205.
- Zhao Y., Li L. Colorimetric properties and application of temperature indicator thermochromic pigment for thermal woven textile. Textile Research Journal, 2018, vol. 89, pp. 3098–3111.